The effects of the addition of small amount of Zr (less than 2 at%) to the fcc phase of the Pd–Cu hydrogen separation alloy were investigated. Hydrogen flux variations in Pd–Cu and Pd–Cu–Zr alloys in the presence of 1000 ppm H2S + H2 feed gas showed a marked effect of Zr addition in improving the resistance to sulphur poisoning.

Graphical abstract: A novel Pd–Cu–Zr hydrogen separation membrane with a high tolerance to sulphur poisoning

Supplementary files

Article information

Article type
Communication
Submitted
28 May 2015
Accepted
08 Sep 2015
First published
08 Sep 2015

Chem. Commun., 2015,51, 15842-15845

A novel Pd–Cu–Zr hydrogen separation membrane with a high tolerance to sulphur poisoning

S. Nayebossadri, J. D. Speight and D. . Book, Chem. Commun., 2015, 51, 15842 DOI: 10.1039/C5CC04327A

To request permission to reproduce material from this article, please go to the Copyright Clearance Center request page.

If you are an author contributing to an RSC publication, you do not need to request permission provided correct acknowledgement is given.

If you are the author of this article, you do not need to request permission to reproduce figures and diagrams provided correct acknowledgement is given. If you want to reproduce the whole article in a third-party publication (excluding your thesis/dissertation for which permission is not required) please go to the Copyright Clearance Center request page.

Read more about how to correctly acknowledge RSC content.

Social activity

Spotlight

Advertisements