Issue 72, 2024

Polyurethanes synthesized using biomass-derived furan diols as sustainable triboelectric materials

Abstract

This work shows that various polyurethanes (FPUs) prepared using biomass-derived furan diols can be applied as promising tribopositive materials. The elastic FPUs having appropriate glass transition temperature (Tg) could be incorporated into polyethylene terephthalate (PET) fabrics to form FPU/PET films. The optimal FPU-4/PET film showed promising triboelectric performance with output voltages (Vp–p) up to 405 V and a maximum power density (Pmax) of 32 mW cm−2.

Graphical abstract: Polyurethanes synthesized using biomass-derived furan diols as sustainable triboelectric materials

Supplementary files

Article information

Article type
Communication
Submitted
24 6 2024
Accepted
23 7 2024
First published
24 7 2024

Chem. Commun., 2024,60, 9741-9744

Polyurethanes synthesized using biomass-derived furan diols as sustainable triboelectric materials

J. Y. Jang, Y. Byun, S. You, S. Kim, D. Lee, S. Kim and S. U. Son, Chem. Commun., 2024, 60, 9741 DOI: 10.1039/D4CC03073G

To request permission to reproduce material from this article, please go to the Copyright Clearance Center request page.

If you are an author contributing to an RSC publication, you do not need to request permission provided correct acknowledgement is given.

If you are the author of this article, you do not need to request permission to reproduce figures and diagrams provided correct acknowledgement is given. If you want to reproduce the whole article in a third-party publication (excluding your thesis/dissertation for which permission is not required) please go to the Copyright Clearance Center request page.

Read more about how to correctly acknowledge RSC content.

Social activity

Spotlight

Advertisements