Issue 23, 2023

Advances in research on the inhibitory effect of 3D current collector structures for lithium dendrites

Abstract

Lithium is considered the “Holy Grail” of anode materials in lithium metal batteries owing to its extremely low electrochemical potential and high specific capacity. However, during the charging/discharging process, the uneven deposition of lithium can lead to the formation of lithium dendrites. The rapid growth of lithium dendrites can puncture the membrane and cause a short circuit, resulting in a safety hazard. In addition, some lithium dendrites break or fall off to form “dead lithium” during the long cycle, which reduces the coulombic efficiency (CE) of the battery. Lithium dendrites greatly affect the application of lithium metal batteries (LMBs). Three-dimensional (3D) current collectors with a high specific surface area and high porosity can regulate lithium-ion flux distribution, reduce the local current density, and guide the uniform deposition of lithium, which can effectively inhibit the growth of lithium dendrites. This review is devoted to summarizing the research progress on 3D current collector structures in recent years, focusing on the suppression of lithium dendrite growth by various 3D current collector structures, including ordered arrangement structures, irregular structures, gradient structures, graded porous structures, foam structures, and alloy frameworks. Considering the current research tendency, the challenges and prospects of various 3D current collector structures are discussed to provide a reference for the further development of advanced lithium metal anodes.

Graphical abstract: Advances in research on the inhibitory effect of 3D current collector structures for lithium dendrites

Article information

Article type
Review Article
Submitted
09 jul. 2023
Accepted
10 oct. 2023
First published
12 oct. 2023

Inorg. Chem. Front., 2023,10, 6767-6791

Advances in research on the inhibitory effect of 3D current collector structures for lithium dendrites

S. Xiang, Y. Fu, C. Yin, Y. Hou, H. Tian and Z. Yin, Inorg. Chem. Front., 2023, 10, 6767 DOI: 10.1039/D3QI01290E

To request permission to reproduce material from this article, please go to the Copyright Clearance Center request page.

If you are an author contributing to an RSC publication, you do not need to request permission provided correct acknowledgement is given.

If you are the author of this article, you do not need to request permission to reproduce figures and diagrams provided correct acknowledgement is given. If you want to reproduce the whole article in a third-party publication (excluding your thesis/dissertation for which permission is not required) please go to the Copyright Clearance Center request page.

Read more about how to correctly acknowledge RSC content.

Social activity

Spotlight

Advertisements