Issue 5, 2016

Deactivation mechanisms of tin-zeolites in biomass conversions

Abstract

Metal-containing zeolites comprise outstandingly active and selective catalysts for a multitude of Lewis-acid and redox catalysed reactions that valorise renewable substrates into chemicals. Herein, focussing on tin-zeolites applied to the isomerisation of dihydroxyacetone (DHA) and xylose, we systematically study the influence of the framework type (MFI, MOR, BEA and FAU), preparation method (hydrothermal synthesis or alkaline-assisted metallation), hydrophobicity and nature of the solvent (water or methanol) on their intrinsic activity and, especially, on their stability. BEA and FAU zeolites were more active than MFI and MOR stannosilicates in aqueous and, particularly, in methanol-based tests owing to the larger relative amount of tetrahedral tin sites and/or superior mass transfer properties. Hydrothermally-prepared zeolites generally exhibited higher turnover frequencies than those obtained by a post-synthetic approach in view of their higher tin quality and less hydrophilic character. Remarkably, continuous-flow tests in a fixed-bed reactor indicated that exposure to reaction conditions for 24 hours could provoke dramatic changes in performance. Mainly due to amorphisation and modification of the tin structure (from tetra- to hexacoordination), the activity and selectivity of MOR, BEA and FAU zeolites were substantially, if not fully, depleted in the aqueous isomerisation of DHA, while MFI zeolites, especially the post-synthetically stannated sample, better preserved their initial performance. These deactivation phenomena were alleviated through the use of methanol, an industrially more amenable solvent, but, due to the greater retention of activity, fouling was more pronounced, particularly for MFI zeolites. In contrast, more extensive metal leaching was detected owing to the higher solubility of tin in the alcohol rather than water, where it hydrolyses into insoluble hydroxide species. In xylose isomerisation, hydrothermally-prepared MFI and BEA stannosilicates displayed reasonably stable operation. Deactivation mechanisms partly resembled those of the aqueous DHA isomerisation, but the chelating properties of the substrate played a greater detrimental role in tin loss.

Graphical abstract: Deactivation mechanisms of tin-zeolites in biomass conversions

Supplementary files

Article information

Article type
Paper
Submitted
10 9月 2015
Accepted
02 11月 2015
First published
04 11月 2015

Green Chem., 2016,18, 1249-1260

Author version available

Deactivation mechanisms of tin-zeolites in biomass conversions

G. M. Lari, P. Y. Dapsens, D. Scholz, S. Mitchell, C. Mondelli and J. Pérez-Ramírez, Green Chem., 2016, 18, 1249 DOI: 10.1039/C5GC02147B

To request permission to reproduce material from this article, please go to the Copyright Clearance Center request page.

If you are an author contributing to an RSC publication, you do not need to request permission provided correct acknowledgement is given.

If you are the author of this article, you do not need to request permission to reproduce figures and diagrams provided correct acknowledgement is given. If you want to reproduce the whole article in a third-party publication (excluding your thesis/dissertation for which permission is not required) please go to the Copyright Clearance Center request page.

Read more about how to correctly acknowledge RSC content.

Social activity

Spotlight

Advertisements