Synthesis of solid superacid catalyst with acid strength of H0⩽–16.04
Abstract
A solid superacid catalyst with an acid strength of H0⩽–16·04, which was active for reactions of propane and butane, was obtained by exposing Zr(OH)4, prepared by the hydrolyses of ZrOCl2 and ZrO(NO3)2, to 1 N H2SO4 and then calcining in air at 575–650 °C.