High-yield production of 2D crystals by wet-jet milling

Author affiliations

Abstract

Efficient and scalable production of two-dimensional (2D) materials is required to overcome technological hurdles towards the creation of a 2D-material-based industry. Here, we present a novel approach developed for the exfoliation of layered crystals, i.e., graphite, hexagonal-boron nitride and transition metal dichalcogenides. The process is based on high-pressure wet-jet-milling (WJM), resulting in a 2 L h−1 production of 10 g L−1 of single- and few-layer 2D crystal flakes in dispersion making the scaling-up more affordable. The WJM process enables the production of defect-free and high quality 2D-crystal dispersions on a large scale, opening the way for their full exploitation in different commercial applications, e.g., as anode active material in lithium ion batteries, as reinforcement in polymer–graphene composites, and as conductive inks, as we demonstrate in this report.

Graphical abstract: High-yield production of 2D crystals by wet-jet milling

Back to tab navigation

Supplementary files

Article information


Submitted
25 Apr 2018
Accepted
06 Jul 2018
First published
06 Jul 2018

Mater. Horiz., 2018,5, 890-904
Article type
Communication

High-yield production of 2D crystals by wet-jet milling

A. E. Del Rio Castillo, V. Pellegrini, A. Ansaldo, F. Ricciardella, H. Sun, L. Marasco, J. Buha, Z. Dang, L. Gagliani, E. Lago, N. Curreli, S. Gentiluomo, F. Palazon, M. Prato, R. Oropesa-Nuñez, P. S. Toth, E. Mantero, M. Crugliano, A. Gamucci, A. Tomadin, M. Polini and F. Bonaccorso, Mater. Horiz., 2018, 5, 890
DOI: 10.1039/C8MH00487K

Social activity

Search articles by author

Spotlight

Advertisements