High dielectric thin films based on barium titanate and cellulose nanofibrils

Jie Taoa, Shun-an Cao*a, Rui Fengb and Yulin Deng*c
aSchool of Power and Mechanical Engineering, Wuhan University, Wuhan, 430072, China. E-mail: shunancao@163.com
bSchool of Material Science and Engineering, Wuhan University of Technology, Wuhan, 430070, China
cSchool of Chemical & Biomolecular Engineering, Renewable Bioproducts Institute, Georgia Institute of Technology, Atlanta, GA 30332-0620, USA. E-mail: yulin.deng@rbi.gatech.edu

Received 25th December 2019 , Accepted 31st January 2020

First published on 4th February 2020


Abstract

A series of composite films based on tetragonal barium titanate (BTO) and cellulose nanofibrils (CNF) with high dielectric constant are prepared using a casting method in aqueous solution. No organic solvent is involved during the preparation, which demonstrates the environmental friendliness of the novel material. With less than 30 wt% of filler loading, the excellent distribution of BTO nanoparticles within the CNF matrix is revealed by the FE-SEM images. The dielectric constant of the CNF/BTO (30 wt%) composite film reaches up to 188.03, which is about seven times higher than that of pure CNF (25.24), while the loss tangent only rises slightly from 0.70 to 1.21 (at 1 kHz). The thin films kept their dielectric properties on an acceptable level after repeatedly twisting or rolling 10 times. The improvement of thermal stability is observed with the presence of BTO. The outstanding dielectric properties of the CNF/BTO composite film indicates its great potential to be utilized in energy storage applications.


Introduction

In the past decades, considerable research effort has been made to exploit sustainable energy to replace fossil fuels and reduce pollution.1 High dielectric materials (HDMs) are of vital importance in energy storage and conversion devices for solar and wind energy because of their high energy density and power density. HDM based capacitors receive much attention in the applications of portable electronics, hybrid electric vehicles, and so on.2 Excellent HDMs can significantly cut down dissipation, improve the efficiency of energy storage, and shrink the size of devices.3 Organic/inorganic composites are some of the most extensively studied HDMs as they combine the merits of both components, such as enhanced dielectric properties, outstanding thermal stabilities, bio-compatibility, light weight, low cost and remarkable processing properties.4–7

Ferroelectric ceramics such as lead-free barium titanate (BaTiO3, BTO) have long been of interest as fillers for high dielectric composites.8,9 This is due to their high dielectric constant (as high as 7000),10 low dissipation, impressive piezoelectric and pyroelectric properties.11,12 The effects of size, shape (e.g., nanoparticles, nanorods, nanowires, nanocubes), crystal phase (e.g., cubic, tetragonal, orthorhombic, rhombohedral), matrix, surface conditions, porosity, filler loading and distributions have been discussed intensively in the literature.13–18 By adjusting these factors, a range of BTO based composites have been reported to have splendid dielectric properties.19–24 Dang et al.25 modified BTO particles (diameter = 700 nm) with 1.0 wt% of silane coupling agent (KH550) to improve its compatibility with polyvinylidene fluoride (PVDF), and the relative dielectric constant (εr) of the PVDF/BTO (40.0 vol%) composite (thickness = 1 mm) is more than 50, whereas the loss tangent (tan[thin space (1/6-em)]δ) is lower than 0.03 (at 1 kHz). In order to improve the thermal stabilities, Dang's research group26 then prepared polyimide (PI)/BTO composite by in situ polymerization. With 40 vol% of BTO (diameter ∼ 100 nm) loaded, the εr of the films (thickness 10–70 μm) reaches 18, while tan[thin space (1/6-em)]δ is below 0.01 (at 1 kHz). More PVDF based polymers are employed as the dielectric matrix, and their εr is in the range from 30 to 50 (at 1 kHz) with tan[thin space (1/6-em)]δ lower than 0.05.27–29 Kim et al.30 investigated polycarbonate (PC) as the matrix for chemically functionalized BTO and obtained a series of thin films nanocomposite (thickness = 3.89 μm). With a filler content of 50 vol%, the εr of the sample film is 37 ± 2, and tan[thin space (1/6-em)]δ is <0.03 (at 1 kHz). Luo et al.31 designed a 3D BTO network and synthesized a composite by injecting epoxy solutions into the porous structure. With 30 vol% BTO (size of grain = 0.5–1 μm) loaded, a high εr of 200 is achieved with a tan[thin space (1/6-em)]δ of 0.14 (at 1 kHz).

The recent researches based on BTO fillers focus more on improving breakdown strength and reducing tan[thin space (1/6-em)]δ to pursue higher energy density and storage efficiency.31–38 Generally, most of the applied polymer matrices are non-biodegradable or even toxic. And some of the matrix polymers, such as polycarbonate, reported in the literature are fragile or stiff, which are not suitable for soft and portable electronic applications. Therefore, more and more researchers are exploring safe, green and environmentally friendly alternatives. Cellulose, nanocellulose and their derivatives are reported to be a promising replacement for the traditional polymer dielectric matrices.39–62 Chiang et al.63 mixed BTO (diameter < 2 μm) with cyanoethyl cellulose (CEC) in acetone and prepared a well-dispersed composite with a thickness of 100–350 μm. The εr of the composite increases from 21 for pure CEC to 133 (at 1 kHz) with the addition of 51 vol% BTO. Jia et al.64 reported a three-phase composite (thickness ∼ 75 μm) based on 30 wt% BTO (diameter ≈ 100 nm), 24 wt% antimony tin oxide (ATO, diameter ≈ 10 nm), and CEC. The εr of the CEC/ATO/BTO nanocomposite film reaches 66.08 with a tan[thin space (1/6-em)]δ of ∼0.1 (at 1 kHz). Cellulose is a common and almost inexhaustible resource in nature. Recently, novel nanocellulose garners attention because of its specific properties such as good dielectric properties, low coefficient of thermal expansion, flexible, excellent mechanical properties, high transparency, low density, and strong chemical durability.65–74 It worth to note that nanocellulose is made from pure mechanical grinding, thus no toxic solvent is needed for its production. Hassan et al.11 doped BTO (diameter ≈ 180 nm) into 2,2,6,6-tetramethylpiperidinyl-1-oxyl (TEMPO) oxidized cellulose nanofibrils (CNFs). With 5 wt% BTO added, the εr of the composite films of TEMPO-modified CNF (TCNF) and BTO (thickness of 0.09–1 mm) is 49[thin space (1/6-em)]000, which is four times higher than that of pure TCNF films (11[thin space (1/6-em)]034 at 1 kHz). And tan[thin space (1/6-em)]δ is increased from ∼0.01 for pure CNF to ∼2. In our previous study, titanium dioxide (TiO2) was used as the filler, and the dielectric properties of CNF/TiO2 and TCNF/TiO2 nanocomposite were compared.42 It was found that CNF is a better choice than TCNF as the high dielectric matrix for the sake of reliability and energy saving. With 50 wt% of TiO2 loaded, the εr of the CNF/TiO2 nanocomposite films is 19.51 with a tan[thin space (1/6-em)]δ of 0.81.

Based on the above discussions, here we report a 0–3 composite high dielectric system by directly mixing zero-dimensional BTO with three-dimensional CNF in aqueous solution. A series of flexible free-standing CNT/BTO nanocomposite films was prepared by casting method and hot-press treatment. We choose isotropic BTO particles as filler due to its simplicity synthesis in practical applications. BTO nanoparticles were thermally treated to get a tetragonal phase, which is reported to have a higher εr than a cubic phase.18 Theoretically, the positively charged surface of BTO nanoparticles should be able to adhere to the negatively charged surface of CNF.11 Since both BTO and CNF are highly dispersible in water, no organic solvent was used during the process. Morphologies, phase compositions, dielectric related properties and thermal stabilities of the CNF/BTO sample films were measured and evaluated, and the results demonstrate that the obtained nanocomposite has great potential to be practically utilized in energy storage applications.

Experimental

Materials

CNF slurry with a solid content of ∼3% was supplied by Cellulose Lab Inc. (Canada) and used as received.75–78 The CNF has a diameter of 6–80 nm with a length of several micrometers. BaTiO3 nanoparticles (diameter < 100 nm, 99.9%) was purchased from Aladdin Co., Ltd. (China), and calcined at 1000 °C for 10 hours. Deionized water was obtained by a Millipore Direct-Q3 water purification system.

Sample preparation

The CNF/BTO nanocomposite films were prepared by simply mixing and solution casting method, as shown in Fig. 1. The CNF/BTO nanocomposite films were prepared by simply mixing and solution casting method, as shown in Fig. 1. CNF slurry was diluted into 0.3 wt% by deionized water, and stirred by a homogenizer (RCD-1A, Changzhou yuexin, China) for 5 min. After the dilution, a certain amount of BTO was added according to the dry weight percentage, and the solution was homogenized for 5 min again. Subsequently, the solution was poured into a Petri dish and dried in a fume hood for several days. Finally, the obtained film was hot-pressed under 80 °C for 3 hours. The thickness of the flexible films was in the range of 30–100 μm.
image file: c9ra10916a-f1.tif
Fig. 1 Preparation of CNF/BTO nanocomposite films.

Measurement and characterization

The surface and cross-section morphologies of sample films were investigated by field-emission scanning electron microscopy (FE-SEM, TESCAN MIRA3, Czech Republic) with an accelerating voltage of 5 kHz. Prior to the measurement, the samples were coated with a thin layer of gold using a sputter coater (Quorum SC7620, UK) in a vacuum to reduce charge interruptions. Energy-dispersive X-ray spectroscopy (EDS, Oxford X-Max20, UK) was used to analyze the distribution of BTO in the CNF matrix. X-ray diffraction (XRD) patterns of BTO particles and CNF/BTO composite films were determined by an X-ray diffraction spectrometer (XRD, PANalytical XPert Pro, Netherlands). The XRD patterns were recorded with Cu Kα radiation (λ = 1.542 Å) at 40 kV and 40 mA in the 2 theta (2θ) value range from 5° to 80°. The thermal stabilities of the nanocomposites were tested by thermogravimetric analysis and differential scanning calorimetry (TGA-DSC, Netzsch STA449F3, Germany) at a heating rate of 10 °C min−1 from 35 °C to 790 °C under a nitrogen atmosphere. The dielectric constant, loss tangent and AC electrical conductivity of sample films were studied using an LCR meter (Keysight E4980A, USA). The results were recorded in the frequency range from 40 Hz to 1 MHz with an oscillation signal of 1 V at ambient temperature. Prior to the measurement, gold electrodes were sputtered on both sides of the specimens, and the test was repeated four times for each composition. The relative dielectric constants (εr) of the sample films were calculated by eqn (1):
 
image file: c9ra10916a-t1.tif(1)
where, C is the capacitance; ε0 is the absolute dielectric constant of vacuum, ε0 = 8.854 × 10−12 F m−1; A is the electrode area, A = 4.52 × 10−6 m2; d is the thickness of the sample film. The polarization–electric field (PE) curves of the sample films were measured with a ferroelectric tester (Radiant Precision Multiferroic II, USA) at 100 Hz.

Results and discussion

Morphology

Well dispersion of BTO filler is conducive to uniform packing of CNF/BTO nanocomposite, leading to better dielectric properties. The surface and cross-section morphologies of the pure CNF and CNF/BTO composite films were investigated by FE-SEM images (shown in Fig. 2). Pure CNF film had a smooth surface and laminated structure (Fig. 2a and d). The morphological changes induced by BTO fillers on the CNF are very clear. In the lower range of filler content, BTO particles exhibited good dispersion in the CNF matrix, in turn, the composite films kept as dense as pure CNF film. With the addition of 30 wt% BTO, small voids and a rough surface started to be seen due to the aggregation of BTO (Fig. 2b and e). BTO particles with a diameter of 0.5–1.0 μm are resulted from high-temperature calcination, and there are strong forces between particles.79 Generally, BTO particles are still uniformly dispersed throughout the CNF matrix, which is in good accordance with EDS results (Fig. S1–S6). In the specimens with higher BTO content, the laminated structure disappeared, and big spheres with a diameter of >10 μm are observed (Fig. 2c and f). The films exhibit porous and loose structure due to the weakening of CNF chain–chain interactions by the inclusion of BTO particles.79 This result shows that uniform CNF/BTO nanocomposite films can be obtained by simple mechanical mixing and casting methods when filler content below 30 wt%.
image file: c9ra10916a-f2.tif
Fig. 2 Surface and cross-section FE-SEM micrographs of pure CNF (a and d), CNF/BTO (30 wt%) (b and e) and CNF/BTO (90 wt%) (c and f) composite films.

Phase composition

The dielectric properties of the composite are influenced by the crystal properties of the constituents. Tetragonal BTO has a higher dielectric constant than other phases, e.g., cubic phase. Taking this advantage, tetragonal BTO has much higher commercial value than other phases. The phase compositions of pure CNF, untreated BTO, thermally treated BTO, and CNF/BTO (30 wt%) composites were recorded by XRD patterns, as is presented in Fig. 3. The abroad peak in the region of 15° to 17° and at 22.6° are corresponding to the partly crystalline structure of CNF.11,62,80 The peak intensity of CNF in the nanocomposite films decreased with the addition of BTO due to the destruction of the ordered structure.64 The XRD pattern of thermally treated BTO was in line with tetragonal BTO (JCPDS No. 89-1428). Especially, the characteristic splitting peak of the tetragonal phase was seen distinctively at 45°.79,81,82 Owing to the higher crystallinity of BTO, its peaks were much sharper than that of CNF. In the XRD pattern of CNF/BTO composite, the peak intensity of both CNF and BTO decreased compared with pure CNF and BTO. It is ascribed to the addition of nanofillers, which destroys the ordered structure of the CNF and reduces its crystallinity.83 It is worth mentioning that the peak positions of both CNF and BTO remained unchanged in the CNF/BTO composite, which indicates that the mechanical mixing process does not affect the crystalline structure of these two constitutes.61
image file: c9ra10916a-f3.tif
Fig. 3 XRD patterns of pure CNF, untreated BTO, thermally treated BTO, and CNF/BTO (30 wt%) nanocomposite films.

Dielectric properties

The dielectric properties usually refer to the relative dielectric constant (εr) and loss tangent (dissipation factor, tan[thin space (1/6-em)]δ). Towards the application of energy storage, conductivity and PE hysteresis loop were also examined. All of these properties are considerably affected by the frequency. The frequency dependence of εr and tan[thin space (1/6-em)]δ was studied, as shown in Fig. 4a and b. In the low-frequency range of 40–10 kHz, both εr and tan[thin space (1/6-em)]δ decreased sharply with the increase of frequency, and a tan[thin space (1/6-em)]δ peak was presented in the plot of samples with 0–40 wt% BTO. These are typical characteristics of electrode effect and Maxwell–Wagner–Sillars interfacial polarization.50,60,84–86 With the frequency going up, the high periodic reversal of the electric field makes it harder for dipoles and charge carriers, which accumulated at the interface, to catch up with the change of frequency. Hence, the interfacial polarization is decreased and results in lower εr and tan[thin space (1/6-em)]δ.87
image file: c9ra10916a-f4.tif
Fig. 4 Dielectric properties of CNF/BTO nanocomposite films. The influence of frequency and filler content on the (a) dielectric constant, (b) dielectric loss, and (c) AC conductivity (d) PE hysteresis curves of CNF/BTO nanocomposites.

In the meantime, εr increases with filler content before 30 wt% and decreases with the further addition of BTO. It can be explained by Tanaka's model, which assumes that the interface of a filler particle consists of three layers: a bonded layer, a bound layer, and a loose layer. Additionally, there is an electric double layer overlapping the above three layers.88 Reducing the particle size of BTO to the nanoscale, as well as increasing BTO loading, offers larger surface areas for interfacial polarization, resulting in an extraordinary increase of both εr and tan[thin space (1/6-em)]δ.72 However, at the same time, the bonded layer and bound layer of the nanoparticles impair the motion of dipoles and leads to a decrease of εr and tan[thin space (1/6-em)]δ. Besides, the response of dipoles and ionic carriers in the loose layer is more complicated. Coincidentally, BTO aggregations started to be seen with a filler content of 30 wt% in FE-SEM images. It can be ascribed to the far-field effect of the double electric layer, which makes the loose layers of neighbored nanoparticles collaborate with each other. On the one hand, the resulted imperfection of heterogeneous structures helps to improve εr and tan[thin space (1/6-em)]δ. On the other hand, the porous structure brought by severe aggregation can dramatically cut down εr and tan[thin space (1/6-em)]δ.

In the higher frequency range of above 100 kHz, εr and tan[thin space (1/6-em)]δ were almost insusceptible to the frequency and remains constant. It illustrates that electronic polarization, atomic polarization, and orientation polarization starts to play a predominant role. In this frequency range, filler content also has no obvious influence on εr and tan[thin space (1/6-em)]δ. The εr of CNF/BTO composite films reaches its maximum value of 188.03 with 30 wt% of BTO, which is more than seven times higher than that of pure CNF, whose εr is 25.24 (at 1 kHz). Meanwhile, the tan[thin space (1/6-em)]δ is only slightly grown from 0.70 to 1.21 (at 1 kHz). The dielectric constant of CNF/BTO composite is competitive with other BTO based composites, whose εr is in the range from 30 to 50,25−30 and cellulose-based composites, whose εr is lower than 135.63,64 However, similar to most of other dielectric composites, higher εr is accompanied with higher tan[thin space (1/6-em)]δ. Therefore, more efforts to decrease the loss tangent is still needed. In general, the outstanding dielectric properties of CNF/BTO nanocomposite film render it a promising candidate for capacitor applications.

To further explore the electric properties of CNF/BTO (30 wt%) nanocomposites, the frequency dependence of AC conductivity (σAC) was tested and compared with pure CNF (as shown in Fig. 4c). The σAC of both samples ascended with the increase of frequency. In the lower frequency range of 40 Hz to 100 kHz, the trend was gradual, while it turned rapidly with the frequency further increased. This phenomenon complies well with Dyre's random free energy barrier model.89 The frequency-dependent property of σAC is related to the hopping of the charge carriers in the localized state and upper states in the conduction band. And this process can be accelerated by higher frequency.11,61 Composite films with 30 wt% BTO exhibited higher σAC than that of pure CNF. It is attributed to its higher crystallinity, as evidenced by XRD patterns. Besides, the integration of BTO in CNF piles up more interfacial areas and charges, resulting in higher σAC. At 1 kHz, the σAC increased from 3.15 × 10−7 S cm−1 for CNF to 1.07 × 10−6 S cm−1 for CNF/BTO (30 wt%).

The polarization–electric field (PE) hysteresis curve is an efficient way to evaluate the energy storage properties. The PE hysteresis curves of pure CNF and the CNF/BTO (30 wt%) were measured, as shown in Fig. 4d. Both remnant polarization (Pr) and saturated polarization (Ps) of CNF/BTO composite films were higher than that of pure CNF. It demonstrates that the addition of BTO makes it easier to be polarized, which is also proved by the results that CNF/BTO composite has a higher εr than that of pure CNF. However, the Pr of the composite film was very close to Ps, suggesting a low efficiency of energy storage.11 The polarization of CNF/BTO film saturated before the electric field reached its maximum value. It may be caused by the leakage current which is the result of a heterogeneous structure. In order to be utilized in the area of energy storage application, more efforts should be made on improving the dispersion of BTO fillers and reducing the remnant polarization.

Influence of twisting treatments

In order to study the potential of this high dielectric film as a soft electronic material, the dielectric properties of CNF/BTO (30 wt%) nanocomposite after being repeatedly twisted into a roll (CNF/BTO-R) and ball (CNF/BTO-B) for 10 times, and their dielectric properties were measured again, as shown in Fig. 5. Though both the εr and tan[thin space (1/6-em)]δ decreased after the rolling treatment. The εr for untreated CNF/BTO, CNF/BTO-R, and CNF/BTO-B are 129.56, 90.58, and 43.44, respectively, while the tan[thin space (1/6-em)]δ are 1.07, 0.65, and 0.51, respectively. The CNF/BTO-B films exhibited lower εr and tan[thin space (1/6-em)]δ than that of CNF/BTO-R, which might be caused by more air being entrapped in the film during the twisting or rolling process. This was proved by the observation of the rougher surface and higher thickness (by ∼5%) of CNF/BTO-B. It is worth to note that the rolled CNF/BTO-B films still showed higher dielectric properties compared with other reported composites.42 And at high frequency, the difference of εr and tan[thin space (1/6-em)]δ between these samples are much smaller, which suggests the possibility of the flexible CNF/BTO film to be utilized in the high-frequency applications such as antenna.
image file: c9ra10916a-f5.tif
Fig. 5 The influences of rolling treatments on (a) dielectric constant and (b) loss tangent of CNF/BTO nanocomposite films.

Thermal stability

In practical application, thermal stability is one of the most important concerns. The TGA-DSC curve of CNF/BTO (30 wt%) composite film was measured, as depicted in Fig. 6. Two steps were presented in the degradation process. The first degradation step is the slight weight loss before 100 °C, resulting from the evaporation of moisture.42 The temperature at 5.0% weight loss (T5%) is considered as the start signal of degradation. CNF/BTO (30 wt%) nanocomposite has a T5% of 284 °C, which is slightly higher than that of pure CNF (265 °C, Fig. SI 7). It means that the doping of BTO makes an improvement in thermal stability. The second degradation step located in the temperature range from 250 °C to 400 °C, where there is a drastic drop of weight, combined with a DTG peak at 340 °C and a DSC endothermal peak at 325 °C. This dramatic drop is due to the decomposition of CNF.
image file: c9ra10916a-f6.tif
Fig. 6 TGA-DSC curves of CNF/BTO (30 wt%) nanocomposite film.

Conclusions

A series of high dielectric nanocomposite films based on zero-dimensional tetragonal BTO and three-dimensional CNF were prepared by casting method in aqueous solution. No organic solvents were involved during the preparation, which illustrates the environmental friendliness of the composites. BTO had good distribution within the CNF matrix in the lower range of filler content. The high amount of BTO particles resulted in a porous structure, which led to the drop of dielectric constant. The εr of CNF/BTO composite films reached its maximum value of 188.03 with 30 wt% of BTO, which was more than seven times higher than that of pure CNF, whose εr was 25.24 (at 1 kHz). Meanwhile, the tan[thin space (1/6-em)]δ was only slightly grown from 0.70 to 1.21 (at 1 kHz). The thin film keeps its dielectric properties on an acceptable level even after the twisting treatments. The presence of BTO helps to improve the thermal stability of the composite films. More efforts still need to be made to cut down the remanent polarization and improve the compatibility between the BTO filler and CNF matrix. However, the excellent properties of CNF/BTO composite film demonstrate its great potential to be utilized as a green candidate for HDMs in the field of energy storage.

Conflicts of interest

There are no conflicts to declare.

Acknowledgements

The authors acknowledge assistance from the Analytical and Testing Center of Wuhan University for XRD measurements.

References

  1. G. Manika and G. Psarras, eXPRESS Polym. Lett., 2019, 13, 749–758 CrossRef CAS.
  2. K. Bormanis, A. Kalvane, A. Burkhanov, L. Eglite and R. Dikov, Ferroelectrics, 2019, 538, 12–19 CrossRef CAS.
  3. Y. Jiao, L. Deng, S. Yang and P. Zhang, J. Appl. Polym. Sci., 2019, 136, 47254 CrossRef.
  4. L. Hu, J. Zhong, Y. Tian, X. Zheng, J. Cheng and Z. Pu, J. Mater. Sci.: Mater. Electron., 2019, 30, 221–229 CrossRef CAS.
  5. X. Zhang, Y. Wang, Y. Sheng, H. Ye, L. Xu and H. Wu, Chem. Phys. Lett., 2019, 723, 89–95 CrossRef CAS.
  6. M. Panda, A. Mishra and P. Shukla, SN Appl. Sci., 2019, 1, 230 CrossRef.
  7. P. Beena and H. Jayanna, Polym. Polym. Compos., 2019, 27, 619–625 CAS.
  8. T. Sebastian, A. Michalek, M. Hedayati, T. Lusiola and F. Clemens, J. Eur. Ceram. Soc., 2019, 39, 3716–3721 CrossRef CAS.
  9. W. Li, M. Chen, Y. Yang, D. Yuan, Y. Ren and X. Cai, J. Appl. Polym. Sci., 2019, 136, 47447 CrossRef.
  10. M. D. Waugh, Electron. Eng. Times, 2010, 34–36 Search PubMed.
  11. M. L. Hassan, A. F. Ali, A. H. Salama and A. M. Abdel-Karim, J. Phys. Org. Chem., 2019, 32, e3897 CrossRef.
  12. L. Zhang, Y. Wang, M. Xu, W. Wei and Y. Deng, ACS Appl. Energy Mater., 2019, 2, 5945–5953 CrossRef CAS.
  13. J. Fu, Y. Hou, M. Zheng and M. Zhu, J. Mater. Sci., 2018, 53, 7233–7248 CrossRef CAS.
  14. J. Fu, Y. Hou, M. Zheng, Q. Wei, M. Zhu and H. Yan, ACS Appl. Mater. Interfaces, 2015, 7, 24480–24491 CrossRef CAS PubMed.
  15. P. Hu, Y. Shen, Y. Guan, X. Zhang, Y. Lin, Q. Zhang and C. W. Nan, Adv. Funct. Mater., 2014, 24, 3172–3178 CrossRef CAS.
  16. X. Zhang, J. Jiang, Z. Shen, Z. Dan, M. Li, Y. Lin, C. W. Nan, L. Chen and Y. Shen, Adv. Mater., 2018, 30, 1707269 CrossRef PubMed.
  17. C. Nawanil, W. Makcharoen, K. Khaosa-Ard, T. Maluangnont, W. Vittayakorn, D. Isarakorn and N. Vittayakorn, Integr. Ferroelectr., 2019, 195, 46–57 CrossRef CAS.
  18. B. Jiang, J. Iocozzia, L. Zhao, H. Zhang, Y.-W. Harn, Y. Chen and Z. Lin, Chem. Soc. Rev., 2019, 48, 1194–1228 RSC.
  19. R. Popielarz, C. Chiang, R. Nozaki and J. Obrzut, Macromolecules, 2001, 34, 5910–5915 CrossRef CAS.
  20. L. Gao, Q. Liu, Z. Gao and Y. Lin, Polym. Compos., 2008, 29, 1160–1164 CrossRef CAS.
  21. Z. Li, L. A. Fredin, P. Tewari, S. A. DiBenedetto, M. T. Lanagan, M. A. Ratner and T. J. Marks, Chem. Mater., 2010, 22, 5154–5164 CrossRef CAS.
  22. P. Saini, M. Arora, G. Gupta, B. K. Gupta, V. N. Singh and V. Choudhary, Nanoscale, 2013, 5, 4330–4336 RSC.
  23. Q. Li, K. Han, M. R. Gadinski, G. Zhang and Q. Wang, Adv. Mater., 2014, 26, 6244–6249 CrossRef CAS PubMed.
  24. X. Zhang, Y. Shen, Q. Zhang, L. Gu, Y. Hu, J. Du, Y. Lin and C. W. Nan, Adv. Mater., 2015, 27, 819–824 CrossRef CAS PubMed.
  25. Z.-M. Dang, H.-Y. Wang and H.-P. Xu, Appl. Phys. Lett., 2006, 89, 112902 CrossRef.
  26. Z. M. Dang, Y. Q. Lin, H. P. Xu, C. Y. Shi, S. T. Li and J. Bai, Adv. Funct. Mater., 2008, 18, 1509–1517 CrossRef CAS.
  27. J. Li, J. Claude, L. E. Norena-Franco, S. I. Seok and Q. Wang, Chem. Mater., 2008, 20, 6304–6306 CrossRef CAS.
  28. P. Kim, N. M. Doss, J. P. Tillotson, P. J. Hotchkiss, M.-J. Pan, S. R. Marder, J. Li, J. P. Calame and J. W. Perry, ACS Nano, 2009, 3, 2581–2592 CrossRef CAS PubMed.
  29. K. Yang, X. Huang, Y. Huang, L. Xie and P. Jiang, Chem. Mater., 2013, 25, 2327–2338 CrossRef CAS.
  30. P. Kim, S. C. Jones, P. J. Hotchkiss, J. N. Haddock, B. Kippelen, S. R. Marder and J. W. Perry, Adv. Mater., 2007, 19, 1001–1005 CrossRef CAS.
  31. S. Luo, Y. Shen, S. Yu, Y. Wan, W.-H. Liao, R. Sun and C.-P. Wong, Energy Environ. Sci., 2017, 10, 137–144 RSC.
  32. Y. Wang, J. Cui, Q. Yuan, Y. Niu, Y. Bai and H. Wang, Adv. Mater., 2015, 27, 6658–6663 CrossRef CAS PubMed.
  33. Q. Chen, Y. Shen, S. Zhang and Q. Zhang, Annu. Rev. Mater. Res., 2015, 45, 433–458 CrossRef CAS.
  34. X. Huang and P. Jiang, Adv. Mater., 2015, 27, 546–554 CrossRef CAS PubMed.
  35. T. V. Prateek and R. Gupta, Chem. Rev., 2016, 116, 4260–4317 CrossRef PubMed.
  36. X. Zhang, Y. Shen, B. Xu, Q. Zhang, L. Gu, J. Jiang, J. Ma, Y. Lin and C. W. Nan, Adv. Mater., 2016, 28, 2055–2061 CrossRef CAS PubMed.
  37. Y. Hao, X. Wang, K. Bi, J. Zhang, Y. Huang, L. Wu, P. Zhao, K. Xu, M. Lei and L. Li, Nano Energy, 2017, 31, 49–56 CrossRef CAS.
  38. Z. Pan, L. Yao, J. Zhai, D. Fu, B. Shen and H. Wang, ACS Appl. Mater. Interfaces, 2017, 9, 4024–4033 CrossRef CAS PubMed.
  39. E. D. Cranston and D. G. Gray, Biomacromolecules, 2006, 7, 2522–2530 CrossRef CAS PubMed.
  40. R. J. Moon, G. T. Schueneman and J. Simonsen, JOM, 2016, 68, 2383–2394 CrossRef CAS.
  41. W. Yang, L. Jiao, W. Liu and H. Dai, Nanomaterials, 2019, 9, 107 CrossRef PubMed.
  42. J. Tao, S.-a. Cao, W. Liu and Y. Deng, Cellulose, 2019, 26, 6087–6098 CrossRef CAS.
  43. N. Madusanka, S. G. Shivareddy, M. D. Eddleston, P. Hiralal, R. A. Oliver and G. A. Amaratunga, Carbohydr. Polym., 2017, 172, 315–321 CrossRef CAS PubMed.
  44. H. Y. Choi and Y. G. Jeong, Compos. B Eng., 2019, 168, 58–65 CrossRef CAS.
  45. A. El Sayed and S. El-Gamal, J. Polym. Res., 2015, 22, 97 CrossRef.
  46. S. K. Mahadeva, K. Walus and B. Stoeber, ACS Appl. Mater. Interfaces, 2014, 6, 7547–7553 CrossRef CAS PubMed.
  47. X. L. Zeng, L. B. Deng, Y. M. Yao, R. Sun, J. B. Xu and C. P. Wong, J. Mater. Chem. C, 2016, 4, 6037–6044 RSC.
  48. Y. B. Pottathara, V. Bobnar, M. Finšgar, Y. Grohens, S. Thomas and V. Kokol, Polymer, 2018, 147, 260–270 CrossRef CAS.
  49. Y. Pottathara, S. Thomas, N. Kalarikkal, T. Griesser, Y. Grohens, V. Bobnar, M. Finšgar, V. Kokol and R. Kargl, New J. Chem., 2019, 43, 681–688 RSC.
  50. M. Mohiuddin, K. K. Sadasivuni, S. Mun and J. Kim, RSC Adv., 2015, 5, 34432–34438 RSC.
  51. Y. Beeran, V. Bobnar, S. Gorgieva, Y. Grohens, M. Finšgar, S. Thomas and V. Kokol, RSC Adv., 2016, 6, 49138–49149 RSC.
  52. T. Inui, H. Koga, M. Nogi, N. Komoda and K. Suganuma, Proceedings of the 14th IEEE International Conference on Nanotechnology, Toronto, Canada, 2014 Search PubMed.
  53. S. Ji, J. Jang, E. Cho, S. H. Kim, E. S. Kang, J. Kim, H. K. Kim, H. Kong, S. K. Kim and J. Y. Kim, Adv. Mater., 2017, 29, 1700538 CrossRef PubMed.
  54. S. D. Milovidova, O. V. Rogazinskaya, A. S. Sidorkin, N. H. Thuong, E. V. Grohotova and N. G. Popravko, Ferroelectrics, 2014, 469, 116–119 CrossRef CAS.
  55. K. T. Nguen, S. Milovidova, A. Sidorkin and O. Rogazinskaya, Phys. Solid State, 2015, 57, 503–506 CrossRef CAS.
  56. H. Nguyen, A. Sidorkin, S. Milovidova and O. Rogazinskaya, Ferroelectrics, 2016, 501, 180–186 CrossRef CAS.
  57. H. Nguyen, A. Sidorkin, S. Milovidova and O. Rogazinskaya, Ferroelectrics, 2016, 498, 27–35 CrossRef CAS.
  58. D. Y. Liu, G. Sui and D. Bhattacharyya, Compos. Sci. Technol., 2014, 99, 31–36 CrossRef CAS.
  59. C. Yang, C. Chen, Y. Pan, S. Li, F. Wang, J. Li, N. Li, X. Li, Y. Zhang and D. Li, Electrochim. Acta, 2015, 182, 264–271 CrossRef CAS.
  60. V. Anju and S. K. Narayanankutty, AIP Adv., 2016, 6, 015109 CrossRef.
  61. S. P. Raghunathan, S. Narayanan, A. C. Poulose and R. Joseph, Carbohydr. Polym., 2017, 157, 1024–1032 CrossRef CAS PubMed.
  62. A. Kafy, K. K. Sadasivuni, H. C. Kim, A. Akther and J. Kim, Phys. Chem. Chem. Phys., 2015, 17, 5923–5931 RSC.
  63. C. Chiang and R. Popielarz, Ferroelectrics, 2002, 275, 1–9 CrossRef CAS.
  64. C. Jia, Z. Shao, H. Fan and J. Wang, RSC Adv., 2015, 5, 15283–15291 RSC.
  65. M. Nogi, S. Iwamoto, A. N. Nakagaito and H. Yano, Adv. Mater., 2009, 21, 1595–1598 CrossRef CAS.
  66. D. Klemm, F. Kramer, S. Moritz, T. Lindstrom, M. Ankerfors, D. Gray and A. Dorris, Angew. Chem., Int. Ed. Engl., 2011, 50, 5438–5466 CrossRef CAS PubMed.
  67. B. Poyraz, A. Tozluoğlu, Z. Candan and A. Demir, J. Polym. Eng., 2017, 37, 921–931 CAS.
  68. Y. Fujisaki, H. Koga, Y. Nakajima, M. Nakata, H. Tsuji, T. Yamamoto, T. Kurita, M. Nogi and N. Shimidzu, Adv. Funct. Mater., 2014, 24, 1657–1663 CrossRef CAS.
  69. X. Du, Z. Zhang, W. Liu and Y. Deng, Nano Energy, 2017, 35, 299–320 CrossRef CAS.
  70. A. M. Abdel-karim, A. H. Salama and M. L. Hassan, J. Phys. Org. Chem., 2018, 31, e3851 CrossRef.
  71. U. Celano, K. Nagashima, H. Koga, M. Nogi, F. Zhuge, G. Meng, Y. He, J. De Boeck, M. Jurczak and W. Vandervorst, NPG Asia Mater., 2016, 8, e310 CrossRef CAS.
  72. A. Kafy, K. K. Sadasivuni, A. Akther, S.-K. Min and J. Kim, Mater. Lett., 2015, 159, 20–23 CrossRef CAS.
  73. Y. Li, M. Misra and S. Gregori, IET Circuits, Devices Syst., 2017, 11, 638–647 CrossRef.
  74. A. Petritz, A. Wolfberger, A. Fian, T. Griesser, M. Irimia-Vladu and B. Stadlober, Adv. Mater., 2015, 27, 7645–7656 CrossRef CAS PubMed.
  75. Z. Lu, W. Hu, F. Xie and Y. Hao, Cellulose, 2017, 24, 2827–2835 CrossRef CAS.
  76. X. An, D. Cheng, L. Dai, B. Wang, H. J. Ocampo, J. Nasrallah, X. Jia, J. Zou, Y. Long and Y. Ni, Appl. Catal. B Environ., 2017, 206, 53–64 CrossRef CAS.
  77. H. Lu, L. Zhang, B. Wang, Y. Long, M. Zhang, J. Ma, A. Khan, S. P. Chowdhury, X. Zhou and Y. Ni, Cellulose, 2019, 26, 4909–4920 CrossRef CAS.
  78. Y. Zhao, W. Dang, L. Si and Z. Lu, Cellulose, 2019, 26, 2035–2046 CrossRef CAS.
  79. A. F. Ali, M. L. Hassan, A. A. Ward and E. M. El-Giar, Polym. Compos., 2017, 38, 893–907 CrossRef CAS.
  80. S. Kamel, A. A. Haroun, A. M. El-Nahrawy and M. A. Diab, J. Renewable Mater., 2019, 7, 193–203 Search PubMed.
  81. H. Xu and L. Gao, J. Am. Ceram. Soc., 2003, 86, 203–205 CrossRef CAS.
  82. F.-S. Yen, H.-I. Hsiang and Y.-H. Chang, Jpn. J. Appl. Phys., 1995, 34, 6149 CrossRef CAS.
  83. C. Jia, Z. Shao, H. Fan, R. Feng, F. Wang, W. Wang, J. Wang, D. Zhang and Y. Lv, Composites, Part A, 2016, 86, 1–8 CrossRef CAS.
  84. S. Emmert, M. Wolf, R. Gulich, S. Krohns, S. Kastner, P. Lunkenheimer and A. Loidl, Eur. Phys. J. B, 2011, 83, 157–165 CrossRef CAS.
  85. H. B. Lu and X. Y. Zhang, J. Appl. Phys., 2006, 100, 054104 CrossRef.
  86. M. Samet, V. Levchenko, G. Boiteux, G. Seytre, A. Kallel and A. Serghei, J. Chem. Phys., 2015, 142, 194703 CrossRef CAS PubMed.
  87. M. Abutalib, Phys. B, 2019, 557, 108–116 CrossRef CAS.
  88. T. Tanaka, M. Kozako, N. Fuse and Y. Ohki, IEEE Trans. Dielectr. Electr. Insul., 2005, 12, 669–681 CrossRef CAS.
  89. M. Beztout, A. Boukerrou, H. Djidjelli, C. Barres and F. Fenouillot, Cellul. Chem. Technol., 2015, 49, 517–528 CAS.

Footnote

Electronic supplementary information (ESI) available. See DOI: 10.1039/c9ra10916a

This journal is © The Royal Society of Chemistry 2020