Graphene-wrapped sulfur-based composite cathodes: ball-milling synthesis and high discharge capacity
Received
5th August 2014
, Accepted 19th September 2014
First published on 19th September 2014
Abstract
A facile ball-milling route, which can help in large-scale synthesis, is developed to prepare graphene-wrapped sulfur/carbon nanotubes composite. Electrochemical tests show that the obtained composite demonstrates high sulfur utilization and good cycle performance. As calculated by the total mass of the composite, a high reversible capacity of 626.0 mA h g−1 can be obtained after 70 cycles at a current density of 400 mA g−1.
Introduction
The urgent demand for high-power and high-energy-density battery systems has spurred extensive research in developing novel electrode materials, in response to the development of electric vehicles (EVs) and hybrid electric vehicles (HEVs). Elemental sulfur has been proposed as one of the most promising cathode materials for next-generation high-energy density rechargeable batteries, due to its high theoretical capacity of 1672 mA h g−1, as well as environmental friendliness, abundance, and economic price.1–3 Despite these advantages, the commercialization of Li–S batteries is still seriously limited by their low sulfur utilization and poor cycle life, arising from the insulating nature of sulfur (5 × 10−30 Ω−1 cm−1 at 25 °C) and the dissolution of polysulfides. During the discharge–charge process, the generated higher-order polysulfides can diffuse through the electrolyte to the anode and react with the lithium anode to form lower-order polysulfides. These reduced products can also diffuse back to the sulfur cathode, and this cyclic process is known as the “shuttle effect”.1–3 Such a parasitic process results in poor cycle life, low coulombic efficiency and low utilization of sulfur active materials. To address these problems, there have been extensive investigations into improving sulfur cathodes by using conductive carbon as the sulfur immobilizer and conductive matrix.1–3 Among these carbon materials, graphene is of particular interest, due to its large surface area (ca. 2600 m2 g−1), excellent mobility of charge carriers (20
000 cm2 V−1 s−1), high chemical and thermal stability, and superior mechanical flexibility.1–9 For composites based on graphene and sulfur, a significantly enhanced electrochemical performance has been obtained. However, due to the strong π–π stacking and hydrophobic interactions, graphene sheets are easy to agglomerate during the experiment, and thus a complicated solution process is always needed to obtain uniform graphene-based composites.4–9 This results in high cost and poor control in the consistency of the active material, seriously limiting their practical applications. Thus, the development of facile and large-scale synthesis routes to prepare homogeneous cathodes based on sulfur and graphene is of immense importance for commercial production of lithium–sulfur batteries.
Ball-mill technology is widely used for grinding materials in industrial applications. For its application in the synthesis of electrode materials, the advantages can be described as follows: (1) the large-scale synthesis of homogeneous electrode materials can be easily realized, which is important for the consistency of the battery materials; (2) reliable operation to ensure reproducible results; and (3) it is suitable for various synthesis systems and appealing for many practical applications, due to its economy and easy replicability.10–13 Following all the discussions above, we designed a continuous ball-milling strategy to prepare a high performance graphene-wrapped sulfur/carbon nanotubes composite. In this strategy, first, sulfur and carbon nanotubes are homogeneously mixed via ball-milling, as it has been suggested that sulfur particles will be closely attached to the surface of carbon nanotubes during the ball-milling process, thereby producing a highly uniform mixture.12–15 Then, graphene oxide and hydrazine are added during the continuous ball-milling process to produce a surface coating layer. The hollow and cross-linked carbon nanotubes ensure the fast transport of electrons from carbon to sulfur and facilitate lithium-ion diffusion throughout the whole material. Moreover, the surface coating layer can further restrict the dissolution of polysulfide. The unique structure of the designed surface of the graphene-coated sulfur/carbon nanotubes composite can offer a high electrochemical performance.
Experimental
2.1. Preparation and characterization
To prepare the precursor sulfur/carbon nanotubes composite (S/CNT composite), sulfur and multi-walled carbon nanotubes (diameter: 10–20 nm, length: 5–15 μm, ≥95%) with a weight ratio of 3
:
2 were added in the agate tank (50 mL) and then mixed well by ball-milling. The ball-milling was performed in a planetary ball mill (QM-3SP04, Nanjing) under ambient conditions at a speed of 300 rpm for 3 h. For the synthesis of graphene-wrapped sulfur/CNT composite (graphene@S/CNT composite), graphene oxide (0.2 g, Tianjin Plannano Technology Co., Ltd) and S/CNT composite (0.4 g) were first distributed homogenously in ethanol (10 mL) by stirring. Then, the mixture and hydrazine (1 mL, 35 wt% solution in water, Sigma Aldrich) were added in the agate tank and ball-milled at a speed of 500 rpm for 3 h. The obtained sample was washed with water and ethanol, and finally, dried at 60 °C for 12 h.
The as-prepared samples were characterized by X-ray diffraction (XRD, Model LabX-6000, Shimadzu, Japan), thermogravimetric analysis (TGA, SDT Q600), scanning electron microscopy (SEM, JSM-7001F), and transmission electron microscopy (TEM, FEI Tecnai F20).
2.2. Electrochemical measurements
The working electrodes were prepared by compressing a mixture of active materials, acetylene black, and binder (polytetrafluoroethylene, PTFE) in a weight ratio of 70
:
20
:
10. Lithium metal was used as the counter and reference electrodes. The electrolyte was lithium bis(trifluoromethanesulfonyl)imide (2.8 M) dissolved in a mixture of dimethoxyethane (DME) and dioxolane (DOL) in a volume ratio of 1
:
1. LAND-CT2001A galvanostatic testers were employed to measure the electrochemical capacity at a current density of 400 and 800 mA g−1, and the cycle life of the working electrodes at room temperature. The cut-off potentials for charge and discharge were set at 3.0 and 1.5 V (vs. Li+/Li), respectively. Cyclic voltammetry (CV) experiments were conducted using a CHI 600E potentiostat at a scan rate of 0.1 mV s−1.
Results and discussion
Fig. 1a includes the XRD patterns of sulfur, carbon nanotubes, S/CNT composite and graphene@S/CNT composite. As shown, the crystalline state of sulfur is retained after the ball-milling, which is in contrast with the previous thermal treatment routes.16,17 The graphene@S/CNT composite demonstrates a similar pattern to the S/CNT composite due to the amorphous state of graphene, and also weaker peaks of sulfur, due to the coating of graphene. Fig. 1b shows the TGA curves of the S/CNT composite and graphene@S/CNT composite obtained at a heating rate of 10 °C min−1 under an argon atmosphere. As can be seen, the sulfur content in the graphene@S/CNT composite is ca. 50 wt%. Furthermore, it should be mentioned that there is an extra 4 wt% loss up to 600 °C for the graphene-wrapped composite, whereas the curve of S/CNT is flat. The extra weight loss may also be attributed to the evaporation of sulfur, as the violent ball-milling process will generate a tight coating layer, and even produce a weak binding between graphene and sulfur. Similar to sulfur/nanoporous carbon composite, a higher temperature is needed to overcome the restriction of such a coating or binding.18
 |
| Fig. 1 XRD patterns of sulfur, carbon nanotubes, S/CNT composite and graphene@S/CNT composite (a); TGA curves of the S/CNT composite and graphene@S/CNT composite (b). | |
SEM was carried out to illustrate the morphology of the as-prepared samples. As shown in Fig. 2a and b, it can be clearly seen that the S/CNT composite is composed of micro-sized particles with cross-linked carbon nanotubes. No sulfur particles can be observed, indicating the homogenous mixture of sulfur and carbon nanotubes. For the graphene@S/CNT composite, a different morphology is observed. It can be seen that there is further aggregation of the composite particles, which are coated by graphene. The reduction of graphene oxides leads to the shrinkage and re-stacking of graphene nanosheets,19 thus wrapping the particles together to form the surface-coated composite. By comparing Fig. 2b and d, it can be seen that the loose cross-linked structure disappears and that the S/CNT composite is completely encapsulated by the graphene coating layer. To further illustrate the microstructure of the sulfur-based composite, TEM images are shown in Fig. 2e and f. For the graphene@S/CNT composite, it can be clearly seen that the reduced graphene sheets encapsulate the S/CNT composite particles to form a hierarchical structure, and the surface coated graphene layer can be clearly observed in Fig. 2f. It should be mentioned that some small amounts of nanotubes are not wrapped, and hence, further research focused on the ball-milling speed or solvent is still needed to obtain more uniform composite. On the other hand, the exposed nanotubes can also facilitate the transport of electrolyte ions into the composite, to produce a high electrochemical performance.
 |
| Fig. 2 SEM and TEM images of the S/CNT composite (a and b) and graphene@S/CNT composite(c–f). | |
Fig. 3 shows the cyclic voltammograms (CVs) of the as-prepared S/CNT composite and graphene@S/CNT composite at a scan rate of 0.1 mV s−1. Two clearly different curves can be observed. For the graphene coated composite, during the initial cathodic process, a pair of peaks around 2.18 and 1.85 V can be observed, which relate to the two-step reduction of S8 to lithium polysulfides and eventually to Li2S.1–3 In contrast with the previous reports,6–8,16,17,20,21 the second peak is obviously broadened. The possible reason can be attributed to the tight package of graphene during the ball-milling process and the strong adsorption ability of the carbon nanotubes, which can lead to a high electrochemical polarization.22 For the S/CNT composite, only one cathodic peak around 2.1 V can be observed, due to the dissolution of Li2S8, further confirming the restriction effect of graphene in the graphene@S/CNT composite.
 |
| Fig. 3 Cyclic voltammograms of the S/CNT composite and the graphene@S/CNT composite at a scan rate of 0.1 mV s−1. | |
Based on the above results, it can be concluded that the obtained composite contains a cross-linked conductive matrix, hollow channels, and a tight surface coated graphene layer, which makes it a promising high-performance sulfur-based cathode. To evaluate the electrochemical performance of the as-prepared samples, cell tests were conducted (Fig. 4). Fig. 4a includes the initial discharge–charge curves of the obtained composites at a current density of 400 and 800 mA g−1. For the S/CNT composite, it demonstrates a low discharge and charge capacity of 170 and 164 mA h g−1 at a current density of 400 mA g−1, respectively. In comparison, the graphene@S/CNT composite presents a different discharge–charge curve, and a flat potential plateau around 2.1 V can be observed, which corresponds to the transfer from S82− to lower-order polysulfide.1–3 Without graphene wrapping, the S82−ions will dissolve into the electrolyte before transformation, and the conventional flat plateau disappears, accounting for the sulfur/carbon nanotubes composite, which is consistent with the result of the CVs. On the other hand, the initial discharge and charge capacity of graphene@S/CNT composite is 906.6 and 840.3 mA h g−1, whereas it is about 1813.2 and 1680.6 mA h g−1 as calculated by weight of sulfur, further confirming the restriction on the dissolution of polysulfides by introducing the graphene coating. A high initial discharge capacity, exceeding the theoretical capacity of sulfur, can be observed in the other sulfur/carbon composite.18,23,24 However, if the extra weight loss (4 wt%) of the graphene-wrapped composite is attributed to the loss of sulfur, the initial discharge capacity calculated by the sulfur is 1678 mA h g−1, perfectly equal to the theoretical capacity of element sulfur. When the current density is enhanced to 800 mA g−1, it is obvious that the discharge–charge curves are well-retained, and the initial discharge capacity is 658 mA h g−1. The capacity retention can be as high as 72.6%, indicating the good kinetic process of the composite.
 |
| Fig. 4 Initial discharge–charge curves (a) and cycle performance (b) of the graphene@S/CNT composite and S/CNT composite at different current densities (composite); cycle performance (c) of the graphene@S/CNT composite at different current densities (composite). | |
Fig. 4b includes the cycle curves of the obtained composites at different current densities. As shown, the graphene@S/CNT composite shows a good cycle performance, and after 70 cycles, the discharge capacity can be retained at 626.0 mA h g−1 at the current density of 400 mA g−1, which is about 1252.0 mA h g−1 as calculated by the weight of sulfur. Furthermore, it is worth mentioning that the composite shows a high coulombic efficiency above 95% after the 2nd cycle. The reversible discharge capacity (1256.0 mA h g−1) is among the best results compared to the graphene and sulfur-based composites synthesized by other methods,7–9,25–29 indicating that the ball-milling route is a practical route for the large-scale synthesis of high performance sulfur-based composites. At a current density of 800 mA g−1, it can be seen that the obtained composite still shows a good cycle performance and even after the 100th cycle, a discharge capacity of 425.8 mA h g−1 can be obtained, which is about 851.6 mA h g−1 as calculated by the weight of sulfur. It should be emphasized that although the sulfur content is low, the graphene@S/CNT composite still demonstrates a high discharge capacity, as calculated for the composite due to the high sulfur utilization. The high reversible capacity of 626.0 mA h g−1 is among the best results compared to the graphene and sulfur-based composites prepared via complicated solution synthesis processes and/or templates.4,5,7–9,25–27
By considering all the results above, it can be concluded that a high discharge capacity has been obtained by a simple ball-milling route, without employing a complex solution synthesis or thermal treatment processes. The high performance of the graphene@S/CNT composite can be attributed to its unique structure and can be elaborated as follows: (1) the hollow carbon nanotubes conductive matrix ensures fast electron and Li-ion transport throughout the composite, thus producing a high sulfur utilization at a high current density; (2) the intact hollow tubes of the carbon nanotubes trap the polysulfides and accommodate a volume change to maintain the structural stability of the composite during the discharge–charge process; and (3) the homogeneous and tight surface coating of graphene effectively restricts the dissolution of the polysulfides and further enhances the utilization of sulfur, due to its excellent conductivity. In conclusion, sulfur-based composites with the same high performance can be obtained via a practical ball-milling route as compared to fabrication via a complicated solution route.
Conclusions
A graphene-wrapped sulfur/carbon nanotubes composite was successfully prepared via the ball-milling method. Compared to previous solution-based methods, the large-scale synthesis of a graphene-wrapped sulfur composite with high consistency can be easily achieved by this strategy. The homogeneous coating of graphene on the sulfur/carbon nanotubes composite can be observed from the SEM and TEM characterization, and it leads to a high electrochemical performance of the obtained composite. At a current density of 400 mA g−1, the graphene@S/CNT composite demonstrates a high initial discharge capacity of 906.6 mA h g−1 and a good cycle performance. After the 70th cycle, the capacity can be stabilized at 626.0 mA h g−1, as calculated by the total mass of composite. When the current density is increased to 800 mA g−1, the discharge capacity still reaches up to 658.0 mA h g−1, and the capacity is retained at 426.8 mA h g−1 after 100 cycles, which is 851.6 mA h g−1, as calculated by the weight of sulfur. The good performance can be attributed to the synergistic effect of the graphene coating, the carbon conductive matrix, and the intact hollow tubes. The continuous ball-milling route can also be applied to prepare other graphene-wrapped sulfur–carbon materials.
Acknowledgements
This work has been supported by the Chinese National Science Funds (no. 51202094); the Priority Academic Program Development of Jiangsu Higher Education Institutions; and the Natural Science Foundation (no. 12KJB150010) of Jiangsu Education Committee of China.
Notes and references
- A. Manthiram, Y. Z. Fu and Y. S. Su, Acc. Chem. Res., 2013, 46, 1125 CrossRef CAS PubMed.
- S. Evers and L. F. Nazar, Acc. Chem. Res., 2013, 46, 1135 CrossRef CAS PubMed.
- D. Bresser, S. Passerini and B. Scrosati, Chem. Commun., 2013, 49, 10545 RSC.
- M. Xiao, M. Huang, S. S. Zeng, D. M. Han, S. J. Wang, L. Y. Sun and Y. Z. Meng, RSC Adv., 2013, 3, 4914 RSC.
- G. He, C. J. Hart, X. Liang, A. Garsuch and L. F. Nazar, ACS Appl. Mater. Interfaces, 2014, 6, 10917 CAS.
- N. Mahmood, C. Z. Zhang, H. Yin and Y. L. Hou, J. Mater. Chem. A, 2014, 2, 15 CAS.
- J. Xie, J. Yang, X. Y. Zhou, Y. L. Zou, J. J. Tang, S. C. Wang and F. Chen, J. Power Sources, 2014, 253, 55 CrossRef CAS PubMed.
- R. J. Chen, T. Zhao, J. Lu, F. Wu, L. Li, J. Z. Chen, G. Q. Tan, Y. S. Ye and K. Amine, Nano Lett., 2013, 13, 4642 CrossRef CAS PubMed.
- S. T. Lu, Y. W. Cheng, X. H. Wu and J. Liu, Nano Lett., 2013, 13, 2485 CrossRef CAS PubMed.
- C. Lai, Z. Z. Wu, Y. X. Zhu, Q. D. Wu, L. Li and C. Wang, J. Power Sources, 2013, 226, 71 CrossRef CAS PubMed.
- L. Z. Ouyang, L. N. Guo, W. H. Cai, J. S. Ye, R. Z. Hu, J. W. Liu, L. C. Yang and M. Zhu, J. Mater. Chem. A, 2014, 2, 11280 CAS.
- X.-B. Cheng, J.-Q. Huang, Q. Zhang, H.-J. Peng, M.-Q. Zhao and F. Wei, Nano Energy, 2014, 4, 65 CrossRef CAS PubMed.
- L. Zhu, W. C. Zhu, X.-B. Cheng, J.-Q. Huang, H.-J. Peng, S.-H. Yang and Q. Zhang, Carbon, 2014, 75, 161 CrossRef CAS PubMed.
- J. Z. Chen, F. Wu, R. J. Chen, L. Li and S. Chen, New Carbon Mater., 2013, 28, 428 CAS.
- W. Weng, S. W. Yuan, N. Azimi, Z. Jiang, Y. Z. Liu, Y. Ren, A. Abouimrane and Z. C. Zhang, RSC Adv., 2014, 4, 27518 RSC.
- G.-C. Li, G.-R. Li, S.-H. Ye and X.-P. Gao, Adv. Energy Mater., 2012, 2, 1238 CrossRef CAS.
- X. F. Wang, X. P. Fang, X. W. Guo, Z. X. Wang and L. Q. Chen, Electrochim. Acta, 2013, 97, 238 CrossRef CAS PubMed.
- J. Kim, D.-J. Lee, H.-G. Jung, Y.-K. Sun, J. Hassoun and B. Scrosati, Adv. Funct. Mater., 2013, 23, 1076 CrossRef CAS.
- S. F. Pei and H.-M. Cheng, Carbon, 2012, 50, 3210 CrossRef CAS PubMed.
- N. Jayaprakash, J. Shen, S. S. Moganty, A. Corona and L. A. Archer, Angew. Chem., Int. Ed., 2011, 123, 1 CrossRef.
- Y.-S. Su and A. Manthiram, Nat. Commun., 2012, 3, 1166 CrossRef PubMed.
- J. L. Wang, J. Yang, J. Y. Xie, N. X. Xu and Y. Li, Electrochem. Commun., 2002, 4, 499 CrossRef CAS.
- D.-J. Leel, M. Agostini, J.-W. Park, Y.-K. Sun, J. Hassoun and B. Scrosati, ChemSusChem, 2013, 6, 2245 CrossRef PubMed.
- S. S. Zhang, Frontiers in Energy Research, 2013, 1, 1 Search PubMed.
- H.-J. Peng, J.-Q. Huang, M.-Q. Zhao, Q. Zhang, X.-B. Cheng, X.-Y. Liu, W.-Z. Qian and F. Wei, Adv. Funct. Mater., 2014, 24, 2772 CrossRef CAS.
- W. Z. Bao, Z. Zhang, W. Chen, C. K. Zhou, Y. Q. Lai and J. Li, Electrochim. Acta, 2014, 127, 342 CrossRef CAS PubMed.
- B. Wang, Y. F. Wen, D. L. Ye, H. Yu, B. Sun, G. X. Wang, D. Hulicova-Jurcakova and L. Z. Wang, Chem.–Eur. J., 2014, 20, 5224 CrossRef CAS PubMed.
- K. H. Kim, Y.-S. Jun, J. A. Gerbec, K. A. See, G. D. Stucky and H.-T. Jung, Carbon, 2014, 69, 543 CrossRef CAS PubMed.
- J.-Q. Huang, H.-J. Peng, X.-Y. Liu, J.-Q. Nie, X.-B. Cheng, Q. Zhang and F. Wei, J. Mater. Chem. A, 2014, 2, 10869 CAS.
|
This journal is © The Royal Society of Chemistry 2014 |
Click here to see how this site uses Cookies. View our privacy policy here.