Top Khac Le†
ab,
The-Hung Mai†c,
Muhammad Aamir Iqbald,
Dimitra Vernardoue,
Van-Duong Daof,
Vinoth Kumar Ponnusamy*ghi,
Chandra Sekhar Rout*j and
Phuong V. Pham*c
aFaculty of Materials Science and Technology, University of Science, Ho Chi Minh City 700000, Vietnam
bVietnam National University, Ho Chi Minh City 700000, Vietnam
cDepartment of Physics, National Sun Yat-sen University, Kaohsiung 80424, Taiwan. E-mail: phuongpham@mail.nsysu.edu.tw
dSchool of Materials Science and Engineering, Zhejiang University, Hangzhou 310027, China
eDepartment of Electrical and Computer Engineering, School of Engineering, Hellenic Mediterranean University, Heraklion 71410, Greece
fFaculty of Biotechnology, Chemistry, and Environmental Engineering, Phenikaa University, Hanoi 100000, Vietnam
gDepartment of Medicinal and Applied Chemistry and Research Center for Precision Environmental Medicine, Kaohsiung Medical University, Kaohsiung 807, Taiwan. E-mail: kumar@kmu.edu.tw
hDepartment of Medical Research, Kaohsiung Medical University Hospital, Kaohsiung 807, Taiwan
iDepartment of Chemistry, National Sun Yat-sen University, Kaohsiung 80424, Taiwan
jCentre for Nano and Material Sciences, Jain University, Bangalore 562112, India. E-mail: r.chandrasekhar@jainuniversity.ac.in
First published on 27th October 2023
Graphene has garnered increasing attention for solar energy harvesting owing to its unique features. However, limitations hinder its widespread adoption in solar energy harvesting, comprising the band gapless in the molecular orbital of graphene lattice, its vulnerability to oxidation in oxidative environments, and specific toxic properties that require careful consideration during development. Beyond current challenges, researchers have explored doping graphene with ionic liquids to raise the lifespan of solar cells (SCs). Additionally, they have paid attention to optimizing graphene/Si Schottky junction or Schottky barrier SCs by enhancing the conductivity and work function of graphene, improving silicon's reflectivity, and addressing passivation issues at the surface/interface of graphene/Si, resulting in significant advancements in their power conversion efficiency. Increasing the functional area of graphene-based SCs and designing efficient grid electrodes are also crucial for enhancing carrier collection efficiency. Flaws and contaminants present at the interface between graphene and silicon pose significant challenges. Despite the progress of graphene/Si-based photovoltaic cells still needs to catch up to the efficiency achieved by commercially available Si p–n junction SCs. The low Schottky barrier height, design-related challenges associated with transfer techniques, and high lateral resistivity of graphene contribute to this performance gap. To maximize the effectiveness and robustness of graphene/Si-based photovoltaic cells, appropriate interlayers have been utilized to tune the interface and modulate graphene's functionality. This mini-review will address ongoing research and development endeavors using van der Waals graphene heterojunctions, aiming to overcome the existing limitations and unlock graphene's full potential in solar energy harvesting and smart storage systems.
However, the classification of SCs is organized into three categories of generations.1 The first category comprises single- and poly-crystalline Si, which boast the highest efficiency level (26.6%).2 The next classification refers to SCs that employ a cadmium telluride thin film (CdTe) and copper indium gallium selenide (CIGS) with the highest reported performance (23.35%).3 Including various sub-categories, the third category involves the SCs based on newly found materials and has been widely explored to enhance the efficiency of SCs.4 In addition, SCs using 2D materials e.g., MoS2, WSe2, and graphene are classified in a diverse category.5–9 Currently, research and development (R&D) as along with commercialization activities of Si-based SCs are mostly directed in enhancing the power conversion efficiency (PCE) while reducing manufacturing expenses.10 Interestingly, graphene has been found to be a promising candidate to revolutionize the SC market. Extensive studies have examined the integration of graphene into Si PV technology, motivated by the extraordinary physical properties of graphene. These attributes encompass exceptional electrical conductivity, carrier mobility, thermal conductivity, mechanical flexibility, stability, and dominant transmittance (97.7% monolayer graphene in visible region).11–13 Thus, the R&D efforts focused on incorporating graphene into devices used for SCs have rapidly progressed, resulting in high PCEs exceeding 15% in copious distinguished applications. Several works associated with incorporating of graphene into PVs for numerous vital roles, such as the active layer and electrode, have been reported.14–16
One crucial challenge in creating high-performance SCs for energy harvesting and practical implementations is the efficient generation/separation of paired electron–hole from photo-induced processes, followed by the effective transfer of these separated charge carriers to the electrodes. In this context, graphene revealed significant improvement. Consequently, research has been performed to explore and evaluate the graphene/Si Schottky junction (G/S-SJ) device for various applications utilizing the internal photoemission process. Hence, SCs that utilize a SJ, with graphene acting as a metal and Si as a semiconductor, have been duly recognized as a suitable example of Schottky junction devices (SJDs).17
In this review, the emergence of G/S SB-SCs and PVs concerns are exhibited in relation to the extensive endeavors to enhance the performance of low-cost SCs. The charge transport mechanism in G/S SB-SCs is elucidated, along with several approaches that facilitate the optimization of such devices for PCE to explore the further mechanism principle of the heterostructured devices. Additionally, the difficulties and potential opportunities associated with G/Si SB-SCs in the field of PV technology are discussed, with the aim of paving the way for the design of next-generation solar energy harvesting systems.
Owing to its physical/chemical/mechanical features, graphene-based heterojunction SCs exhibited an good efficiency (18.5%) when combined with GaAs structure.58 After achieving positive results in research and development trials, a feasible manufacturing process for small-scale commercial production of thin-film and dye-sensitized photo-supercapacitors using graphene has been effectively developed and implemented.59–61 However, large-scale manufacturing of these SC types remains challenging to date. SB-SCs, which are made using the method of direct deposition of a transparency electrode or thin film of metal on a moderately doped semiconductor wafer, have gained significant attention in PVs.62 They have advantages over traditional p–n junction SCs in terms of being inexpensive and simple to manufacture.63 Nevertheless, conventional SB-SCs require a thick metal layer that hinders solar radiation absorption. Thus, ITO has been explored as an alternative, but its limited resources and fragile nature limit its application in flexible devices. To overcome these challenges, graphene sheets have been successfully employed in SB-SCs, permitting the production of cost-effective, flexible solar panels with excellent environmental stability, eco-friendliness, and efficiency exceeding 10%. The demand for flexible SCs in various applications including wearable/implantable microsystems and wireless sensor networks for IoT, makes G/Si SB-SCs highly attractive for the PVs market.
Recently, the vehement efforts have been proceeded to develop new-generation G/Si SB-SCs, with a signify attention on chemical doping techniques to achieve high Schottky barrier height and efficiency. However, the chemical-doped G/Si SCs often exhibit rapid degradation due to the oxidative nature of the dopants. An alternative promising strategy is being explored to develop the chemical-doping-free G/Si SCs, which exhibit stability over several months. Regrettably, the effectiveness of these SCs is limited due to the high electrical resistance of graphene films and the low Schottky barrier of the G/Si heterojunction. Recently researches show that the PCE of G/Si SCs has been enhanced by doping technique with PbS quantum dots64 and electrical-field doping with a liquid gate circuit.65 Chemical doping into the graphene can generate more acceptor carriers and improve conductivity. However, they have limitations including significant light loss and the instability of the integrated liquid medium that prevent them from being used in practice.66
On the other hand, doping effects caused by solid interactions have been documented in graphene-assisted heterojunctions e.g., MoF6/graphene67,68 and MoO3/graphene.69 This advancement's lack of chemical reactions offers a promising approach for achieving steady graphene doping. From this perspective, a study was conducted to explore the interactions in graphene/fluorographene heterostructures, targeting to improve the output of G/Si SCs. Interestingly, fluorographene is a novel derivative of graphene that features dipoles created by C–F bonds in graphite, making it one of the thinnest known insulators. It is made by revealing graphene to fluoride gases, and its electrical features are adjusted via its C/F ratio.68 Simulated studies have demonstrated the interactions between graphene with other 2D materials (graphene and MoS2). Notably, the F atoms present in fluorographene function as receptors of electrons, leading to the transfer of charge-coupled 2D elements onto fluorographene and potentially causing p-type doping. Density functional theory (DFT) was employed to examine the optical characteristics of graphene hexagonal boron nitride (h-BN) and fluorographene.70 Fluorographene exhibits exceptional capability in decoupling graphene from the substrate. These distinctive properties make fluorographene an attractive option for optimizing G/Si SCs.
The pioneering study by Zhu et al. in 2010 explored the feasibility of G/n-Si SB-SCs achieving an efficiency of 1.65%.48 G/Si SB-SCs hold promise for effectively separating charge carriers due to their substantial built-in potential. Graphene holds a key role for the efficiency of these SCs because it acts as both active layer and transparent electrode.71,72 This requires the graphene to exhibit more physical properties such as good photo-generated charge carriers, high electron mobiles safely electron transport. In less than 10 years, G/Si SB-SCs achieved up to 15% efficiency due to the 100 times greater than (approximately 2.5 × 105 cm2 V−1 s−1) of electron mobility comparing Si substrate.73 Graphene, being a zero-band-gap semiconductor, exhibits the remarkable ability to absorb light across a broad spectrum. Moreover, electrons within graphene can traverse several micrometers without scattering, showcasing its exceptional transport characteristics.74 SCs using graphene such as hole transporter based on G/Si structure were first created by depositing a graphene thin film on Si surface.48 However, the graphene layer exhibited higher sheet resistance (a few kΩ), negatively affecting its conductivity. Consequently, it impeded the flow of photo-generated current in G/Si SCs, leading to an extraordinary reduction in their PCE. Initially, researchers explored the chemical doping on a top graphene surface, which involved the introduction of a p-type dopant into the graphene material. However, HNO3 and bis-(trifluoromethane sulfonyl)amide (TFSA) are the most widely utilized dopants in G/Si SCs.75,76 By introducing a TFSA layer, the highest reported increase in efficiency (1.9% to 8.6%) of G/Si SCs with the use of doping was achieved. Also, several other dopants, such as boron doping77 and doping with chemicals such as SOCl2, HNO3, HCl, and H2O2 were introduced by various research groups.75,78 Coating the top surface of graphene with a dopant proved highly effective in reducing its resistance. However, despite the benefits of chemical doping, a significant limitation is its unsteadiness in the atmospheric media, leading to surface deterioration and eventually restoring the cell's efficiency to its initial value. For this reason, graphene oxide (GO) and Pt nanoparticles (NPs) have been recognized as suitable dopants for the top surface of G/Si SCs.79,80 In G/Si SCs, a transparent MoO3/Ag/MoO3 heterojunction layer over graphene was applied, resulting in an increased ϕwf, reduced series resistance, and improved efficiency (0.86 to 3.5%) of graphene.69 Bhopal et al.81 reported an increase in efficiency from 4.3 to 5.01% in G/Si SCs using an Ag/Ni electrode to decrease the contact resistivity. NiO-induced doping in G/Si SCs was employed to lower the series resistance, enhance the SJ quality as well as improve cell robustness.82 In particular, effect contact of metallization front electrodes provides a direct electrical contact between graphene layer and the Si substrate. This low-resistance contact improves charge carrier extraction and reduces series resistance, leading to enhanced solar cells performance. Moreover, the process of depositing a metal layer onto the front surface of solar cells is well-established and relatively straightforward. Common deposition techniques like sputtering or evaporation are widely used for this purpose. While the efficiency of solar cells through the using the chemical induced doping could also be improved by enhanced carrier mobility and tunable properties. NiO is a prime example for the doping method, which can significantly promote the mobility of charge carriers. Besides, NiO doping can mitigate carrier recombination at the graphene/Si interface. By reducing recombination, the efficiency of charge carrier extraction and collection increases, leading to higher overall solar cells performance. Nevertheless, the limitations of these two methods still exist, and affects to quality of energy conversion. Typically, the controllable thickness and shape of electrodes is extremely important, due to the depending on the thickness and layout of the metal front electrode, there is a possibility of shading some of the active solar cell area, which can decrease efficiency, or in the doping method, achieving uniform doping across the entire solar cells area can be challenging, and any non-uniformity might lead to performance variations. Additionally, the stability of the NiO-doped layer and its interaction with other materials need to be accessed for potential degradation over time, which could impact long-term performance of the solar cells. Therefore, choosing the appropriate method will depend on factors such as the specific cell design, the level of performance enhanced desired, fabrication complexity, material compatibility. Furthermore, ongoing research may lead to improvements and refinements in these methods over time.
Fig. 2 (a) Design of G/n-Si SC, a layer of graphene was applied onto SiO2/Si substrate, forming a junction. (a) has been reproduced from ref. 73 with permission from American Chemical Society. (b) Energy band diagram in G/n-Si SB-SCs and the displacement of electron–hole pairs. (b) has been reproduced from ref. 83 with permission from Wiley-VCH. (c) A visual representation depicting the uncomplicated creation of a G/Si SB-SCs through a heterojunction structure is shown. This process involves three key factors: interfacial layer, chemical doping, and ARC coating. These factors collectively contribute to improving efficiency and prolonging the durability of G/Si SCs. (c) reproduced from ref. 84 with permission from Royal Society of Chemistry. |
(1) |
(2) |
Electron/holes at regions of G/Si junction as light illuminated will generate the photovoltage (V) and it reaches maximum value in open-circuit voltage (VOC). As SC short-circuited, photogenerated carriers flow through the external circuit, resulting in a maximum current called ISC. Nevertheless, in practical use, SCs function within a range that lies between a short-circuit condition and an open-circuit condition. Due to the rectifying characteristics and non-linear voltage–current behavior of the G/Si junction, a maximum output power (Pmax) can be achieved.
PCE of the G/Si SCs quantifies the extent to which sunlight energy is changed into electricity. It can be conveyed using eqn (3).
(3) |
(4) |
External quantum efficiency (EQE) is characterized as the ratio of charge carriers to incident photons of a specific energy, and its determination can be achieved through the utilization of eqn (5).
(5) |
Internal quantum efficiency (IQE) refers to the count of charge carriers for each absorbed photon within the SC. IQE is evaluated by subtracting the photons lost due to reflection and transmission from the EQE. This connection can be mathematically represented using eqn (6).
(6) |
(7) |
(8) |
Fig. 3a and b displays the J–V curves of G/Si SCs for varying RS and RSH values, respectively.83 It is evident that the FF of the SCs exhibits a significant relationship with sheet resistance of graphene. Reducing the sheet resistance leads to increased FF, indicating that improving graphene's sheet resistance can be accomplished by focusing on high-quality growth, precise transfer, and controlled doping technique. The impact of shunt resistance transforms into relevance only when the resistance decreases below 10 kΩ. Otherwise, it has minimal to minimal results on the efficiency of G/Si SCs regardless of any variation in resistance. Given the provided experimental values for parasitic resistance (Rs = 10.5 Ω, Rsh = 45 MΩ), it can be concluded that the impact of series resistance on efficiency is significantly more detrimental (Fig. 3c).
Fig. 3 Voltage–current characteristics and FF of a theoretical G/Si SCs with various (a) series resistance, (b) sheet resistance. (a) and (b) have been reproduced from ref. 83 with permission from Wiley-VCH. Experimental G/Si SCs with (c) series resistance and sheet resistance, which is estimated from the reverse bias I–V sweep. (c) has been reproduced from ref. 48 with permission from Wiley-VCH. |
Fig. 4 (a) The diagram of band structure and ϕwf of the MLG/Si interface prior to and following the doping process. (b) Raman spectroscopy results showing the spectra of MLG and FLG with and without the presence of Au NPs. (c) Dark J–V curves of the FLG/Si SCs with and without Au NPs. The inset presents the graphs of dV/d(lnJ) versus I, enabling the determination of the series resistance RS of cells. (b)–(d) have been reproduced from ref. 89 with permission from American Institute of Physics. |
Aside from increasing the number of layers, doping has been established as an effective method for reducing the sheet resistance of graphene. Different doping approaches using chemical doping have been successfully utilized. Heteroatom doping involves the substitution or bonding of atoms like oxygen, boron, nitrogen, phosphor, and sulfur, with carbon atoms in the graphene lattice. Nevertheless, dopants are chosen over heteroatom doping for application in G/Si SCs. Amongst different dopants, HNO3, SoCl2, and AuCl3 have shown promising results. Cui et al. found that SoCl2 is the most effective dopant to improve the PCE of SCs to 2.3% due to decreased sheet resistance.75 SoCl2 modified graphene also decreases sheet resistance from 735 to 405 Ω sq−1. Feng et al. with demonstrated a reduction in series resistance (Rs) of the SCs from 6.11 Ω cm2 to 4.07 Ω cm2 and an improvement in PCE from 2.9% to 4.35% after immersing the device in HNO3, along with VOC, JSC, FF enhancement to 495 mV, 17.22 mA cm−2 and 51%, respectively.72,85 Although chemical doping has shown promising results in reducing graphene resistance and SC efficiency, there is concern regarding the durability of the covalent functionalization of graphene. Degradation of the functionalization caused by the ambient air can result in a significant decrease in PV enhancement by up to 50%. However, doping by gold chloride (AuCl3) has demonstrated better environmental stability than other reported methods.86 The reduction of Au3+ to Au NPs by transferring charges from graphene results in p-doping of graphene, leading to substantial enhancements in conductivity. The sheet resistance by AuCl3-dopped MLG results in reducing sheet resistance and enhancing efficiency.73,87
In addition, doping with organic compounds can also improve the physical properties of graphene.90,91 For example, doping with trifluoromethanesulfonic amide (TFSA) resulted in an increase in the PCE of the G/Si device from was increased 1.9% to 8.6%, an increase in the JSC from 14.2 to 25.3 mA cm−2, and an increase in the VOC from 0.43 to 0.54 V, for doped and un-doped graphene, respectively.76 When TFSA is functionalized on monolayer graphene, it has been observed that the resistance decreases from 1200 to 300 Ω cm−2 without notable impact on transmittance. Most of these dopant’s p-dope the graphene, leading to a decrease in the sheet resistance of graphene by shifting the graphene Fermi level downward or increasing the ϕwf. Since graphene also behaves as a junction layer, the increase in the ϕwf has additional implications at the interface. The enhanced graphene ϕwf leads to an elevated SBH, thereby establishing a more robust built-in electric field and more efficient separation of carriers. As depicted in Fig. 4a, the rise in Voc following the doping process enhances the built-in potential Vo and the barrier height (ϕb). This adjustment aligns with the variance of the work function of MLG (ϕG) and the electron affinity of Si (χ).88 Chemical doping raises ϕG, promoting enhanced charge transfer and collection at the interface. Consequently, the enhancement brought about by doping in the G/Si SCs combines improvements in graphene sheet resistance and an elevated Schottky barrier height.
Taking into consideration the instability of chemical doping, it is not practical for the utilization of graphene/Si PV devices. Therefore, more reliable doping techniques are increasingly coveted, and researchers have recently commenced investigating alternative approaches including physical and light-induced doping. Some metals (metal’s EF lower than graphene’s EF) have been found to effectively p-dope graphene. The doping capacity of metal NPs is determined by their ϕwf, with metals possessing higher ϕwf demonstrating more effective graphene doping. Successful p-doping is indicated by a blue shift in the 2D Raman peak upon deposition of Au NPs (Fig. 4b).89 By optimizing the Au NPs size, the PCE of G/Si SCs was increased to 7.34%. Au/HNO3 co-doped graphene increases the efficiency to 10.20% by achieving a raised ϕwf and improved electrical conductivity of graphene. As depicted in Fig. 4c, the reduction in the series RS of Schottky diode, attributed to the introducing of Au NPs, not only results in a heightened FF but also enhanced Jsc.89 This outcome aligns with findings from previous studies on the effects of HNO3 doping. Similarly, the work shows a high efficiency of 10.69% with Au/TFSA co-doped graphene.90 NPs of another metal, Pt, with a high ϕwf, have also been demonstrated to enhance the PCE to 7% through the integration of physical doping using high ϕwf Pt NPs, improved absorption of SCs in the visible region due to plasmonic effect and the photo-induced doping. Approaches to providing holes or electrons to graphene by using P3HT or TiO2 film were used. The suitability of HUMO of P3HT and VB of Si creates favorable conditions for hole transport under light illumination, enhancing carrier concentration. On the other hand, holes were captured by the traps in TiO2 whereas the electrons were moved to graphene.
In addition, prolong stable of SCs play a signify role. TiOx material coated on graphene can remain or reduce the degradation of PCE of SCs. A PCE value of 12.95% was reached, with degradation of less than 10% after 1-month storage by coated TiO2 layer.91 Efficiency levels of 8.2% and 10.5% were achieved for TiOx/G/p-Si without PMMA and with antireflection (AR) coating of PMMA, respectively. Furthermore, no significant changes in performance were observed over a period of 10 days.92 GO is a multi-functional component for G/Si SCs. For example, GO layer functions as p-type dopant for graphene and also acts as an AR layer within SC. PCE of the G/GO/Si CSs maintained a consistent 10% level over a span of 20 days.79 Using GO as a passivation layer led to a significant improvement in the lifetime of carriers.93 Simultaneously, GO also functioned as a protective; however, its barrier characteristics were observed to diminish at elevated temperatures (400 °C) because of GO decomposition and alterations in its doping levels.93
Fig. 5a and b describe the cross-section of Si nanowires of 2 μm and 5 μm.92 The transmittance spectra show that both Si nanowires of 2 μm and 5 μm before etching exhibit low transmittance.92 It is evident that correlated to planar Si, nanowires exhibit decreased transmission indicating strong light trapping. Similarly, in the case of G/Si SCs, texturing Si into structures such as pillars, nanowires, pyramids, etc. has been employed to minimize light reflection and enhance light absorption. These non-planar features redirect the incident light back into the Si rather than allowing it to transmit through the Si, leading to improved absorption through light trapping and subsequently boosting the overall PCE. Fan et al. fabricated Si NWs through metal-assisted etching method.94 The G/Si NWs SJ demonstrated higher absorption contrasted to the graphene/planar Si junction leading to the enhancing efficiency of up to 2.865% because the Si NWs contribute an immediate pathway to the overall improvement in performance due to direct and fast pathway of electron–hole collection as light trapped on the planar junction. Feng et al. implemented the pillar to enhance light absorption using photolithography and inductive coupled plasma (Fig. 6).72 The result implies that the Si pillar exhibits more absorption correlated with planar Si. The absorption intensity is strongly affected by pillar height and achieves the highest absorption with 900 nm pillar height. The PCE of G/Si pillar devices was measured to be 1.96% (which could be further enhanced to 3.55% by HNO3 doping), surpassing that of G/planar-Si SCs (1.65%). Xie et al. prepared the Si hole array (SiHA) using photolithography and reaction ion etching (RIE).95 The surface of SiHA displayed a smooth texture, validating the presence of minimal surface recombination velocity. As illustrated in Fig. 7, the light absorption of SiHA intensified as the depth of the holes increased, underscoring its heightened light-trapping capabilities.94,95 Through the mixture of light trapping in SiHA and the utilization of AuCl3 for graphene doping, researchers achieved a high PCE of 10.40%.94,95 These devices indicated remarkable stability, maintaining their increased efficiency even after being stored in ambient air for about 3 months.
Fig. 5 Tilted cross-sectional SEM images visuals portraying (a) arrays of nanowires measuring 2 μm and (b) arrays of nanowires measuring 5 μm. Scale bars are 10 μm for both images. In addition, (c) transmission spectra of thin Si structures are provided for the comparison: prior to etching (red), subsequent to etching into 2 μm (green), and following etching into 5 μm (black) nanowires. (a)–(c) have been reproduced from ref. 92 with permission from American Chemical Society. |
Fig. 7 (a) Schematics diagrams of G/planar Si, (b) G/Si NW junctions. (a) and (b) have been reproduced from ref. 94 with permission from American Chemical Society. (c) Schematic presentation of the G/Si HA SB-SCs, (d) top-view SEM image of the G/Si HA device. The area included by graphene films shows darker contrast in the SEM image. (e) Top-view and (f) cross-sectional view SEM images of the as-prepared SiHA. Insets present the enlarged SEM images, (g) PV characteristics, and (h) EQE spectra of the G/Si HA SB-SCs with various hole depths. (c)–(h) have been reproduced from ref. 95 with permission from Royal Society of Chemistry. |
Fig. 8 (a) Patterning of the Si substrate, (b) relationship between refractive index and wavelength for certain ARC materials. (a) and (b) have been reproduced from ref. 96 with permission from Royal Society of Chemistry. (c) Light reflection spectra of a g/Si SCs prior to (black) and following (red) the application of a TiO2 colloid coating, illustrating antireflection effect, (d) J–V characteristics of an as-deposited G/Si SCs, after HNO3 vapor doping, and after TiO2 coating (together with HNO3 doping), respectively. (c) and (d) Have been reproduced from ref. 97 with permission from American Chemical Society. (e) Reflectance spectra of PMMA-extracted and PMMA-grown graphene samples on quartz slides, (f) J–V curves of PMMA-removed and PMMA-coated (2000 rpm) G/Si SCs before and after HNO3 doping. (e) and (f) Have been reproduced from ref. 98 with permission from Royal Society of Chemistry. |
Fig. 8f demonstrates the JSC, FF, and PCE of PMMA extracted-G/Si and PMMA-G/Si SCs of 22.61 mA cm−2, 32.22%, 3.12%, and 33.64 mA cm−2, 45.56%, 6.55%, respectively.99 In particular, the PCE of HNO3-doped PMMA-G/Si SCs up to 13.34%. It is noteworthy that the structure of PMMA was not affected by the HNO3 doping, making the doping procedure of PMMA coated graphene convenient. Ding et al.100 utilized double layered MgF2/ZnS coating on G/Si SCs, serving a dual intention. Firstly, for Si SCs operating in the range of 380 to 1100 nm, ZnS and MgF2 have higher (n = 2.5) and lower (n = 1.4) refractive indices, respectively. Therefore, the MgF2/ZnS double layer served as an effective ARC. Secondly, by adjusting the thickness of ZnS and MgF2, different colors could be transmitted to G/Si SCs. The color tuning process for G/Si SCs was easy due to the transparent nature of graphene. Fig. 9 depicts the display, visuals, and CIE chromaticity coordinates of seven colors for G/Si SCs with DL-MgF2/ZnS films.100
Fig. 9 G/Si SB-SCs with (a) schematic presentation of the color device, (b) photographs of device area: 1 cm2 with various colors, and (c) coordinates of seven colors in CIE chromaticity. (a) and (b) Has been reproduced from ref. 99 with permission Elsevier. |
Fig. 10 illustrates the reflectance spectra of different colored MgF2/ZnS coated G/Si SCs.99 It is evident that the absorption was enhanced correlated to pristine G/Si SCs. Comparable trends were seen for the EQE spectra. Remarkably, the multi-color G/Si SCs achieved a high PCE of 10.7–13.2%.99 By utilizing an enhanced MgF2/ZnS antireflection layer, the PCE of the device reached an impressive value of 14.6%.99
Fig. 10 (a) Modeled (dash lines) and observed (solid lines) reflection spectra of DL-MgF2/ZnS-coated G/Si heterojunction SCs (b) EQE spectra of the uncoated and G/Si SCs with various structural colors, (c) J–V spectra of the devices with various structural colors. J–V spectra of the devices without coating and with enhanced anti-reflection coating were also indicated for comparison, (d) contrast of the J–V and EQE (inset) among SL-ZnS-coated and DL-MgF2/ZnS-coated G/Si devices. (a)–(d) Have been reproduced from ref. 99 with permission from Elsevier. |
Recently, the insulating material of h-BN, an appealing choice as a barrier layer for G/Si SCs due to high transparency, dangling bond-free surface, and proper band alignment with n-Si substrate.101 Fig. 11 presents the band diagram of G/h-BN/Si SCs, highlighting the effects of h-BN insertion.101 It's clear that compared to a basic G/Si interface, the introduction h-BN creates a substantial barrier that impedes electron transfer at the interface.102 However, it simultaneously enables easy transport of holes from Si to graphene. Through the incorporation of the BN layer, PCE of the G/Si SCs attained 10.93%, which indicated a 15% efficient enhancement contrasted to the reference device.
Fig. 11 Energy band diagrams of the G/Si SB-SCs (a) without and (b) with an h-BN electron blocking layer. (a) and (b) have been reproduced from ref. 102 with permission from Elsevier Presentations of band diagrams for the SCs. The PV procedures (c) in the graphene/n-Si and (d) in the graphene/MoS2/n-Si SCs are indicated. (c) and d have been reproduced from ref. 101 with permission from Royal Society of Chemistry. |
Semiconductor layers with thickness (∼50 nm) can be employed as barrier layers, offering a more convenient processing approach compared to insulators which require decreased thickness. MoS2 thin film grown by different methods has been utilized as an interfacial barrier layer to improve PCE of SCs. The insertion of MoS2 layer introduces a shift in the EF, causing the lowest part of the CB and the top of VB of the MoS2 layer at the interface of graphene to move upward, as shown in Fig. 11a–d.101 This creates an energy barrier at the interface between MoS2 and n-Si and enhances the entire energy barrier among graphene and n-Si. The additional energy barrier provided by the MoS2 layer effectively blocks the photogenerated electrons in the Si, serving as an efficient electron-blocking layer. Alike band bending at the interface of the semiconductor barrier layer/n-Si interface has been noted in the cause of WO3/n-Si structures.101 The substantial disparity in energy levels between the EF of WO3 and Si prompts a marked transfer of charges from Si, leading to a pronounced upward bending of the band at the interface of WO3 and Si. Consequently, the built-in field (Vbi) of the G/Si SCs is improved inserting the WO3 interlayer, leading to a notable improvement in PCE from 3.99% in G/Si SCs to 10.59%. Utilizing MoO3 layers also contributed to elevating the PCE to 12.2% as a result of the significant ϕwf discrepancy in MoO3, leading to the spontaneous injection of holes from the MoO3 layer to Si.101 As a result of this hole injection process, a hole inversion layer is created at the surface of Si, generating a robust built-in electric field. This process effectively curbs recombination. Through additional device optimization steps involving graphene doping and the application of polymer anti-reflection coating, a high PCE of 12.2% was accomplished.
Organic semiconductors, P3HT also act as a hole transport layer and block the electron to reduce the recombination. Fig. 12 illustrates the band of P3HT and Si that LUMO and HUMO of P3HT are 3.2 and 5.1 eV, while the lowest conduction band and highest valence band are 4.05 and 5.17 eV.106 This substantial offset allows the transport of holes, but it hinders the electrons. Optimized graphene/P3HT/Si NW array and graphene/P3HT/Si NH array devices achieved power conversion efficiencies of 9.94% and 10.34%, respectively.
Fig. 12 Band diagram schematic of hybrid SCs. Figure has been reproduced from ref. 106 with permission from American Chemical Society. |
A significant interaction at the interface between Si and MoO3 layers has been noted, resulting in the remarkable attainment of PCE value of 12.2%. A substantial work ϕwf disparity was observed in MoO3, leading to the spontaneous injection of holes from the MoO3 layer to Si. This hole injection mechanism instigates the formation of a hole inversion layer on the Si surface and triggers the establishment of potent built-in electric field, effectively suppressing the recombination. Through additional device optimization steps involving graphene doping and the application of polymer anti-reflection coating, a high-PCE of 12.2% was accomplished.
With its numerous advantages as a component of an SC, it possesses some limitations that can hinder it from being considered one of the best materials for an efficient SC. Graphene is widely regarded as a pivotal conductor of electricity, but it lacks a band gap in its molecular orbital structure, a shortcoming that researchers have been working to rectify over the years. Once this limitation is overcome, graphene can serve as an exceptionally efficient anode in virtually any type of SCs. Another challenge associated with graphene is its susceptibility to oxidation in oxidative environments. This oxidation leads to structural changes that subsequently impact its chemical properties. Efforts are underway to develop strategies to mitigate the effects of oxidation and enhance graphene's stability. Despite these challenges, researchers are actively working to overcome these limitations and harness the full potential of graphene for SC applications. The chemical alterations and structural changes that can occur in graphene pose a significant challenge when considering large-scale energy production. Moreover, graphene exhibits some toxic properties, which is a matter that requires to be carefully examined in its development. Secondary cells typically have two electrodes, whereas SCs have only one electrode. This creates two main issues: changes in the ϕwf value and the direction of electron flow. The electron flow system in a SC with only one electrode is complex, and maintaining the integrity of the entire process is a significant task. Researchers have attempted to modify the ϕwf to address this challenge but altering the ϕwf of a specific material is a difficult endeavor. Aside from this persisting issue, it has been discovered that depositing graphene electrodes into the solar setup has proven to be a difficult task. The bottom of a graphene electrode is deposited on a substrate material (usually glass or elastomers) that acts as the foundation makes up for the SCs.120 Owing to the poor dispersion properties of graphene, water is used as an appropriate solvent during this deposition process. However, various organic solvents are being tested to replace water in order to achieve a higher degree of dispersion. In typical graphene-induced SCs, when integrated into an n-Si SB-SCs with AM 1.5 illumination, it demonstrates a PCE of 8.6%. This value can be increased 4.5 times when doping the SC material. To achieve this, graphene is doped with ionic liquids such as bistriflimide, bis(trifluoromethanesulfonyl)amide, and others.121–123 The doping process alters the chemical potential of graphene, leading to an increased carrier density, ultimately elevating the built-in potential of the SCs. This, in turn, enables a longer cell lifespan compared to traditional SCs. Recent approaches in optimizing G/Si SB-SCs were developed. These strategies can be divided into optimizing (i) the ϕwf and conductivity of graphene, (ii) Si's reflectivity, and (iii) modifying the G/Si interface. Through the implementation of these strategies, the PCE has risen from 1.5% to 15.8% in less than 10 years. Despite the fast advancements in this area, there are remaining matters that require further attention.
Firstly, various strategies have been explored to improve the PCE of SCs including passivation and band-engineering of the G/Si interface, insertion of an antireflection layer or nano-micro structures in enhancing the light harvest, the control of the number of graphene layers, and the chemical doping of graphene which has been confirmed to be the most efficient method for optimizing SC performance. Despite the introduction of numerous doping dopants, the durability of SCs remains a challenging issue due to the unsteadiness of the doping process. An increased stable single-walled carbon nanotube (SWa-CNT)/Si SCs with a PCE greater than 11% after 10 months of ambient encounter was demonstrated.124 By inserting a GO interlayer to develop a G/Si interface, new structure of G/GO/Si SC occupies 95% of its original level after one week of storage in the open air.125 Similarly, an Al2O3 interlayer was inserted by Rehman et al.115 among the graphene and Si to inhibit the surface charge recombination at the interface, and their SC maintained its efficiency without degradation even after 9 months of exposure to ambient air. Initially, chemical doping of graphene led to a significant deterioration of G/Si SCs. Recently, GO demonstrated some PCE durability where Yavuz et al. published the degradation in PCE less than 1% after 3 weeks.79,126 Nevertheless, more research into the stability under various parameters, such as humidity and temperature, is needed. Moreover, alternative materials such as a CNT-oxide-Si cell with a PDMS anti-reflective coating were employed to reveal a small drop in efficiency from 10.9% to 9.1% in air over 20 days. Thus, materials with high durability, like CNTs, can be utilized to ensure the stability of a SC. Investigating new SC structures, such as introducing an interlayer to engineer G/Si interface to create a metal–insulator–semiconductor (MIS) structure, could also be a vital direction in this field.
Secondly, although the PCE of G/Si SCs managed 15.8% in a few years, it still falls short of the PCE achieved by commercially available Si–p–n junction SCs. One of the limitations contributing to this is the decreased electrical conductivity and ϕwf of graphene. As a result, the energetic region of current studies involving G/Si SCs is relatively small (<10 mm2). Researchers demonstrated the device performance in various device areas from 4 to 100 mm2. Interestingly, the PCE decreased from 10.56% to 3.62%, with an increase in the device area. This reduction in efficiency can be attributed to series resistance, which influences performance of SCs at larger scales. This result underscores the direct relationship between the energetic region of a SC and its overall behavior.127 Furthermore, it has been reported in another study that the PCE of G/Si SCs lowered from 14.5% to 10.6% as the active region raised from 4.7 mm2 to 14.5 mm2.97 However, through interface engineering, it has been demonstrated that G/Si SCs can reach a PCE over 7% with a device region of 0.09 cm2.125 It is essential to raise the active area to a minimum of 0.1 cm2 for further improvement. Due to high sheet resistance of the graphene layer, the collection efficiency of photogenerated charge carriers would be decreased with a larger size of the device's active area. A grid electrode has been introduced to the traditional window-based device structure to reduce the resistance of graphene layer.128 This grid electrode design facilitates low-resistance contact with the graphene layer and enhances carrier collection efficiency. Therefore, employing a fine metal electrode design on the front side is essential to favor carrier collection throughout the entire device region. Another significant matter is the long-term durability of these G/Si SCs. With the passage of time, the performance of these SCs begins to deteriorate, particularly after the doping process. A number of researchers have studied the durability of G/Si SCs during storage and attempted to mitigate the deterioration. Xie et al.95 noted outcomes after various time intervals, indicating that the PCE of G/Si SCs decreased from 10.40% to 7.42% within 3 months.
Third, graphene is commonly moved on a Si substrate to create an SJ. However, graphene is fragile, and the remaining copper particles may stay on the graphene film after wet etching.129,130 These contaminants at the G/Si interface can act as short-circuit channels, resulting in current loss. As expected, the leakage current becomes more prominent as the device area increases. Therefore, the increased area of graphene is an important parameter affecting collection efficiency. To address this issue, advanced manufacturing and transfer skills must be addressed to reduce the flaws and contaminants encountered during the wet transfer method. Additionally, an alternative approach involves directly growing graphene on the semiconductor surface, resulting in a more uniform graphene with fewer structural defects.131
On the other hand, G/Si PVCs are progressing in large-scale integration, offering high-efficiency and sustained solar technologies.84 Nevertheless, the performance of G/n-Si single-junction cells falls short compared with that of p–n junction of SCs due to some main causes, such as low Schottky barrier height, transfer-based SC design, and high lateral resistivity of graphene. The interfacial barrier height of G/n-Si SCs is ϕG − ϕSBH = ϕG − χn-Si = 0.65 eV which is lower than the Si energy bandgap (1.1 eV at 300 K). The G/Si SC designs evolved by moving graphene onto the Si substrates through a polymer-film-based chemical-transfer procedure. This process can cause defect centers, exacerbating interfacial carrier recombination and ultimately lowering the PV performance. The mobility of charge carriers of layer graphene grown by CVD is better than other methods. Nevertheless, a single graphene layer has a higher sheet resistance (100–100 Ω−1) than the solar-grade doped Si (50–100 Ω−1) of the p–n junction SCs.132 Such high lateral resistivity of graphene films results in inefficient losses such as increased RS and decreased fill factors in G/Si PV heterojunction cells. Several approaches to overcoming the challenges of G/Si PV devices have been explained.84 The following part outlines strategies for tuning the interface utilizing suitable interlayers and modulating the functionality of graphene, all aimed at reaching highly efficient and robust G/Si SCs.
Graphene's impact on the field of solar energy harvesting devices is not limited to revolutionizing renewable energy assets. It is also a promising material for smart energy generation and storage devices. Nevertheless, conventional energy generators are incapable of providing responses to environmental changes and traditional energy storage devices lack functionalities other than providing electricity, posing challenges. However, graphene owing to its microscopic structure modification and exceptional physicochemical properties offers potential solutions to these issues. Thus, intelligent energy generation and storage and smart electric devices that can engage with receptive to external stimuli are becoming increasingly important and highly demanded. Recently, the key advances that involve the integration of graphene into smart energy generation and storage systems were systematically reviewed by Ye et al.133 In the context of smart energy generation, the authors discussed graphene-derived electric generators that can harvest electricity in response to external stimuli, such as flowing liquid, moisture, pressure force, friction, and heat. These advanced energy storage solutions exhibit remarkable features such as wearability, deformability, printability, responsiveness to stimuli, integration capabilities, miniaturization, and self-healing properties, showcasing the exciting possibilities enabled by graphene in the realm of energy storage.
Industrial production has been extremely high with a massive global demand for graphene-based commercial products. In PVs, graphene has been discovered as an electrode in SC technologies thanks to its brilliant properties. Recent advancements in G/Si-based (SB-SCs) have received considerable attention. With the noble continued efforts of researchers, the PCE for G/Si SCs has dramatically increased from 1.65% to 15%, which is comparable to that of metal halide perovskite cells with the highest efficiency of 20–22%.134 However, there is a great opportunity for enhancement in the behavior of G/Si SCs. To improve the overall PCE of G/Si SCs, chemical doping of graphene, interfacial layer utilization, and anti-reflection coatings have played significant roles. The surface recombination in influencing FF was expanded with prominence on the passivation approach and the use of a thin hole transport interlayer. All parameters such as JSC, VOC, and FF, eventually establish the PCE of certain G/Si SCs. In perceptions, G/Si appears to offer new utilizations for future-generation SCs. Despite its fast progress, there are challenges and limitations to its implementation on a commercial scale. One of the major challenges lies in achieving continuous graphene growth with excellent material quality. Additionally, the environmental durability of G/Si SCs is a concern. However, recent advancements suggest that graphene-based electronics combined with Si can lead to high-efficiency SCs with commercial viability. Therefore, G/Si heterostructure systems demonstrate industrial potential, as efforts are being made to reduce costs and capitalize on their lightweight nature and corrosion resistance, making them an ideal material for PVs. Several companies and research institutes are now emphasizing on graphene chemistry R&D to enhance the efficiency and production of induced graphene in SCs. Following the successful implementation of graphene electrodes in the SC, various other electronic entities are exploring improving graphene in their machinery in order to reach the same level of efficiency in those sectors. The automotive industry can become more environmentally friendly by incorporating SCs, which enhance the speed and range of solar cars. In conclusion, graphene-induced SCs are considered one of the most significant inventions of this decade, capturing the attention and driving the development of the global scientific community. Furthermore, scientists are actively working towards enhancing the efficiency of graphene-based SCs to maximize energy harnessing. By promoting solar energy, graphene holds a key role in facilitating sustainable, clean, and environmentally friendly energy productions and utilization worldwide (Fig. 13). Importantly, graphene's success extends beyond SCs to encompass various notable applications, including sensors, photodetectors, and smart energy generation and storage devices.
Fig. 13 The promising prospects of van der Waals graphene heterojunctions integrated into the solar energy harvesting. |
Footnote |
† These authors contributed equally to this work. |
This journal is © The Royal Society of Chemistry 2023 |