Delithiation/lithiation behaviors of three polymorphs of LiVOPO4

Author affiliations

Abstract

LiVOPO4 is an attractive high-voltage cathode with rich polymorphs (α, β and αI). We present here a comparison of the behaviors of three LiVOPO4 polymorphs during delithiation/lithiation. Experimental and computational work suggests that α-LiVOPO4 suffers from more severe conductivity problems among the three forms. For the first time, our preliminary studies on lithiated β-Li2VOPO4 demonstrate that the orthorhombic structure of β-LiVOPO4 could be retained after lithiation, which is consistent with the finding for the other two forms.

Graphical abstract: Delithiation/lithiation behaviors of three polymorphs of LiVOPO4

Back to tab navigation

Supplementary files

Publication details

The article was received on 13 Sep 2018, accepted on 02 Nov 2018 and first published on 02 Nov 2018


Article type: Communication
DOI: 10.1039/C8CC07446A
Citation: Chem. Commun., 2018,54, 13224-13227

  •   Request permissions

    Delithiation/lithiation behaviors of three polymorphs of LiVOPO4

    G. He, W. H. Kan and A. Manthiram, Chem. Commun., 2018, 54, 13224
    DOI: 10.1039/C8CC07446A

Search articles by author

Spotlight

Advertisements