Most Farida
Khatun
ab,
Takuya
Okamoto
*ac and
Vasudevanpillai
Biju
*ac
aGraduate School of Environmental Science, Hokkaido University, Sapporo, Hokkaido 060-0810, Japan. E-mail: biju@es.hokludai.ac.jp; okamotot@es.hokudai.ac.jp
bPharmacy Discipline, Khulna University, Khulna-9208, Bangladesh
cResearch Institute for Electronic Science, Hokkaido University, Sapporo, Hokkaido 001-0020, Japan
First published on 16th October 2023
Rationally assembled supramolecular structures of organic chromophores or semiconductor nanomaterials show excitonic properties different from individual molecules or nanoparticles. We report polymer-assisted assembly formation and thermal modulation of excitonic recombination in self-assembled formamidinium lead bromide perovskite quantum dots.
A polymer matrix is a technologically relevant host for dispersing and assembling optically active molecules and nanoparticles into stimuli-responsive devices. Williams et al. reported mechanically tuning optical properties of sticky polymer-grafted silica nanoparticle superlattices.7 Miyamoto et al. demonstrated mechanochromic perovskite nanosheet hydrogels.8 For thermochromism, Sussman et al. prepared a transparent film consisting of a polymer core and a composite shell, which becomes colored by heat-induced structural changes.9 So far, polymer hosts such as polyvinylpyrrolidone,10 polystyrene,11 polymethyl methacrylate,12 and polycarbonate13 have been applied to encapsulate nanoscale MHPs for protecting them from moisture and heat. Conversely, Gong et al. reported stretch-induced PL intensity enhancement for CsPbBr3 PQDs in a polymer composite.14 Also, Bade et al. demonstrated a stretchable perovskite LED using a MAPbBr3–polymer composite.15 Despite such emerging applications of MHP–polymer composites, stimuli-responsive excitonic recombination dynamics of perovskite assemblies in host materials remain largely unexplored.
We demonstrate reversible shifts in PL color and lifetime of FAPbBr3 PQD assemblies in polybutadiene (PBD) thin films as a function of temperature. FAPbBr3 PQD is selected due to the large differences in the PL spectral maxima and lifetimes between isolated and self-assembled PQDs.4a PBD is selected as the host matrix for making PQD assemblies, considering its elasticity, low glass transition temperature (Tg < 210 K), and optical transparency. The PL spectrum of isolated PQDs in toluene redshifts by >70 nm due to assembly formation during PQD–PBD film preparation. Also, the PL lifetime of a PQD assembly is much longer (345 ns) than isolated PQDs (1.3 ns). The green emission of a PQD assembly in a PBD film changes into cyan due to heat-induced (from 296 to 323 K) dissociation. This color change is due to a PL band ca. 480 nm corresponding to PQDs separated from assemblies. Correspondingly, the PL lifetime of a PQD assembly decreases from 345 to 74 ns. Interestingly, the PL color and lifetime are reversed by cooling the PQD–PBD film from 323 to 296 K. We discuss the PL color and lifetime changes of PQD assemblies from the viewpoint of exciton recombination in different dielectric environments.
We synthesized FAPbBr3 PQDs by the modified hot injection method.4a The synthesis procedure of PQDs is described in the ESI.†Fig. 1a shows the absorption and PL spectra of the as-synthesized PQD colloidal solution. The light-yellow-colored PQD solution shows blue emission under UV light (Fig. 1a inset). The sharp excitonic absorption peak (ca. 437 nm) and blue emission (ca. 441 nm) suggest strong quantum confinement and excitonic recombination of photo-excited PQDs, similar to low dimensional MHPs.4a,b,16 The excitonic absorption and PL bands are consistent with the quantum size (ca. 5 nm) of PQDs, as observed in the scanning transmission electron microscope (STEM) image (Fig. 1b). The as-synthesized PQD colloidal solution shows mono-exponential PL decay (Fig. 1c) with a short PL lifetime of 1.3 ns.
We prepared FAPbBr3 PQD-only and PQD–PBD films to verify PQD assembly formation in films. The films were prepared by drop-casting of the corresponding solutions in toluene. The PL color of a PQD-only film prepared from a 10 mg mL−1 solution in toluene is changed from blue to green during drying, consistent with our previous report.4a The small-angle x-ray scattering (SAXS) pattern (Fig. 1d) of the film showed an intense peak ca. 2.4 nm−1, supporting the quantum size of PQDs and a short interparticle distance of 2.6 nm. A PQD–PBD thin film was prepared by mixing a FAPbBr3 PQD colloidal solution (10 mg mL−1 in toluene) with a PBD solution (25 mg mL−1 in toluene), followed by drop-casting of 5 μL of the mixture on a glass coverslip. As the polymer host shrink during drying up, the polymer chains gathered isolated PQDs to form PQD assemblies in the film (Fig. 2a). STEM images of a PQD–PBD thin film (Fig. 2b and Fig. S1, ESI†) suggest the formation of polymer-assisted PQD assemblies.
To understand PL color and spectral changes of PQD samples during assembly formation, we examined the PL images and spectra of PQD-only and PQD–PBD films. Fig. 2c shows the corresponding PL images and spectra of a PQD–PBD film. The PL color of the film is changed from blue to green during assembly formation by solvent evaporation. Correspondingly, the PL spectrum is shifted from 460 to 532 nm. Low dimensional MHPs show strong quantum confinement, correspondingly blue-shifted absorption and PL bands, and short PL lifetimes. Conversely, due to strong dielectric screening, large PNCs and MHP microcrystals show red-shifted PL bands.17 Reabsorption-emission or inner filtering induces PL spectral redshift to thick MHP samples.17c,d Conversely, PNCs or PQDs in self-assembled films show red-shifted PL spectra and long PL lifetimes compared to isolated PNCs or PQDs due to increased interparticle-interaction-induced dielectric screening and exciton/carrier diffusion in films.4a,b,17b,d The PL lifetime of a PQD-only solution is increased from 1.3 (Fig. 1c) to 19.5 ns (Fig. 2d) in a PQD–PBD solution. As the PQD–PBD film was dried up in ambient air, the PL lifetime of PQDs increased to 83.8 ns (Fig. 2d). The PL lifetime was further increased to 345 ns after 4.5 h drying of the film. The PL spectral redshift and PL lifetime increase suggest PQD assembly formation in the film. Fig. 2e shows the plots of PL lifetime and optical bandgap of PQDs in a PQD–PBD film during drying. The correlation between PL lifetimes and optical bandgaps in Fig. 2e indicates increasing dielectric screening,4a,b weakening quantum confinement,4a,b increasing electronic coupling,4b,18 and decreasing surface trap density4a of PQDs during PQD assembly formation. The SAXS pattern of the PQD–PBD mixture shows a peak at the same position as the PQD film (Fig. 1d and 2f), suggesting PQD assembly formation in SAXS samples with or without PBD. In both cases, the interparticle spacing is determined by the capping ligands.
To understand the assembly formation mechanism and explore the thermal modulation of exciton dynamics in the assemblies, we investigated temperature-dependent PL properties of PQD–PBD films. A film was heated from 296 to 323 K on a micro heat plate (KITAZATO, KM-1), during which PL spectra, PL images, and PL decays of the film were recorded at different time intervals. Fig. 3a shows the PL spectra of a PQD–PBD film at different temperatures. Initially, the PL peak was at 544 nm [Fig. 3a(i)] for a completely dried PQD–PBD film at 296 K. As the temperature was increased to 323 K, the PL peak blue-shifted (Δλ = 14 nm) with the appearance of a shoulder band at 495 nm [Fig. 3a(ii)]. Correspondingly, the average PL lifetime of the film was decreased from 345 [Fig. 3b(i)] to 74 ns [Fig. 3b(ii) + (iii)]. Nevertheless, a PQD-only film does not show much PL spectral shift by heating from 296 to 323 K (Fig. S2a, ESI†). The largely blue-shifted PL spectrum (Δλ = 39 nm) and decreased PL lifetime of the film at 323 K are comparable to the mechanically dissociated FAPbBr3 PQD-only films (Fig S2b, ESI†).4a
The PL spectral blueshift of PQD assemblies with increasing temperature19 is the opposite of the Varshini model,20 which predicts PL redshift of semiconductors. Wang et al. reported the temperature-dependent (280 K → 320 K) PL spectral blueshift for a FAPbBr3 PNC film (Δλ ∼ 7 nm) due to optical phonon scattering.19a Yang et al. observed a PL spectral blueshift for FAPbBr3 PNCs with increasing temperature from 90 to 350 K due to phase transition (at 150 K) and thermal expansion (Δλ ∼ 3 nm for 290 K → 320 K).19b For other A-site cation MHPs, Woo et al. reported a PL spectral blueshift (Δλ < 5 nm) for MAPbBr3 with increasing temperature from 280 K to 300 K due to the thermal lattice expansion and electron–phonon interactions,19c and Li et al. reported a PL spectral blueshift (80 K to 280 K) and small redshift (from 280 K to 360 K) for a CsPbBr3 PNC film with increasing temperature.19d Although the small blueshift of the main PL band from 544 to 530 nm [from Fig. 3a(i) to Fig. 3a(ii)] can be attributed to the temperature-dependent exciton–phonon property of FAPbBr3 PQD assemblies, the largely blue-shifted (Δλ = 39 nm) shoulder band with a short PL lifetime suggests that the thermal expansion of the polymer chains partially dissociates PQD assemblies in the film, increasing inter-PQD distances and decreasing dielectric screening. The residual green emission after prolonged heating indicates reminiscent assemblies or fused PQDs. The PQD–PBD film was heated within the phase transition temperature of FAPbBr3.21
We repeatedly heated and cooled the PQD–PBD film to validate the reversibility of PQD assembly formation and dissociation. The main PL peak was red-shifted from 530 nm to 544 nm by cooling the film from 323 K to 296 K, with an appreciable decrease in the PL intensity of the blue-shifted shoulder band [Fig. 3a(ii)]. Also, the PL lifetime was increased from 74 to 128 ns by cooling down the film. The PL redshift from 530 to 544 nm is attributed to the temperature-dependent PL property of FAPbBr3 PQDs. However, the PL intensity decrease for the blue-shifted shoulder band and the PL lifetime increase during cooling are attributed to the reassembling of PQDs by the shrinking polymer host. Nevertheless, the complete disappearance of the shoulder band or complete recovery of the PL lifetime was not accomplished, suggesting PQD reassembling is partially hindered by the polymer chains occupying around a fraction of the thermally separated PQDs, which was confirmed by the PL spectral blueshift (Fig. S3a, ESI†) and lifetime decrease (Fig. S3b, ESI†) by increasing the polymer concentration in precursor solution of PQD–PBD film.
Finally, we rationalize the structural and PL property changes of the PQD assembly from the viewpoint of exciton/carrier recombination dynamics (Fig. 3c and d). A PL spectral redshift and long PL lifetime during PQD assembly formation are attributed to decreased inter-PQD distance. As the PQDs come closer, the electronic wavefunctions of neighboring PQDs overlap, leading to miniband formation.4b,18 Green-emitting PNCs with weak quantum confinement are also formed by ligand stripping of PQDs.4a The PL lifetime increase during assembly formation is attributed to decreased surface trap density and increased exciton dielectric screening.4a,b Consequently, the surface trap-related nonradiative recombination rate (knr) decreases, and the strong dielectric screening in the assemblies helps photogenerated excitons to split into carriers,22 increasing the PL lifetime. Conversely, the thermal expansion of the polymer dissociates PQDs from PQD assemblies, increasing the inter-PQD distance and lowering the strength of inter-PQD interactions. Therefore, when heated, a PQD–PBD film shows blue-shifted PL and a short PL lifetime. The incomplete recovery of the PL spectrum and lifetime is due to the incomplete separation of PQDs.
In summary, we demonstrate FAPbBr3 PQD assembly formation in a polymer and the heat-induced modulation of the PL color and lifetime of the assemblies. We concluded that the thermal expansion or shrinkage of the polymer host controls PQD assemblies and their excitonic properties, providing new dimensions to perovskite-based sensing devices.
We acknowledge the financial support under the MEXT JSPS grant-in-aid for scientific research (23H01781 and 21K14580). This work was performed under the Research Program of “Dynamic Alliance for Open Innovation Bridging Human, Environment and Materials” in “Network Joint Research Center for Materials and Devices.” We acknowledge a JST DX doctoral scholarship.
Footnote |
† Electronic supplementary information (ESI) available: Materials and methods, synthesis of PQDs, STEM image, PL spectra, PL lifetime plot, PL wavelength plot. See DOI: https://doi.org/10.1039/d3cc02621c |