Tuning operation temperature of charging-free thermally regenerative electrochemical cycles driven by semiclathrate hydrate formation

Abstract

Electrolytes with a strong temperature dependence of the redox potential, denoted as the temperature coefficient, are required to increase the voltage of thermo-electrochemical devices. In our previous study, we revealed that the temperature coefficient of ferrocyanide/ferricyanide redox couple ([Fe(CN)6]4−/3−) dramatically increases in a mixture of water and tetrabutylammonium fluoride (TBAF) owing to the formation of semiclathrate hydrate (SCH). However, the temperature range in which a high temperature coefficient is obtained is limited to the vicinity of the SCH formation temperature. In this study, we demonstrate that this temperature range can be adjusted using organic salts that provide different SCH formation temperatures, such as tetrabutylammonium chloride and tetrabutylphosphonium chloride (TBPC). Replacing the organic salt affects both the temperature range and magnitude of the temperature coefficient. The calculation using the developed model to evaluate the contribution of SCH formation revealed the origin of the difference in temperature coefficient, such as the dependence of redox potential of [Fe(CN)6]4−/3− on organic salt concentration in the liquid phase, and the temperature dependence of organic salt concentration in the liquid phase. Furthermore, we assembled a thermo-electrochemical device for a charging-free thermally regenerative electrochemical cycle using electrolytes with different organic salts. The devices using different organic salts were operated in distinct temperature ranges: 292–297 K for the TBAF-based system and 276–280 K for the TBPC-based system. This study expands the applicability of high-voltage thermo-electrochemical devices driven by the SCH formation.

Graphical abstract: Tuning operation temperature of charging-free thermally regenerative electrochemical cycles driven by semiclathrate hydrate formation

Supplementary files

Article information

Article type
Paper
Submitted
22 Dec 2025
Accepted
26 Feb 2026
First published
04 Mar 2026

Sustainable Energy Fuels, 2026, Advance Article

Tuning operation temperature of charging-free thermally regenerative electrochemical cycles driven by semiclathrate hydrate formation

Y. Matsui and Y. Maeda, Sustainable Energy Fuels, 2026, Advance Article , DOI: 10.1039/D5SE01681A

To request permission to reproduce material from this article, please go to the Copyright Clearance Center request page.

If you are an author contributing to an RSC publication, you do not need to request permission provided correct acknowledgement is given.

If you are the author of this article, you do not need to request permission to reproduce figures and diagrams provided correct acknowledgement is given. If you want to reproduce the whole article in a third-party publication (excluding your thesis/dissertation for which permission is not required) please go to the Copyright Clearance Center request page.

Read more about how to correctly acknowledge RSC content.

Social activity

Spotlight

Advertisements