Issue 31, 2020

Prospects for defect engineering in Cu2ZnSnS4 solar absorber films

Abstract

Complex compound semiconductors, such as the emerging solar cell material Cu2ZnSn(S,Se)4 (CZTS), present major experimental challenges in terms of understanding and controlling growth processes and defect formation. This study aims to shed light upon the complicated interplay of the synthesis conditions and CZTS thin film properties. Composition-spread thin films are fabricated in different atmospheric conditions during the annealing step. The span of the single-phase region is identified by a phase analysis combining XRD and Raman mapping. The phase characterisation is strengthened by STEM-EDX analysis. Our results show that the stability of the CZTS phase is strongly affected by the process conditions which is observed as a shift in the secondary phase boundaries and different levels of maximum cation ordering achieved in the different samples. With regard to the photoluminescence intensity, all investigated samples show the same trends: regions with Cu3SnS4 secondary phase show the lowest intensity, while the presence of SnSx secondary phases greatly enhances the photoluminescence intensity. The single-phase region features an overall low photoluminescence intensity without a remarkable composition dependence and we propose the presence of deep defects in absence of secondary phases that limit the radiative recombination. We discuss implications for future efforts in defect engineering toward improving the efficiency of CZTS thin film devices.

Graphical abstract: Prospects for defect engineering in Cu2ZnSnS4 solar absorber films

Supplementary files

Article information

Article type
Paper
Submitted
05 मार्च 2020
Accepted
28 अप्रैल 2020
First published
29 अप्रैल 2020
This article is Open Access
Creative Commons BY-NC license

J. Mater. Chem. A, 2020,8, 15864-15874

Prospects for defect engineering in Cu2ZnSnS4 solar absorber films

K. Rudisch, A. Davydova, L. Riekehr, J. Adolfsson, L. Quaglia Casal, C. Platzer-Björkman and J. Scragg, J. Mater. Chem. A, 2020, 8, 15864 DOI: 10.1039/D0TA02598D

This article is licensed under a Creative Commons Attribution-NonCommercial 3.0 Unported Licence. You can use material from this article in other publications, without requesting further permission from the RSC, provided that the correct acknowledgement is given and it is not used for commercial purposes.

To request permission to reproduce material from this article in a commercial publication, please go to the Copyright Clearance Center request page.

If you are an author contributing to an RSC publication, you do not need to request permission provided correct acknowledgement is given.

If you are the author of this article, you do not need to request permission to reproduce figures and diagrams provided correct acknowledgement is given. If you want to reproduce the whole article in a third-party commercial publication (excluding your thesis/dissertation for which permission is not required) please go to the Copyright Clearance Center request page.

Read more about how to correctly acknowledge RSC content.

Social activity

Spotlight

Advertisements