Marek Rychter*ab,
Anna Baranowska-Korczycb and
Janina Luleka
aDepartment of Pharmaceutical Technology, Faculty of Pharmacy, Poznan University of Medical Sciences, Grunwaldzka 6, 60-780 Poznan, Poland. E-mail: mrychter@ump.edu.pl
bNanoBioMedical Center, Adam Mickiewicz University Poznan, Umultowska 85, 61-614 Poznan, Poland
First published on 23rd June 2017
The review discusses the progress in the design and synthesis of bioactive agents incorporated into vascular grafts obtained by the electrospinning process. Electrospun fibers can be applied as an artificial extracellular matrix for tissue engineering and drug delivery, improving tissue regeneration and therapeutic outcomes. A large number of active substances are loaded into the fibers, such as growth factors, heparin, NO donors, statins, antibiotics or anti-inflammatory agents. There are various methods for bioactive substance incorporation including direct blending, emulsion, and coaxial electrospinning as well as covalent and non-covalent binding of the bioactive molecules to the fiber surface. The release mechanism of the drug depends on the synthesis route, active substance properties, and polymer matrix nature. The electrospun materials represent a very promising building block for the fabrication of effective vascular prosthesis in the near future.
In recent years, tissue-engineered vascular grafts capable of inducing neovascularization process have gained huge interest.6–8 Several reports related to scaffold-free grafts and their formation from biodegradable materials with high compatibility and similarity to surrounding and autologous tissue have been noted.9–11 To design effective and efficient polymer-based vascular grafts, their properties should be similar to natural blood vessels, including thrombotic resistance and sufficient mechanical strength. Additionally, they need to be capable of inducing endothelial coverage, followed by gradual degradation till total resorption with full tissue regeneration.12 Moreover, materials involved in graft fabrication should be non-immunogenic and should demonstrate properties promoting cell attachment and growth. Nevertheless, still there are certain unsolved issues connected with scaffold-based systems for vascular tissue engineering, such as lack of sufficient growth factor reservoir13 or improper cell recruitment, differentiation, and proliferation caused by the influence of scaffold nanotopography.14
In order to solve the problem of insufficient revascularization, occurring after graft implantation, a number of studies are currently focused on integrative approach involving the use of polymer scaffold as bioactive substance delivery system. The drugs are incorporated into the polymer matrix or immobilized on the outermost surface to these scaffolds.15 Polymer-based scaffolds demonstrate characteristics of advanced drug delivery systems for cardiovascular diseases treatment, including high loading capacity, high loading efficiency of single and multiple active substances. Moreover, they prevent fast release and rapid clearance of labile compounds e.g. growth factors, which significantly improve their delivery profile.16 It was found that the natural, as well as synthetic compounds, have demonstrated the ability to originate revascularization process. Advanced scaffolds have combined advantages of synthetic polymers including high mechanical durability and high resistance to processing conditions with an abundance of cell binding sites of natural polymers in order to improve overall biocompatibility.7,17
This paper reviews the synthesis and properties of polymer-based scaffolds and effects of their use as bioactive substance delivery materials in vascular tissue engineering. The discussed data are focused on the electrospinning process and its considerable interest in vascular tissue engineering. The study provides new insights into electrospun materials and their application as bioactive substance delivery base with a special attention payed to the treatment of cardiovascular conditions. In this contribution, electrospinning is presented as the most effective, efficient and low-cost method for vascular graft fabrication and development. Additionally, several techniques of active substance incorporation and immobilization to electrospun materials are also provided. The release mechanism of the active substance from polymer-based scaffolds is also presented. This review indicates that polymer electrospun fiber materials offer a great potential as vascular grafts for tissue engineering.
Electrospinning process allows to obtain the fibers characterized by a different diameter, from nano- to micro-meters, controlled by process parameters. This method can produce composite fibers depending on the formulation of starting polymer solution.18 However, synthetic polymer degradation time should be appropriate for cell infiltration and tissue restoration guided by electrospun vascular graft.19 The natural polymers, such as collagen, elastin or gelatin, are widely used as an additional component to increase cell attachment.20
During electrospinning process, the syringe containing polymer solution is connected to a syringe pump, which is responsible for a constant and controllable fed rate. Fig. 1 presents a scheme of a typical electrospinning setup with a rotating drum collector. In general, the mechanism behind electrospinning technique is based on the electrostatic force, which is used to stretch the solution ejected from a spinneret. When a high voltage is applied to a metallic needle, a repulsive force is formed, as the induced charges are evenly distributed over the surface of the polymer drop, which is coming out from the metallic needle. When the electrostatic forces exceed the surface tension of the viscoelastic solution, the jet bursts from the spinneret. As the elongation phase continues the location of charge in formed jet starts to change. This process of continuous bending causes the jet to become unstable which results in a number of bending instabilities, which play a crucial role in the reduction of jet diameter.21 In an electric field the solvent evaporates during jet stretching process and finally, solutes solidify on the collector.22
Fig. 1 Scheme of basic electrospinning setup for vascular graft preparation with a graphic representation of the effect of high voltage on electrospun polymer solution. |
In order to dissolve the polymers for electrospinning process, different organic solvents are used. However, solvents are only utilized for manufacturing purposes. Therefore, in the case of electrospun cell scaffolds they should be removed, to the highest extent possible to limit the potential toxicity of their residues. The safety data for residual solvent levels are presented in Pharmacopeia23 and based on this data they are divided into three classes. In the case of the electrospinning technique, the most desirable organic solvents which can be used for tissue engineering purposes are classified to class 2 or class 3 which both are characterized by a limited toxicity.
The electrospinning is a highly modifiable technique for which a number of different electrospinning set-ups were developed including a rotating drum collector, which is applied to tubular structures preparation used as vascular grafts (Fig. 1). This approach provides an efficient solution for producing tubular structures of various sizes. The external diameter of drum collector corresponds to the internal diameter of produced structure. However, methods of electrospun material detachment from rotating drum collector were rarely reported in detail. Some insightful comments on different reported approaches were described by Errico et al. which could be helpful to develop a suitable methodology for tubular structure production for vascular grafts application.24
One of the advantages of a rotating drum collector is the fact that it is capable of orienting fibers circumferentially which is crucial in the development of electrospun vascular graft. Aligned fibers instead of randomly oriented ones are also obtained by either varying the rotating collector parameters or applying additional magnetic or electric field frames.21 Uniaxial aligned fibers have anisotropic tensile properties, which redistributes tensile force equally over produced structure, which would be vital for developing vascular grafts which need to withstand high pressure after their implantation.25 Fibrous scaffolds produced by electrospinning, not only have directional mechanical properties but also can facilitate the orientation and attachment of cells to the fibers. The structures obtained by electrospinning technique have a great potential in mimicking the extracellular matrix (ECM),26 because produced fibers are in the size range of ECM present in natural tissues of living organisms.
Process parameter like higher collector rotation speeds could contribute to greater uniformity in fibers diameter and thus more homogenous mechanical properties of single fibers which have implications in tissue regeneration at the cellular level. As the cell in vivo requires mechanical interaction with ECM to achieve its physiological function like differentiation or tissue restoration, improved mechanical equilibrium of artificial vascular graft will be supportive in neo-tissue formation. Therefore, it is important to consider nano- or micro-mechanical properties of vascular grafts produced by rotating drum collector, due to their impact on cell function and tissue restoration.
Additionally, electrospun fibrous vascular grafts have high surface area and high loading capability which expand their use into drug delivery systems. Furthermore, the arrangement of fibers protects the incorporated bioactive molecules, provides means for their localized delivery and simultaneously limits the general side effects of traditional drug administration.
Incorporation method | Material–polymer/solvent | Bioactive substance | Release period | Mechanical tests | In vitro results | Ref. |
---|---|---|---|---|---|---|
Physical adsorption | Gelatin B/hexafluoroisopropanol | bFGF | 1 hour | — | HUVEC proliferation directly proportional to bFGF concentrations | 68 |
PCL & gelatin/hexafluoroisopropanol | Heparinization + lysozyme | — | Crosslinking improves Young modulus | hSMC attachment and proliferation improved by heparin conjugation | 34 | |
PCL & chitosan/chloroform:methanol & acetic acid:dimethyl sulfoxide | Heparin | 37 days | Heparin adsorption enhanced Young modulus | HUVEC proliferation improved with heparin loading; SMC proliferation decreased by chitosan properties and probably heparin; platelet adhesion significantly inhibited | 80 | |
PCL & gelatin/hexafluoroisopropanol | Heparinization + PDGF–bb | 20 days | — | hSMC proliferation facilitated by PDGF–BB binding to heparin | 73 | |
PCL & gelatin/hexafluoroisopropanol | Heparinization + VEGF | 25 days | Heparinization enhances Young modulus | HUVEC proliferation directly proportional to VEGF loading, improved by binding to heparin | 51 | |
PCL/chloroform:methanol | NO releasing PAS | 28 days | — | HUVEC adhesion enhanced by NO donor loading; AoSMC proliferation reduced | 95 | |
Chemical immobilization | PLLA/hexafluoroisopropanol | Heparinization | — | — | BAEC infiltration increased by plasma treatment followed by heparinization; platelet adhesion limited | 33 |
PCL/methylene chloride:methanol | Biotinization + galactosidase | 3 days (70 h) | Enzyme loading moderately reduces Young modulus and elongation at break | — | 92 | |
PCL/chloroform:methanol | VEGF | — | — | iHUVEC proliferation enhanced on VEGF functionalized scaffold; pHUVEC number reduction over time | 36 | |
Direct blending | PCL/chloroform | Acetylsalicylic acid | 7 days | ASA loading increases Young modulus and stress at break | Platelet adhesion limited even at low ASA content | 98 |
SF & PEO/water | Dexamethasone | 8 days | — | PIEC protected from LPS induced damage by DEX release | 117 | |
BPU/hexafluoroisopropanol | Dipyridamol | 91 days | Dipyridamol loading increases Young modulus and overall strength | HASMC proliferation inhibited; HAEC growth improved by dipyridamole loading; platelet adhesion limited | 102 | |
PCL/dichloromethane:methanol solvent mixture | Heparin | 14 days | — | VSMC growth reduced by heparin addition | 37 | |
PCL/chloroform:ethanol | Paclitaxel | 27 days | PTX loading improves mechanical properties | — | 106 | |
PLGA/hexafluoroisopropanol | Rosuvastatin | 30 days | — | Platelet adhesion decrease directly proportional to rosuvastatin loading | 112 | |
PLGA/hexafluoroisopropanol | Vancomycine | 35 days | — | — | 118 | |
Direct blending/emulsion electrospinning | PELCL/chloroform:tetrafluoroethylene, PLGA/chloroform:tetrafluoroethylene, PCL/chloroform:dimethyofuran, gelatin/tetrafluoroethylene | VEGF, PDGF | 56 days | Multilayer structure improves mechanical properties | EC proliferation enhanced by VEGF; SMC proliferation controlled by dual growth factor delivery | 64 |
Emulsion electrospinning | Core: plant oil, shell: SF & PEO/water | Core: dexamethasone | 8 days | — | PIEC protected from LPS induced damage by DEX release | 117 |
Core: BSA or dextran, shell: PLCL/chloroform | Core: VEGF | 28 days | — | MSC proliferation without differentiation | 42 | |
Core: PBS, shell: PELA & PEG/chloroform | Core: pVEGF and pbFGF polyplexes | 28 days | — | HUVEC growth rate depended on the cytotoxicity of polyplexes and transfect cell GF secretion | 41 | |
Emulsion/coaxial electrospinning | Internal: hydrogel & PELCL, external: emulsion & PELCL | Internal: VEGF, external: PDGF | 12 days | — | EC-rapid growth in the first 6 days; SMC fast growth after 6th day | 40 |
Coaxial electrospinning | Core: distilled water, shell: P(LLA-CL)/tetrafluoroethylene | Core: heparin | 14 days | Heparin encapsulation lowers ultimate strength and strain | EC covered entirely inner graft surface after 7 days | 78 |
Core: PCL or gelatine/tetrahydrofuran, shell: PCL/chloroform:methanol | Core: DBHD/N2O2 | 2.5 days | — | Platelet activation reduced by NO release | 44 |
Bioactive substance | Bioactive substance load | Incorporation method | Material–polymer/solvent | Animal model | Implantation site | Weeks in vivo | Patency | Ref. | |
---|---|---|---|---|---|---|---|---|---|
Growth factors | VEGF | — | Physical adsorption | PCL & gelatin/hexafluoroisopropanol | Rat | Subcutaneous pocket | 4 weeks | — | 51 |
VEGF, PDGF | 0.56 ng mg−1, 0.54 ng mg−1 | Direct blending/emulsion electrospinning | PELCL/chloroform:tetrafluoroethylene, PLGA/chloroform:tetrafluoroethylene, PCL/chloroform:dimethyofuran, gelatin/tetrafluoroethylene | Rabbit | Left common carotid artery | 8 weeks | 100% after 8 weeks | 64 | |
Core: pVEGF & pbFGF polyplexes | — | Emulsion electrospinning | Core: PBS, shell: PELA & PEG/chloroform | Rat | Subcutaneous pocket | 4 weeks | — | 39 | |
Internal: VEGF, external: PDGF | 1.3 ng mg−1, 1.4 ng mg−1 | Emulsion/coaxial electrospinning | Internal: hydrogel & PELCL, external: emulsion & PELCL | Rabbit | Carotid artery | 4 weeks | 100% after 2 weeks, 100% after 4 weeks | 40 | |
Heparin | Heparin | 68.68 ± 1.57 μg cm−2 | Physical adsorption | PCL & chitosan/chloroform:methanol & acetic acid:dimethyl sulfoxide | Rat | Abdominal aorta | 4 weeks | 75% after 4 weeks | 80 |
Core: heparin | 0.012 g per graft | Coaxial electrospinning | Core: distilled water, shell: P(LLA-CL)/tetrafluoroethylene | Canine | Bilateral femoral arteries | 13 weeks (3 months) | 100% after 2 weeks, 75% after 13 weeks | 78 | |
NO donors | Galactosidase + gal-NONOate | 0.018 mg per graft | Physical adsorption | PCL/methylene chloride:methanol | Rat | Abdominal aorta | 4 weeks (30 days) | 100% after 2 weeks, 80% after 4 weeks | 92 |
Active pharmaceutical ingredients | Paclitaxel | 50 to 200 μg per graft | Direct blending | PCL/chloroform:ethanol | Rat | Abdominal aorta | 24 weeks | 100% after 24 weeks | 14 |
Rosuvastatin | 500 & 1250 μg per graft | Direct blending | PLGA/hexafluoroisopropanol | Rabbit | Femoral artery | 4 weeks (28 days) | — | 112 | |
Vancomycin | — | Direct blending | PLGA/hexafluoroisopropanol | Rabbit | Subcutaneous pocket | 5 weeks | — | 118 |
This approach is characterized by relatively mild conditions of the procedure which make it a perfect solution for labile compounds immobilization including proteins like for example growth factors used to improve vascular tissue restoration (Tables 1 and 2). Despite a number of advantages, the non-covalent binding technique is also characterized by a rapid dissolution of bioactive substance from polymer fibers and poor control over its release kinetics. However, in the case of hydrophilic substances like growth factors, which often cause burst release, various methods of surface modification were developed. One of the most interesting is fiber surface heparinization. In the first step, polymer graft surface is usually treated with plasma in order to increase hydrophilicity and activate surface for further modification of amine groups.32,33 After the surface functionalization with heparin, improved affinity towards various growth factors is used to adsorb bioactive molecules via electrostatic interaction on the fiber surface. No-plasma treatment methods were also developed. In such case, electrospun fibers underwent cross-linking procedures which also resulted in free amine groups on fibers surface.34
Direct blending is an optimal solution when bioactive substance and polymer show similar solubility in the solvent. However, the problem of varying solubility might be addressed by dissolving the bioactive substance in solvent miscible with polymer solution.37
In the case of similar solubility in organic solvent, the bioactive substance usually is incorporated directly into the structure of electrospun fibers. Depending on the relation between graft composition and porosity, the release profile may be easily tuned. Perhaps the most serious disadvantage of this incorporation technique involves a high risk of burst release most often caused by bioactive substance location on the surface or near the surface of electrospun fibers.27,38 This method is frequently applied for bioactive substance loading to electrospun vascular grafts (Tables 1 and 2).
When the high voltage is applied fibers with vesicles containing dispersed part of the emulsion in more easily solidifying dispersion medium can be formed. Core–shell fibers can be also formed as a result of relatively fast evaporation of solvent from the region close to the surface in comparison to the central part of the polymer jet. In such circumstances, the viscosity gradient of the core and shell segments changes dramatically and causes a slower rate of the evaporation process in the central part of the jet. In both cases solidified polymer acts as a hydrophobic barrier which provides protection from external conditions for labile bioactive substances including proteins. It was shown during in vitro experiments that burst release effect was limited by applying emulsion electrospinning, therefore it could potentially limit leaching-out effect of shear stress encountered in vivo by bioactive substance loaded vascular grafts.40–42 Examples of its use in vascular graft development are presented in Tables 1 and 2.
This technique enables the synthesis of the fibers made from substances not usually applied for electrospinning process of vascular grafts.43 The core–shell structures are usually similar to the fibers which could be obtained by emulsion electrospinning, where the hydrophobic shell covers and protects the bioactive substances located in the hydrophilic core.
This design improvement reduces burst effect and allows dual-drug loading to both core and shell layers.19 The contact of bioactive substances and organic solvents used in electrospinning is significantly reduced which makes this method more valuable option for labile substance processing (Tables 1 and 2). Moreover, core and shell diameters of the fibers can be controlled and design by changing the process parameters including the flow rate and applied voltage. Coaxial electrospinning reveals better processing versatility compared with emulsion electrospinning or any other form of bioactive substance incorporation method.40,44
The diffusion from polymeric fibers occurs through direct release from the polymer matrix and diffusion across a barrier formed by polymer itself.45 In this diffusion-based mechanism, the release process of molecularly dispersed bioactive substances from the electrospun graft includes passage of bioactive substance molecules through pores within polymer matrix and passage between polymer chains. Both types of diffusion are influenced by the structure of a single fiber and will be the dominant release mechanism in the early stages after vascular graft implantation. The rate of diffusion depends on various factors including crystallinity, physicochemical properties, partition coefficient, the amount of bioactive substance loaded, fiber diameter and its structure.
Most of the polymers used in electrospinning are in semi-crystalline state and form amorphous regions during the spinning process. Bioactive molecules are usually located in the amorphous regions of the semi-crystalline polymers and the initial drug release occurs mostly from these regions of the fibers.37 An increase in crystallinity results in a decrease in the diffusion rate of the bioactive substance. It is attributed to the water penetration of semi-crystalline polymers which initially occurs in the amorphous regions.46 The water infusion from the amorphous regions facilitates the release process and increases the diffusion rate.
The release of bioactive substances from electrospun constructs depends on substrate properties therefore when designing bioactive substance loaded vascular graft both physical and chemical properties of the active substance47 and polymer,48 must be considered.
Hydrophobic substances loaded to electrospun grafts show lower tendency to be distributed in the blood and therefore have slower clearance as their diffusion rate is slow. Contrary, hydrophilic substances have a higher attraction towards aqueous medium, therefore, their clearance is high whereas retention within graft is limited due to fast diffusion rate. In the case of polymer or polymer blends, their hydrophilicity will influence the wettability and aqueous medium penetration through the whole structure.
Another important issue closely related to physicochemical properties of the polymer and bioactive substances is partition coefficient.31,36 The partition coefficient of bioactive substance and polymer can influence bioactive substance distribution within the polymer matrix or near the surface of electrospun fibers. Therefore, it can significantly influence the release rate after graft implantation leading to a frequently encountered problem of initial fast release phase also known as a burst effect. It was found that for some polymer systems the first stage of bioactive substance release is very fast and is responsible for a rapid release of a large part of incorporated dosage.40–42 Additionally, it was found that higher drug loading contributes to a higher risk of burst effect. Therefore, a large part of loaded dosage which rapidly diffuses from the vascular graft may cause severe local toxicity shortly after graft implantation and therefore formulations with high drug loadings should be developed with caution. The initial fast release phase is also typical for fibers loaded with bioactive substance via post-electrospinning incorporation techniques where fast desorption process from the fiber surface drives a rapid depletion of bioactive substance loading.43,49,50 However, covalent immobilization in comparison to non-covalent methods of bioactive substance immobilization, significantly limits the burst release effect.51 In direct blending technique, a high voltage applied during electrospinning process influences the homogenous polymer mixture in the spinneret and can locate evenly distributed bioactive substance near the surface of produced fibers. This process depends vastly on the polarization susceptibility and solubility of incorporated substances but is the main cause of the burst release effect encountered in loaded vascular grafts obtained via direct blending technique.52
The emulsion and coaxial electrospinning are both applied to prevent burst release effect. The vesicle or core–shell structure formation causes a change in diffusion mechanism as the layers of solidified polymer acts as a diffusion barrier whereas vesicles or core becomes the bioactive substance reservoir. Changes in the elongation of the core or vesicle distribution, has a tremendous impact on the release profile as a thinner core diameter or a greater vesicle distribution causes thicker polymer-based barrier which can decrease the release rate of bioactive molecules.42 Therefore, in the case of emulsion and coaxial electrospinning, the initial stages the release profile is mostly affected by the diffusivity of bioactive substance through the polymer barrier.
Discussed burst release phase is followed by a sustained release phase with slower release rate mediated initially also by the diffusion-based mechanism. Sustained release phase is mainly a result of an increasing diffusion distance from the internal part of polymer matrix to its external regions.
The polymers used in electrospinning technique for grafting purposes are biodegradable. In long-term, the degradation process leads to subsequent surface or bulk erosion indicated by a decrease in polymer mass or fiber size which happens along a gradual regeneration of normal living tissue.7 The degradation process of the polymers used to electrospun vascular grafts is a relatively long process, therefore erosion/degradation processes are dominant release mechanisms at the last stages of graft lifespan.53 In long-term after graft implantation, erosion-based mechanism of polymer matrix gradually decreases the diffusion distance and slowly becomes the dominant force behind the release of the bioactive substance from electrospun fibers. In the case of emulsion and coaxial electrospinning degradation of polymer chains and a gradual erosion of polymer barrier affects the passage distance and thus the diffusivity of the bioactive substance. However, when designing a long-term release medical device like bioactive substance loaded vascular graft, the impact of in vivo conditions should not be neglected. It was found that proteinase K and lipase PS enhance PLLA and PCL hydrolytic degradation which could increase the importance of enzyme-stimulated degradation in the release mechanism of bioactive substance in earlier stages of vascular graft lifespan.54
Based on presented data, both – diffusion and degradation-related processes should be considered as potential release mechanisms of bioactive substance from electrospun grafts. In the case of long-term application of vascular grafts, the diffusion, as well as erosion/degradation, contributes to the release process. The dominant release mechanism depends on permeability, wettability and degradation profile of the polymer. The drug release from polymer graft with high permeability and characterized by a slow degradation rate is usually dominated by diffusion-driven mechanisms which produces typical bi-phase release profile. In the case when polymers with low permeability and fast degradation are applied, drug release process is more complex and is regulated by both mechanisms, resulting in a tri-phase release profile with fast release phase, diffusion-driven sustained phase and erosion-driven phase.55,56
The electrospun polymer matrix is an efficient form of drug delivery system which can provide sustained and localized release (Tables 1 and 2). Additionally, modifications of polymer matrix improve incorporation and immobilization of labile substances like growth factors or drugs for vessel regeneration.
Due to its remarkable importance of VEGF in angiogenesis, a study conducted by Guex et al.36 examined the possibility of VEGF immobilization on polymer scaffold for vascular tissue engineering (Table 1). In her study, Guex used a flexible linker molecule in order to increase VEGF immobilization efficiency by reducing steric hindrance.36 Cell studies on immortalized human umbilical vein endothelial cells (iHUVEC) revealed that the cells cultured nine days on VEGF immobilized scaffolds provided sustained mitogenic action. The number of cells was significantly higher for scaffold with VEGF in comparison to non-functionalized ones. Another important finding of this group demonstrated that iHUVEC attachment was increased on micro-sized fibers, in comparison to nano-sized ones which failed to enhance proliferation rate even after nine days.
A different method of active substance incorporation was selected by another group which decided to incorporate VEGF as an emulsion to PLCL fibers (Table 1).42 VEGF was dissolved in bovine serum albumin (BSA) or dextran to form a solution which then was emulsified with PLCL solution in chloroform. Both dextran62 and BSA63 have demonstrated their stability in previous studies. Release study conducted by Tian et al. showed that dextran and BSA presence affected the release profile only during the first 24 h. Mesenchymal stem cells (MSC) study showed no significant difference between core–shell scaffolds and pure PLCL scaffolds. However, after 10 days in both formulations of core–shell grafts, the proliferation of MSC was higher than on normal PLCL scaffolds. Growth factors could also influence the differentiation process of stem cells to other cell types.42 Despite prolonged VEGF release for 28 days, the study of Tian et al. did not demonstrate differentiation of entire MSC population to cardiomyocytes.
In another major study, Zhang et al.40 developed double-layered membrane composed of chitosan hydrogel/poly(ethylene glycol)-b-poly(L-lactide-co-caprolactone) (PELCL) electrospun membrane loaded with VEGF as the internal layer and emulsion/PELCL electrospun membrane loaded with PDGF as the external layer (Tables 1 and 2). In this study, coaxial electrospinning was utilized to obtain double-layered scaffolds. The cumulative release of VEGF after 6 days was 66%, which demonstrated that the release was more rapid than for platelet-derived growth factor (PDGF), which cumulative release of 38% indicated more sustained release pattern. Two different types of cells were cultured on electrospun scaffolds and on tissue-culture polystyrene (TCPS) as a control. Endothelial cells (EC) rapidly adhered and proliferated in the first 6 days, whereas smooth muscle cells (SMC) proliferation rate increased significantly after the 6th day. The relationship between growth factor release from emulsion/coaxial electrospun materials (E/C), without and with different amount of heparin (P1 or P2), and vascular cells proliferation was determined (Fig. 3A–D).
Fig. 3 The relationship between PDGF release behaviors and the VSMCs proliferation. (A) Release profiles of PDGF from the electrospun membranes; (B) CCK-8 value of VSMCs cultured on different samples (p < 0.05); (C) SEM micrographs for VSMCs spreading on the different electrospun membranes on the 6th day; (D) LCSM micrographs for ECM secretion of VSMCs cultured on the different electrospun membranes on day 6 (1000 Å) (green, FITC labeled fibronectin; blue, DAPI stained nuclei). Reproduced from ref. 40 with permission from Elsevier. |
In vivo studies of double layered graft implanted for 4 weeks as rabbit carotid artery replacement provided many useful findings. Neither rupture during its surgical insertion nor leakage during postoperative period was detected. The result obtained after graft explantation indicated endothelialization of luminal surface and an external layer of SMCs, however at the different percentage at different end points. Moreover, the histological analysis of cell coverage was consistent with growth factor release studies, as EC responsible for vascular homeostasis proliferated rapidly in the first week after implantation whereas SMC proliferated in the following weeks after insertion. Nevertheless, both cell types attached only to luminal end external part of the graft, which probably was the effect of insufficient porosity of the scaffold.40
A different approach was chosen by Han et al. who co-electrospun various polymers with gelatin to obtain multilayered scaffolds loaded with VEGF via direct blending and with PDGF via emulsion electrospinning (Tables 1 and 2).64 In vitro release studies demonstrated that VEGF cumulative release was higher than PDGF, which was probably caused by different loading methods and different polymers used to produce loaded fibers. This behavior was beneficial for temporal delivery of growth factors and further tissue regeneration process. Gelatin selected as a material for fiber formation and fast release of VEGF promoted adhesion and proliferation of EC on the luminal surface of electrospun scaffolds which was confirmed by increased expression of a cluster of differentiation 31 (CD31).65
Montero group investigated a new approach to fabricating aligned gelatin fibers with incorporated basic fibroblast growth factor (bFGF) (Table 1).68 The growth factor was physically immobilized within the gelatin scaffolds. The higher alignment of the fibers caused a 28% increase in an in vitro angiogenesis in comparison to scaffolds consisting of randomly oriented fibers. Moreover, greater fiber alignment was found to increase bFGF release by 11% from electrospun scaffolds with aligned fibers, which could be attributed to the swelling profiles of these fibers.
The more complex approach was applied by other researchers who managed to incorporate multiple polyplexes containing bFGF and VEGF encoding plasmids to electrospun constructs. The mixture containing growth factor encoding polyplexes were suspended in phosphate buffered saline (PBS) and emulsified in chloroform containing polyethylene oxide/polylactic acid copolymer (PELA) and polyethylene glycol (PEG) which were afterward electrospun. In this particular case, polyplexes of plasmid DNA (pDNA) were suspected to act as protective agents against critical process parameters.69 The release profile of obtained dual-loaded mats had three distinctive phases: an initial burst release in the first 12 h of the experiment, followed by a sustained release for 3 weeks and 1 week period of gradually decreasing release rate. Initial burst release was probably caused by polyplexes deposition on the surface or near to the fiber surface, which contributed to high release rate in the first hours of the release studies. After 3 weeks of a gradual dissolution of PEG, an increase in the contact surface of a polymer matrix with surrounding medium was noticed, which accelerated further polymer degradation thus enhancing the polyplexes release from the fibers.
A broader perspective of pDNA polyplexes potential was outlined by in vitro cell studies which revealed that their incorporation decreased the cell attachment to the polyplex-loaded fibers. Based on these result authors concluded that the ability to properly guide the cell growth of such constructs, depend both on initial cytotoxicity of incorporated plasmid DNA and transfection rate responsible for growth factors production and thus their effect.
In another study FGF-9 was incorporated into the electrospun structures by both blend and emulsification technique. Mats obtained by both techniques showed no burst release during release study which indicated perfect entrapment of bioactive molecules within polymer fibers. Both methods of incorporation led to a sustained release of FGF-9 for 28 days. However, the cumulative release for emulsion electrospun fibers was lower compared to blend electrospun fibers and reached 37% at the end of release study. There were no significant differences in bioactivity of NIH-3T3 fibroblasts cultured on fibers prepared either by blending or emulsion techniques, while FGF-9 release profiles from both types of fibers had different characteristic.70
Despite being mostly used in combination with other growth factors, PDGF is also regarded as a potential candidate for a bioactive component of electrospun tissue-engineered vascular graft (TEVG). Different methods of PDGF incorporation to the electrospun graft (Tables 1 and 2) have been utilized including double-layered scaffold formation40 or immobilization on heparinized scaffold.73
In the study set out to determine PGDF effect on cell migration,74 coaxial electrospinning method was used to fabricate a PDGF-containing PLCL scaffold for sustained release of growth factor. All three structures spun with different inner phase flow rate showed burst release of PDGF–BB in the first 2 days of the experiment, which was followed by a sustained release till the 28th day. In vitro studies conducted on VSMC revealed satisfying cell attachment when compared to normal PLCL fibers without growth factor loading.74
A research conducted by Luong-Van et al.37 produced heparin loaded PCL scaffolds by utilizing a modified direct blending technique where a non-soluble in methanol heparin was initially dissolved in water, which was then mixed with dichloromethane, before adding it to the methanol solution (Table 1). Accordingly, to other studies76,77 heparin salt addition influenced the charge deposition along the jet which enhanced its elongation during spinning process thus producing fibers with a smaller diameter. Initial, fast release rate of heparin may be beneficial in preventing the proliferation of VSMC shortly after the injury caused by endovascular operations. Pro-inflammatory action assay revealed that PCL fibers did not stimulate tumor necrosis factor α (TNF-α) production by the macrophages.37
Other team created heparin loaded scaffolds by using co-axial electrospinning technique (Tables 1 and 2) where the fiber core contained heparin dissolved in water whereas shell was made from poly(L-lactide-co-ε-caprolactone) (P(LLA-CL)).78 The release of heparin had a typical bi-phase profile with initial fast phase release followed by sustained release for 14 days. The canine model was used for long-term in vivo studies (Fig. 4A–C), due to the fact that the structure and mechanical properties of femoral artery are similar to those found in human vessels.78,79 Fig. 4A shows graft implantation procedure and graft implantation site inspection (Fig. 4B and C) by digital subtraction angiography (DSA) and color Doppler flow imaging (CDFI).
Fig. 4 (A) Surgical implantation of the electrospun tubular graft into the femoral artery of Beagle dog. Typical DSA and CDFI inspection of (B) heparin-loaded and (C) pre-endothelialized grafts after 3 months: the left femoral artery was replaced by heparin-loaded or pre-endothelialized graft, and the right one was replaced by P(LLA-CL) graft. Blood flow in the left femoral artery was further traced by the CDFI image. Reprinted with permission from C. Huang, S. Wang, L. Qiu, Q. Ke, W. Zhai and X. Mo, ACS Appl. Mater. Interfaces, 2013, 5, 2220–2226.78 Copyright 2013 American Chemical Society. |
Before implantation, scaffolds underwent dynamic endothelialization. Results showed that pre-implantation endothelialization and heparin incorporation increased the patency rate about 12.5% for normal scaffolds and 75% for modified scaffolds after 3 months. Non-endothelialized heparin loaded scaffolds were covered with endothelial cell only at the proximal end which was probably caused by slow cell migration rate with the blood flow.
In a recently published study, PCL and chitosan scaffold was produced by utilizing the co-electrospinning technique.80 Heparin was physically adsorbed on the surface of produced fibers (Table 1). This research found that heparin load can be controlled by changing the chitosan ratio within the scaffold. Moreover, due to multiple ionic bonds formed between the polymer chains of electrospun fibers, burst release was limited. The sustained release was observed for the system, from which only 26% of total heparin load was released in one month period. Heparin adsorption on the surface of the fibers extended both activated partial thromboplastin time (APTT) and thrombin time (TT) thus demonstrating high haemo-compatibility. Morphological study of explanted grafts from a rat model revealed full endothelial coverage in heparin loaded scaffolds after 4 weeks.80 In contrast to normal PCL and chitosan grafts, all patent heparin loaded grafts showed clean lumen with no sign of thrombus formation.
Heparin use as a linker molecule was studied by Cheng.33 The study verified the platelet attachment to electrospun PLA scaffolds conjugated with heparin and showed that plasma-treated scaffolds conjugated with heparin exhibited a meaningful reduction in platelet aggregation when comparing to normal PLA scaffolds. Independently of the amount of conjugated heparin all modified scaffolds demonstrated increased bovine aorta endothelial cells (BAEC) attachment. These findings were consistent with other studies which indicated that negative charge of heparin and its water retaining capability, produce a hydrophilic environment suitable for cells.83 Since NH2 groups are considered to be potential linkers for other biomolecules such surface functionalization of currently used biodegradable polymers can improve their biocompatibility.
A similar approach was used in other research, however, no plasma treatment was involved in the heparin conjugation reaction (Table 1).34 Obtained PCL and gelatin scaffolds were cross-linked. The cross-linking process applied in this study was not only essential because of its direct impact on stability and biomechanics of electrospun polymers,84 but also because it allowed more uniform distribution of heparin molecules. Furthermore, surface modification of electrospun polymer increased the loading efficiency in comparison to non-conjugated scaffolds.
The study focused on heparinization methods was continued and resulted in an immobilization of PDGF–BB into PCL/gelatin scaffold.85 The release of growth factors from heparin-conjugated structures occurred during initial phase mainly by dissociation of surface absorbed growth factor or by sustained release depending on the thermodynamic equilibrium.85 In vitro release studies showed that bioactive substance was bound to the heparinized graft by electrostatic forces, which according to the authors was the main factor contributing to a sustained dissociation of PDGF–BB from the surface of the fibers. Obtained data revealed that the release of PDGF was diameter-dependent, where fibers with small diameter released bioactive molecules at a faster rate. The probable reason for such finding was connected with a higher surface area of small diameter fibers, which was exposed to the release medium.86 Furthermore, the presence of growth factors bonded to electrospun construct was detectable even after 20 days, demonstrating the capability of heparinized scaffolds to release PDGF–BB over an extended period of time. According to this study,85 stable heparin conjugation with growth factors limited previously described antiproliferative effect of heparin on vascular smooth muscle cells.75,87
A similar method was also applied to immobilize VEGF to heparinized PCL/gelatin structures.51 Sustained release of VEGF from heparinized scaffolds was observed for 25 days, which proved high binding affinity between VEGF and heparin. The in vivo angiogenesis study in rats revealed that after 4 weeks implanted scaffold was fully covered with cells, and VEGF loading increased the vessel density in the explanted graft (Tables 1 and 2).
In a study conducted by Zhang et al., coaxial electrospinning was used to obtain core–shell fibers containing NO donor – (Z)-1-{N-butyl-N-[6-(N-butylammo-niohexyl)amino]}-diazen-1-ium-1,2-diolate (DBHD/N2O2).44 In physiological conditions this particular NO donor undergoes a spontaneous degradation with a subsequent NO release, therefore it can be regarded as a potential prodrug, where NO is an active substance responsible for clinical relevant outcomes. DBHD/N2O2 itself is regarded as relatively toxic substance, thus its encapsulation within the core–shell structure of fibers was aimed to reduce its toxicity. In this study, the external layer of fibers was produced from either PCL or gelatin (Table 1). The release studies of NO from DBHD/N2O2 incorporated to electrospun fibers revealed maximum NO flux between 2 and 5 h. The continuous release from core–shell fibers was sustained for almost 60 h which was similar to non-axially spun fibers. Nevertheless, after initial burst release, core–shell structure managed to slow down the release rate in comparison to a non-coaxial structure. According to MTT assay, the cytotoxicity of DBHD/N2O2 containing non-coaxially spun scaffolds, was apparent. Coaxial electrospinning produced core–shell structures with PCL or gelatin shell which brought more stable NO release and improved cell viability. Additionally, PCL and gelatin formed a barrier which helped to avoid direct contact of DBHD/N2O2 with cells.44
In another recent study, a novel enzyme prodrug therapy (EZT) approach was adopted in electrospun vascular grafts. This approach provides means for a localized and targeted prodrug delivery.90,91 In a study conducted by Wang et al.92 electrospun vascular graft was immobilized with galactosidase (Table 1), which is capable of decomposing intravenously administered NO donor with a simultaneous release of NO at the graft implantation site.93 NO donor used in this study was galactoside NONOate (Gal-NONOate), which after initial decomposition conducted by a surface-immobilized enzyme, left unbounded NONOate which spontaneously decomposed to NO.94 Ex vivo catalytic properties evaluation based on an arteriovenous shunt procedure indicated that after NO prodrug administration, fluorescent dye-labeled grafts demonstrated evident green fluorescence in contrast to the control groups, indicating localized release of NO. Electrospun grafts were implanted as abdominal artery substitutes in rats (Fig. 5A–G), where platelet adhesion (Fig. 5D1, D2, F1 and F2) and graft endothelialization (Fig. 5E1 and E2) was observed. Quantitative analysis revealed that thickness of neotissue and coverage ratio was significantly higher in the experimental group (with Gal-NONOate administration) than in control (without Gal-NONOate administration) after 2 weeks after implantation. However, after one month no significant difference was detected.92
Fig. 5 Implantation of enzyme-functionalized vascular grafts by replacing a part of the rat abdominal aorta (A), and the luminal surface of explanted vascular grafts at day 7 (B1, B2) and day 14 (C1, C2) without (B1, C1) and with (B2, C2) administrated NO-prodrug observed by a stereomicroscope. SEM images show the platelet adhesion and endothelialization of the enzyme-functionalized PCL grafts without (D1, E1) and with NO-prodrug administration (D2, E2) over days 7 (D1, D2) and 14 (E1, E2). CLSM images show the mepacrine-stained platelets adhered on explanted grafts over day 7 without (F1) and with NO-prodrug administration (F2), and the correlative statistical analysis (G). Scale bar is 50 μm. Data are expressed as mean ± SEM. Reproduced from ref. 92 with permission from Elsevier. |
A study conducted by Andukuri et al. produced a hybrid scaffold consisting of electrospun PCL and peptide amphiphiles (PAs).95 In the discussed study two different PA were synthesized. Each of them contained either a laminin-derived Tyr–Ile–Gly–Ser–Arg endothelial cell adhesive ligands (YIGSR) or polylysine sequence (KKKKK) acting as a nitric oxide (NO) donor. After mixing PAs were reacted with pure NO and then self-assembled on the electrospun PCL scaffold to generate a hybrid scaffold (Table 1). Initial burst release occurred during the first 48 h and was followed by 4 weeks of sustained release. Cell studies conducted on HUVEC and aorta smooth muscle cells (AoSMC) showed that hybrid scaffolds with NO donor enhanced endothelial cells adhesion to scaffold fibers, while simultaneously they did not support smooth muscle cell adhesion. These findings are consistent with other research on the NO control over vascular cells homeostasis.96 Moreover, NO-releasing hybrid scaffolds were found to decrease platelet adhesion, thus limiting the potential thrombosis.
Dipyridamole (DPA) is an antithrombotic drug which is able to reduce platelet aggregation and over-proliferation of SMC by inhibiting adenosine uptake via phosphodiesterase activation inhibition in these cells, resulting in the intracellular increase of cyclic adenosine monophosphate (cAMP) and cGMP levels.99 The same mechanism was reported to protect endothelial cells and stimulate their growth.99,100 Based on these pleiotropic effects of DPA it was hypothesized that its incorporation may improve the clinical outcome of electrospun vascular grafts.101
Direct blend technique was used to incorporate DPA into biodegradable polyurethane urea (BPU) electrospun scaffolds (Table 1).102 Obtained structures showed improved mechanical properties of DPA incorporated scaffolds which according to the authors was a result of hydrogen bond formation between hydroxyl groups of DPA and urea groups of BPU. The burst release was limited, followed by a sustained release of DPA for 91 days with only few fiber defects found by SEM micrographs analysis (Fig. 6A–D).
Fig. 6 (A) In vitro DPA release curves of DPA-loaded BPU scaffolds up to 91 days in PBS at 37 °C. SEM images exhibited fiber morphologies of (B) BPU + 2.5% DPA, (C) BPU + 5% DPA and (D) BPU + 10% DPA after 91 day release. Reproduced from ref. 102 with permission from Elsevier. |
Limited burst release effect and long sustained release phase were probably caused by a proper incorporation of hydrophobic DPA which matched hydrophobic moieties of BPU and placed the active substance within the fiber structure. Both 5% and 10% DPA concentration caused SMC proliferation inhibition in a dose-dependent manner which was consistent with another study.103 Moreover, EC proliferation was improved in comparison to normal BPU scaffolds, but exact concentration needed to obtain this effect is still an area of discussion.
Human blood contact assessment was also conducted (Fig. 7A–F). Compared to the BPU alone, the DPA-loaded BPU scaffolds had improved non-thrombogenicity. This study did not show dose dependency of DPA antithrombotic effect, therefore antiproliferative and antithrombogenic effects probably occurred at different dosage of DPA.102
Fig. 7 Digital images to show human blood clot formation with time of (A) human blood, (B) BPU alone in the human blood and (C) BPU + 10% DPA in the human blood. (D) The absorbance at 540 nm of the lysate of human blood contacted with the scaffold. (E) The TAT complex concentration in PPP after the scaffold has been in contact with human blood. The control is human blood alone. (F) Human blood hemolysis percentages of the scaffolds. Reproduced from ref. 102 with permission from Elsevier. |
Lee et al. used electrospun PLGA tubes containing rosuvastatin as a drug delivering coating for bare metal stents (Tables 1 and 2).112 After electrospinning obtained fibrous tube was mounted on the outside of a commercially available bare metal stent. In vitro platelet adhesion to obtained fibers were found to be significantly lower for fiber with 2 and 5 μg mm−2 rosuvastatin than for normal PLGA fibers and the antiplatelet effect was directly proportional to the concentration of the drug. The in vitro drug release studies showed two-phase release profile. The stable and sustained release of rosuvastatin were observed until the 4th week of the experiment. Hybrid stent covered with rosuvastatin containing coating was implanted in the rabbit descending abdominal aorta. In vivo study of endothelial coverage showed that re-endothelialization was significantly greater in 2 and 5 μg mm−2 hybrid stents (95.5 ± 0.4% and 99.1 ± 0.3% respectively) than in rosuvastatin-free hybrid stent (86.0 ± 0.7%). After four weeks, all three groups exhibited significantly different vascular inflammatory responses, where rosuvastatin loaded hybrid stents showed two times lower response than the control one. Such result could be the effect of either drug-induced improved endothelial function or reduced platelet activation.113,114
Similarly, another representative of (HMG-CoA) reductase inhibitors – simvastatin was directly blended and electrospun with polyethylene oxide (PEO). However, the obtained fibers with the highest investigated 1:4 drug-carrier ratio showed a sustained release over a period of 12 h.115
Still, human clinical trials of electrospun vascular grafts are scarce. Nevertheless, some of the current research might help to address some of the issues responsible for such state of matter.
Cell infiltration and proliferation within the vascular graft, just like in physiological angiogenesis are guided by the time-dependent action of different growth factors. However, excessive revascularization may contribute to neointimal hyperplasia which needs to be counterbalanced by suppressing growth factors activity. Sequential delivery of growth factors has been shown to be responsible for proper vascularization process.
Therefore one of the greatest challenges for future vascular grafts is the spatiotemporal delivery of bioactive substances in response to natural signaling triggers.123 This issue is already an area of extensive research thanks to the introduction of stimuli-responsive polymers. Despite being a novelty such polymers are already extensively studied as they may enable a more controllable release of the bioactive substance. Various external triggers may be used to activate to generate a change in polymer structure with subsequent release of the incorporated substance.
As the pH of arterial blood pressure is in a very narrow range between 7.38 and 7.42, pH-responsive fibers can detect and respond to any alterations in pH homeostasis. Polymers containing bonds susceptible to pH fluctuations show faster degradation rate under acidic conditions which facilitate hydrolysis of acetal of ester groups.124 As a result, this degradation-based mechanism increases the elution rate of the bioactive substance from polymer scaffold. In general, in the case of the cardiovascular system, lowered blood pH indicates either inflammation or more severe conditions including myocardial infarction. Therefore, pH could act as a potential trigger for a controllable release of bioactive substances from the implanted graft.125,126 Additionally, it could enable spatiotemporal delivery of angiogenesis promoting factors like bFGF.127
An interesting approach for bioactive substance delivery involves thermo-responsive particles incorporation into electrospun fibers, which after periodic variation in temperature would release the bioactive substances in a controllable manner.128 These smart scaffolds with predefined temperature-induced phase transition may be an interesting delivery technique and a new approach for a localized delivery of proteins.129,130
Currently, external triggers also gain attention and are often applied to electrospun materials design, as they are explored as a potential improvement in these delivery systems.131
An electric current was identified as a potential trigger for swelling and shrinking of polymer based constructs. By increasing the applied voltage, more carboxylic acid groups of polymers becomes ionized which leads to greater repulsion between fibers and results in fiber swelling.124,132 Because of these properties, modified electro-responsive fibers are utilized to control thrombogenicity and inflammatory responses of electrospun vascular grafts. The heparinized PCL fibers loaded with polypyrrole showed a distinct response to the low alternating current which led to significant decrease in platelet activation and leukocyte adhesion.133
Other potential methods for improving vascular graft patency are connected with gene and plasmid delivery. Electrospun scaffolds modified by simple physical adsorption of small interfering RNA (siRNA) could target genes associated with neointimal hyperplasia.134 Gene silencing via thrombospondin-2 (TSP-2) siRNA delivery in electrospun polyethylene terephthalate (PET) graft was found to decrease TSP-2 gene expression, which contributes to anastomosis of implanted biomaterials.135 Electrospraying technique is an emerging method for nano and microparticles preparation.136 It has been verified as an efficient method for drug loading to microparticles. However, it becomes apparent that it is also suitable for plasmid DNA loading to microparticles.137 Electrospinning technique coupled with electrospraying provides new ways of plasmid-containing microparticles incorporation to vascular grafts, which can induce rapid endothelialization of vascular grafts.138 In order to mimic the complex signaling pathway guiding proper neovessel formation development of novel manufacturing techniques of multiple active substance delivery systems should be one of the priorities of future research. Therefore nano and micro sized particles are widely investigated as new controlled release formulations for delivering single or multiple active substances in a sustainable manner.139,140
New active substance selection140 targeting vascular reconstruction issues is also an interesting approach to developing new drug delivering vascular grafts. In one recent study, ferulic acid (Angelica sp.) and astragaloside IV (Astragalus sp.) were loaded to electrospun scaffolds to promote revascularization. The addition of these plant-derived active substances increased cell viability of EC and VSMC in vitro and promoted angiogenesis after subcutaneous implantation with mild inflammatory reaction.141 Additionally, processing of the new candidates for bioactive substance incorporation to electrospun materials could improve the basic knowledge of process parameters which is essential for further developments in this field.
Furthermore, several issues regarding electrospinning process still need to be addressed to fully exploit the potential of these scaffold-based delivery systems. Proper process parameters optimization is needed in order to improve reproducibility and clinical performance of electrospun scaffolds before starting the first clinical study.
To date most of the conducted release studies of substances incorporated to vascular grafts were performed in vitro, therefore to obtain more preclinical data, a greater number of in vivo studies need to be performed. The endpoint of in vivo studies should also consider the long-term use of vascular grafts which should lead to full tissue regeneration.
Additionally, it is of extreme importance to manage to scale up the whole process to the industrial level. Careful selection of used materials and electrospinning parameters need full optimization to obtain method fully transmissible to large scale production. Therefore, drug eluting vascular grafts design should also involve requirements associated with viability maintenance during storage period prior to final use of electrospun grafts.
Studies in mentioned areas are crucial for developing first clinically available and successful electrospun vascular graft.
Moreover, known issues connected with grafting procedures like the excessive growth of neointima, insufficient cell penetration and proliferation leading to vascular graft failure might be easily addressed by proper active substance incorporation to the electrospun grafts. Nowadays, it became even more apparent that this strategy combining scaffold and delivery system is best-suited for tissue engineered purposes.
This paper summarizes new ways of surface functionalization and active substance incorporation to electrospun scaffolds. A rich variety of utilized polymers, emulsion, and co-axial electrospinning, as well as other setup modifications, allow more efficient application of labile compounds like proteins and growth factors. Furthermore, all these elements allow to obtain more controllable graft structure, providing means for a sustained release of bioactive substance which is well-suited for long-term application of vascular grafts. Due to its versatile nature, electrospinning technique is starting to become a new tool for novel drug delivery systems production for future vascular grafts.
AoSMC | Aorta smooth muscle cells |
APTT | Activated partial thromboplastin time |
ASA | Acetylsalicylic acid |
BAEC | Bovine aorta endothelial cells |
BPU | Biodegradable polyurethane urea |
BSA | Bovine serum albumin |
cAMP | Cyclic adenosine monophosphate |
CCK-8 | Cell counting kit-8 assay |
CD31 | Cluster of differentiation 31 |
CDFI | Color Doppler flow imaging |
cGMP | Cyclic guanosine monophosphate |
COX | Cyclooxygenase |
COX | Cyclooxygenase |
DBHD/N2O2 | (Z)-1-{N-butyl-N-[6-(N-butylammoniohexyl)amino]}-diazen-1-ium-1,2-diolate |
DPA | Dipyridamole |
EC | Endothelial cells |
DSA | Digital subtraction angiography |
ECM | Extracellular matrix |
EPC | Endothelial progenitor cells |
EZT | Enzymes prodrug therapy |
FGF | Fibroblast growth factor |
bFGF | Basic fibroblast growth factor |
pbFGF | Plasmid basic fibroblast growth factor |
Gal-NONOate | Galactoside NONOate |
HMG-CoA | 3-Hydroxy-3-methylglutaryl-coenzyme A |
HFIP | Hexafluoroisopropanol |
hSMC | Human smooth muscle cells |
HUVEC | Human umbilical vein endothelial cells |
iHUVEC | Immortalized human umbilical vein endothelial cells |
pHUVEC | Primary human umbilical vein endothelial cells |
KKKKK | Polylysine sequence |
LCSM | Laser confocal scanning microscopy |
LPS | Lipopolysaccharide |
MSC | Mesenchymal stem cells |
NIH-3T3 | Mouse embryonic fibroblast cells |
NO | Nitric oxide |
PBS | Phosphate buffered saline |
PAs | Peptide amphiphiles |
PCL | Polycaprolactone |
pDNA | Plasmid DNA |
PEG | Polyethylene glycol |
PELA | Polyethylene oxide/polylactic acid copolymer |
PELCL | Poly(ethylene glycol)-b-poly(L-lactide-co-caprolactone) |
PET | Polyethylene terephthalate |
PDGF | Platelet-derived growth factor |
PDGF–BB | Platelet-derived growth factor BB homodimer |
PEO | Polyethylene oxide |
PIEC | Porcine hip artery endothelial cells |
PLCL | Poly(lacticacid-co-caprolactone) |
P(LLA-CL) | Poly(L-lactide-co-ε-caprolactone) |
PLA | Poly(lactic acid) |
PLGA | Poly(lactic-co-glycolic acid), poly(glycolic acid) |
PPP | Platelet poor plasma |
ePTFE | Expanded polytetrafluoroethylene |
PTX | Paclitaxel |
SF | Silk fibroin |
SMC | Smooth muscle cells |
siRNA | Small interfering RNA |
TAT | Thrombin–antithrombin complex |
TCPS | Tissue-culture polystyrene |
TEVG | Tissue engineered vascular graft |
TNF-α | Tumor necrosis factor α |
TSP-2 | Thrombospondin-2 |
TT | Thrombin time |
VEGF | Vascular endothelial growth factor |
pVEGF | Plasmid vascular endothelial growth factor |
VEGFR | Vascular endothelial growth factor receptor |
VSMC | Vascular smooth muscle cells |
YIGSR | Laminin-derived Tyr–Ile–Gly–Ser–Arg endothelial cell adhesive ligands |
This journal is © The Royal Society of Chemistry 2017 |