Synthesis of indium oxide microparticles using aerosol assisted chemical vapour deposition†
Abstract
Microparticles of indium oxide (In2O3) are deposited on glass substrates at 500 °C using aerosol assisted chemical vapour deposition (AACVD). The structural, morphological and optical properties of the as-deposited particles are reported.