Veenasri
Vallem
a,
Erin
Roosa
a,
Tyler
Ledinh
a,
Sahar
Rashid Nadimi
ab,
Abolfazl
Kiani
ab and
Michael D.
Dickey
*a
aDepartment of Chemical and Biomolecular Engineering, North Carolina State University, Raleigh, NC 27695, USA. E-mail: mddickey@ncsu.edu
bDepartment of Chemistry and Biochemistry, California State University, Bakersfield, Bakersfield, CA 93311, USA
First published on 23rd November 2022
Soft pneumatic actuators—such as those used for soft robotics—achieve actuation by inflation of pneumatic chambers. Here, we report the use of the electrochemical reduction of water to generate gaseous products that inflate pneumatic chambers. Whereas conventional pneumatic actuators typically utilize bulky mechanical pumps, the approach here utilizes only electricity. In contrast to dielectric actuators, which require ∼kV to actuate, the electrochemical approach uses a potential of a few volts. The applied potential converts liquid water—a safe, abundant, and cheap fuel—into hydrogen gas. Since the chambers are constructed of hydrogel, the body of the actuator provides an abundant supply of water that ultimately converts to gas. The use of liquid metal for the electrode makes the entire device soft and ensures intimate contact between the chamber walls and the electrode during inflation. The device can inflate in tens of seconds, which is slower than other pneumatic approaches, but much faster than actuating hydrogels via principles of swelling. The actuation volume can be predicted and controlled based on the input parameters such as time and voltage. The actuation shape and position can also be controlled by the position of the electrodes and the geometry of the device. Such actuators have the potential to make tether-less (pump-free), electrically-controlled soft devices that can even operate underwater.
Colloquially, the term bubbles usually refer to small volumes of gas surrounded by a liquid; here we use the term ‘bubble’ more generally to describe elastic chambers filled with gas. Bubbles formed from liquids (or solids) are appealing as actuators because of the enormous change in volume. For example, 1 mol of water increases volume by ∼1244 times when converted to water vapor at room temperature. Such large changes in volume find use in commercial products, such as airbags for cars. Gas can be generated by (i) heating liquid to form vapor (phase change actuators),3 (ii) electrochemically displacing microscale elastic membranes2,4 or fluid (electrochemical actuators)5 (iii) injecting air into expandable chambers (pneumatic actuators)9,11 and (iv) applying electrostatic forces to deform a fluid-filled elastomer chamber (dielectric actuator).7,8 Here, we generate the gas electrochemically to actuate elastomeric chambers composed of a hydrogel.
Pneumatic actuation of elastomeric chambers is commonly used for soft robotics. Such chambers are lightweight and easy to fabricate. They can also provide non-linear motion with simple inputs and use soft materials that interact safely with humans.12 Generally, pneumatic actuators convert electrical energy (from an outlet or battery), to mechanical energy (pumping), and ultimately to pneumatic energy (PV work) that actuates the device. Unfortunately, the pumps used to inflate the chambers are bulky and use tubing that “tethers” the devices, thus limiting their motion. There are exceptions; chemical reactions can rapidly generate pressure without the need for pumps, but use potentially dangerous explosions.13,14 We were motivated to explore ways to inflate pneumatic chambers without a pump and in a way that could be inflated directly with electricity using safe materials. Although dielectric actuators function based on electrical input, they require very high voltages (∼kV) to actuate.15 In contrast, electrochemical actuators require only a few volts (∼V) to actuate.4
The electrochemical actuators used here consist of two electrodes in a hydrogel. The hydrogel serves as an electrolyte medium. Upon applying a voltage between the electrodes, redox reactions occur at the interface between the hydrogel and electrode. One or more of the reactions produce gaseous products depending on the design. The most relevant prior work utilized liquid electrolytes packed in a microscale elastomeric chamber with rigid electrodes.4 Such actuators were used for small-scale (μm) actuation and not soft robotics. We show here that rigid wires are poorly suited for larger (cm scale) devices because the inflation of the chambers separates the hydrogel and the wire. Electrodes that maintain contact with the hydrogel are necessary for proper pneumatic inflation in our design.
We report an entirely soft electrochemical bubble actuator made of liquid metal (LM) electrodes and hydrogel. LM electrodes composed of gallium alloys (here, eutectic gallium indium) have been interfaced with hydrogel before for electrodes,16 energy harvesting,17 and memory devices,18 but not for the purpose of driving electrochemical reactions for bubble actuators. Here, the hydrogel serves two purposes: (1) it forms stretchable chambers that can inflate pneumatically, and (2) it contains water ∼70% water, which serves as the ‘fuel’ for electrochemical actuation. Applying voltage to the LM converts the water from the hydrogel—which is biocompatible and inexpensive—into hydrogen gas. The gas formed inflates the hydrogel membrane forming a bubble that contains hydrogen gas, LM, and a small amount of water from the wall of the hydrogel. Thus, we use the term ‘bubble’ to describe the gas formed19 and the term ‘chamber’ to describe the entire bubble including the hydrogel walls that encase the bubble. The word ‘chamber’ is also used to distinguish between the liquid based electrochemical actuators where liquid electrolyte is filled in an elastic sac, while here, the chamber wall (gel in contact with the LM) provides the electrolyte for actuation. Thus, the pneumatic fuel (water) is ‘embodied’ within the walls of the hydrogel chamber.
The devices can undergo multiple actuation cycles as very little water is consumed per cycle. In principle, such hydrogels can even absorb water from the environment to provide continuous operation.20 The soft LM electrode stays in contact with the hydrogel, which is necessary to form the hydrogen gas continuously. The actuator requires only a few volts of voltage input and actuates within seconds. The actuator retains 60% of the bubble volume for 6 h upon removing the voltage input. Although not a focus here, the design can also be modified to enable reversible actuation, which allows the hydrogel membrane to expand and contract within a few seconds. We characterized the performance of these devices as a function of counter electrode material, input voltage, and device architecture. The actuation volume can be predicted based on the input parameters such as time and voltage. In addition, we studied various device architectures to induce curvature in the system upon bubbling to create hydrogel grippers. To our knowledge, this is the first report of macroscale (∼cm) soft electrochemical actuators where the chamber wall provides the electrolyte for actuation.21 These devices provide pump-free and electronically controlled actuation of soft hydrogel-based devices. Here, we introduce the concept of using soft electrochemical systems that could enable pump-free pneumatic actuation. We characterize the bubbling mechanism by varying the input voltage, time, and distance between the electrodes. We also demonstrate ways to induce curvature in the system that could help perform actions like lifting objects.
Gas formation is enhanced by the use of LM due to its ability to flow to maintain contact with the gel. Upon applying a reducing potential to devices fabricated using only Cu electrodes (Fig. 1D), a thin layer of gas formed around the electrode (Fig. 1E), causing the electrode to lose contact with the hydrogel. Hence, the chamber did not grow further in the absence of liquid metal, as shown in ESI,† Video S1. Applying 15 V for 20 s to the copper electrodes creates insignificant inflation (Fig. 1F) compared to the device made of LM electrodes (Fig. 1C). We also tried to contact the hydrogel chamber with other stretchable electrodes, such as arrays of silver nanowires, but the nanowires quickly degraded in the electrochemical environment.
We used polyacrylamide gel because it is soft, stretchable, and easy to fabricate by simple photopolymerization of a monomer solution (see Experimental section). We used 1.5 mm thick walls as it enables actuation within seconds and retains the bubble volume for several hours. For example, a bubble formed upon inflating for 30 seconds at 10 V input retains 60% of the volume for 6 h after ceasing to apply voltage (ESI,† Fig. S1).
The use of LM and hydrogel in making electrochemical actuators provides the following unique attributes:
1. LM and hydrogel are both inherently soft and therefore help realize soft and deformable actuators.
2. Conventional metal wires lose contact with the gel due to the thin pocket of gas that forms during actuation. In contrast, the LM stays in contact with the hydrogel, which is necessary to continuously form the gas that inflates the chamber.
3. The gas forms from water, which is safe, abundant, and inexpensive.
4. The hydrogel chamber walls, which contain ∼70 wt% water, provide the ‘embodied’ source of water.
5. The devices can undergo multiple actuation cycles since very little water is consumed per actuation (ESI,† Video S2).
6. Although actuation is much slower than pump-based pneumatic actuators, the actuation takes place in seconds, which is faster than hydrogel-based actuators that utilize diffusion of water in or out of the gel to cause swelling (minutes to hours).26,27
7. The LM starts out as a rectangular shape but retracts into a sphere during reduction creating a void that directs the chamber shape. This allows a facile route to regulate the geometry of the chamber (ESI,† Video S3).
Fig. 2 Bubble actuator characterization. (A) A schematic describing the input and output parameters. (B) The current generated in the bubble actuator system and (C) the output (bubble volume) measured as a function of time while applying 5 V. (D) Comparison of experimental and theoretical model results, which are fit with a line with a slope of 1.23 and R2 = 0.998. (E) The bubble volume measured as a function of voltage applied. The bubble volume was recorded at 30 s in each case while a corresponding voltage was applied. The error bars are generated by analyzing the readings from three different devices. The red lines indicate model predictions of the output parameter (dependent variable on y – axis) based on the input (independent variable on x – axis). The distance between the electrodes in the bubble actuator in B, C, D, is 2.5 mm and E is 5 mm. For further details on the role of the distance between the electrodes, see ESI,† Fig. S2. |
The volume of the hydrogen bubble can be calculated using the ideal gas law,
Bubble volume (t) = N(t)RT/P(t) | (1) |
(2) |
The volume expansion of the chamber is opposed by two forces: (1) the surrounding atmospheric pressure, and (2) the elasticity of the walls of the hydrogel chamber. We find that the elasticity of the walls is negligible due to the low modulus and thin nature of the gel (scaling relations are found in the ESI†). Thus, to simplify the analysis, we approximate the pressure to be constant and approximately equal to Patm. Thus,
(3) |
Eqn (3) requires knowledge of the current, which we measured simultaneously during inflation as plotted in Fig. 2B. We fit the data with exponential decay. The Randles equivalent circuit is often used to predict the current response of an electrochemical system to a step change in voltage.28,29 Although the Randles model predicts an exponential decay, the premise of the model does not capture all the physical changes occurring here, such as changes to the shape and contact area of the electrodes. Nevertheless, the data nicely fits to an exponential decay (eqn (4)), which suits the purpose of having a mathematical prediction of current versus time to satisfy eqn (3).
i(t) = A + B exp(−t/τ) | (4) |
The red line in Fig. 2B indicates the best fit using eqn (4).
Fig. 2D plots the experimental chamber volume versus the theoretical bubble volume data. The latter is obtained by using D = RT/nFPatm = 126, slightly smaller than the empirical fit of D = 156. A linear fit gives a slope of 1.23 and R2 = 0.998, intercept 0. A slope greater than 1 suggests that the experimental volume increases more than expected from the theory. This discrepancy could be due to the challenges associated with estimating the bubble volume. We assume the bubble is an ellipsoid. We determine the bubble volume by measuring the diameters of the ellipsoid manually from the side and top view pictures using Image J software. Thus, there could be error (for more details, see ESI†).
Fig. 4 Bubble actuator gripper. Photographs demonstrating the two modes of gripping: (A and B) inward curl gripping and (C and D) outward curl gripping. The grippers held the objects firmly after lifting them off the ground (B) a ball of 4 cm diameter and (D) a 20 ml glass vial in 30 s and 16 s respectively when a voltage input of 10 V is applied. The demonstrations can be found in ESI,† Videos S4 and S5. The scale bars represent 1 cm. |
The actuator retains 60% of its final bubbled state for 6 h upon removing the voltage input. A focus of ongoing and future work is to design vents to enable reversible actuators. For example, our initial results suggest the design can also be modified to enable reversible actuation by venting the gas at a rate that varies non-linearly with inflation. This would allow the hydrogel membrane to expand and contract within a few seconds (ESI,† Video S2). In principle, the hydrogen could also be used further, either as a fuel (for combustion-based actuation) or to simply recombine with oxygen to regenerate the water. Although we did not show it here, gels can be made to be hygroscopic, and thus, it may be possible to harvest additional water from the atmosphere to replace consumed water.20
We characterized the performance of these devices as a function of electrode material, input voltage, and device architecture. We modeled the behavior to show that the actuation volume as a function of time is directly proportional to current. For the gels used here, the current increases with voltage and by decreasing the distance between the electrodes. In addition, we studied various design architectures to induce curvature in the system upon bubbling and demonstrated hydrogel grippers. To our knowledge, this is the first macroscale (cm) soft electrochemical actuator reported. These devices with pump-free and electronically controlled actuation may find use in enabling autonomous soft grippers or haptics. In addition, the unique combination of materials allows a new type of hydrogel actuators that are soft, biocompatible, and can operate underwater.
This work demonstrates a way to use soft electrochemical systems in enabling pump-free pneumatic actuators. There remain challenges and opportunities: (1) establishing reversible actuation using effective mechanical designs and/or novel chemistry. (2) Optimizing the actuator performance such as blocked force and speed by varying the materials of construction and geometry. (3) Limiting water loss from the hydrogels. (4) Identifying chemistries that enable faster actuation, require lower input voltage, and avoid irreversible reaction products that cause active material loss such as electrodes and electrolyte during actuation.
To attach a carbon felt electrode, we follow slightly different fabrication steps. First, we place the carbon felt electrode on the bottom of the mold and pour the pre-gel solution on the top and cure it so one side of the carbon felt is open to the air and the other side is covered with the gel. In parallel, we follow the first and the second steps mentioned above to obtain a hydrogel with pockets filled with LM. Later, we pour a few drops of pregel solution on top of that and place the carbon-felt gel composite with carbon felt facing the air. We then cure it to bind both gels.
Bubble volume is estimated using the volume equation for an ellipsoid, where a was the x-radius of the ellipsoid and b was the y-radius of the ellipsoid, and c was the height of the ellipsoid. a and b are obtained from the top view photograph and c is obtained from the side view photographs as shown in ESI,† Fig. S7. We limit the experimental time to 50 s to prevent bubble bursting.
Footnote |
† Electronic supplementary information (ESI) available. See DOI: https://doi.org/10.1039/d2sm00874b |
This journal is © The Royal Society of Chemistry 2022 |