Abstract

Traditionally, palm oil mill effluent (POME) is treated via open ponding system, which however is land-intensive and requires long hydraulic retention time. For the first time, this paper reports, simultaneously, the kinetics of photocatalytic degradation of POME and the assessment of its gaseous product formations. Characterization of the as-received UV-responsive TiO2 showed that anatase was the predominant crystalline phase with an estimated crystallite size of 45.7 nm and band gap energy of 3.15 eV based on the UV-vis DRS scanning. Moreover, N2-physisorption revealed that the BET specific surface area for TiO2 was 8.73 m2 g−1 with pore size of 22.4 nm. When the photoreactor was blanketed with N2 gas only at a TiO2 loading of 0.5 g L−1, POME degradation was only 4%. Significantly, in the presence of O2, the degradation of POME achieved 23%, and can even attain a maximum of 52.0% at TiO2 loading of 1.0 g L−1 after 240 min of UV-irradiation. This has demonstrated that the hydroxyl generation rate from water species (prevalent in N2-blanket) was considerably slower compared to the hydroxyl generation from the superoxide pathway that originates from externally-supplied O2. It was also found that the POME degradation kinetics adhered to the 1st-order reaction with specific reaction rates (k) ranging from 0.70 × 10−3 to 2.90 × 10−3 min−1. Interestingly, our assessment of the gaseous product formations revealed that the photoreaction employing 1.0 g L−1 TiO2 produced the highest amount of CO2 (38 913 μmol) while 0.5 g L−1 TiO2 produced the highest amount of CH4 (361 μmol). From the FTIR scanning of used catalyst, we can confirm that the chemisorption of organics was practically absent. This has led us to believe that the primary role of TiO2 was to generate hydroxyls for direct attack on the organic compounds in the POME and eventually decompose them into simpler intermediates, CH4, CO2, and water. Moreover, after 20 h under the UV irradiation, POME degradation attained 78.0% and the final COD level dropped to 37 ppm, which is safe to be discharged.

Graphical abstract: A novel photomineralization of POME over UV-responsive TiO2 photocatalyst: kinetics of POME degradation and gaseous product formations

Article information

Article type
Paper
Submitted
17 Apr 2015
Accepted
11 Jun 2015
First published
11 Jun 2015

RSC Adv., 2015,5, 53100-53110

Author version available

A novel photomineralization of POME over UV-responsive TiO2 photocatalyst: kinetics of POME degradation and gaseous product formations

K. H. Ng and C. K. Cheng, RSC Adv., 2015, 5, 53100 DOI: 10.1039/C5RA06922J

To request permission to reproduce material from this article, please go to the Copyright Clearance Center request page.

If you are an author contributing to an RSC publication, you do not need to request permission provided correct acknowledgement is given.

If you are the author of this article, you do not need to request permission to reproduce figures and diagrams provided correct acknowledgement is given. If you want to reproduce the whole article in a third-party publication (excluding your thesis/dissertation for which permission is not required) please go to the Copyright Clearance Center request page.

Read more about how to correctly acknowledge RSC content.

Social activity

Spotlight

Advertisements