Issue 7, 2017

In situ high-precision Ni isotope analysis of metals by femtosecond-LA-MC-ICP-MS

Abstract

In this study, an in situ technique for high-precision determination of Ni stable isotope ratios by femtosecond-laser ablation-multicollector-ICP-MS (fs-LA-MC-ICP-MS) was developed. With this technique, the Ni isotope compositions of Ni-bearing steels (NIST RM-1226 and BAM D 184-1) and a Ni-rod (standard 10209 from MAC) were determined, both by fs-LA-MC-ICP-MS analyses and by solution MC-ICP-MS, the latter in order to verify the results of the in situ analyses. The LA-MC-ICP-MS analyses revealed that all analyzed standard materials were homogeneous within analytical uncertainties and may thus be suitable as external standards for Ni isotope determination by in situ analysis of metal phases and sulfides. Bulk solution MC-ICP-MS and LA-MC-ICP-MS analyses of these metals agreed within their analytical uncertainties of 0.03‰ for the solution analyses and <0.1‰ (2SD, over 12 months) for the LA-MC-ICP-MS analyses. These results imply that the accuracy of the in situ analyses of metals is better than 0.1‰. The average of four solution nebulization analyses of the Ni-rod and D 184-1, and of 16 analyses of the NIST RM-1226 material, revealed δ62Ni values of −0.26‰, 0.12‰, and −0.28‰ relative to NIST SRM-986, respectively. In order to show the applicability and potential of the presented method, the Ni and Fe isotope compositions of a kamacite–taenite interface in IAB iron meteorite Canyon Diablo were determined by fs-LA-MC-ICP-MS analyses. The isotope profile reveals lighter Fe isotopes in kamacite than in taenite, while the Ni isotope composition is vice versa. Evolution of the isotope signals along the interface of these metal phases strongly points to diffusion-driven fractionation of Fe and Ni isotopes during the formation of kamacite by the replacement of taenite. Due to Fe–Ni exchange diffusion between taenite and kamacite and the generally faster diffusion of light isotopes compared to heavy isotopes, the remaining taenite is left with heavier Fe and lighter Ni isotope compositions than the newly formed kamacite. Demonstration of such detailed information about the diffusion processes in the kamacite–taenite system was not possible before, due to the lack of an appropriate high-precision and high spatial resolution technique for in situ Ni isotope analyses.

Graphical abstract: In situ high-precision Ni isotope analysis of metals by femtosecond-LA-MC-ICP-MS

Supplementary files

Article information

Article type
Paper
Submitted
13 Eph 2017
Accepted
07 Jun 2017
First published
07 Jun 2017

J. Anal. At. Spectrom., 2017,32, 1312-1319

In situ high-precision Ni isotope analysis of metals by femtosecond-LA-MC-ICP-MS

M. Weyrauch, M. Oeser, A. Brüske and S. Weyer, J. Anal. At. Spectrom., 2017, 32, 1312 DOI: 10.1039/C7JA00147A

To request permission to reproduce material from this article, please go to the Copyright Clearance Center request page.

If you are an author contributing to an RSC publication, you do not need to request permission provided correct acknowledgement is given.

If you are the author of this article, you do not need to request permission to reproduce figures and diagrams provided correct acknowledgement is given. If you want to reproduce the whole article in a third-party publication (excluding your thesis/dissertation for which permission is not required) please go to the Copyright Clearance Center request page.

Read more about how to correctly acknowledge RSC content.

Social activity

Spotlight

Advertisements