Thermoelectric properties of Eu(Zn1−xCdx)2Sb2

Abstract

The thermoelectric performance of EuZn2Sb2 and EuCd2Sb2 was optimized by mixed occupation of the transition metal position. Samples in the solid solution Eu(Zn1−xCdx)2Sb2 with the CaAl2Si2-type crystal structure (space group [P with combining macron]m1) were prepared from the elements for compositions with x = 0, 0.1, 0.3, 0.5 and 1. The thermoelectric properties were investigated after densification of the products by spark plasma sintering (SPS). The samples show low electrical resistivity, high thermopower and a low lattice thermoconductivity. The highest ZT value of 1.06 at 650 K is obtained for x = 0.1.

Graphical abstract: Thermoelectric properties of Eu(Zn1−xCdx)2Sb2

Article information

Article type
Paper
Submitted
10 Aug 2009
Accepted
11 Sep 2009
First published
25 Sep 2009

Dalton Trans., 2010,39, 1101-1104

Thermoelectric properties of Eu(Zn1−xCdx)2Sb2

H. Zhang, M. Baitinger, M. Tang, Z. Man, H. Chen, X. Yang, Y. Liu, L. Chen, Y. Grin and J. Zhao, Dalton Trans., 2010, 39, 1101 DOI: 10.1039/B916346H

To request permission to reproduce material from this article, please go to the Copyright Clearance Center request page.

If you are an author contributing to an RSC publication, you do not need to request permission provided correct acknowledgement is given.

If you are the author of this article, you do not need to request permission to reproduce figures and diagrams provided correct acknowledgement is given. If you want to reproduce the whole article in a third-party publication (excluding your thesis/dissertation for which permission is not required) please go to the Copyright Clearance Center request page.

Read more about how to correctly acknowledge RSC content.

Social activity

Spotlight

Advertisements