Abstract

An air-stable LiBH4 polymeric composite was successfully prepared by modifying LiBH4 with a gas-barrier polymer matrix, poly(methylmethacrylate) (PMMA). The as-prepared LiBH4@PMMA composite started to dehydrogenate at 53 °C with the first main dehydrogenation peak at 116 °C, and 5.2 wt% of hydrogen released at 162 °C within 1 h.

Graphical abstract: Increased air stability and decreased dehydrogenation temperature of LiBH4via modification within poly(methylmethacrylate)

Supplementary files

Article information

Article type
Communication
Submitted
22 Jul 2013
Accepted
10 Oct 2013
First published
11 Oct 2013

Dalton Trans., 2014,43, 410-413

Increased air stability and decreased dehydrogenation temperature of LiBH4via modification within poly(methylmethacrylate)

J. Huang, Y. Yan, L. Ouyang, H. Wang, J. Liu and M. Zhu, Dalton Trans., 2014, 43, 410 DOI: 10.1039/C3DT51989A

To request permission to reproduce material from this article, please go to the Copyright Clearance Center request page.

If you are an author contributing to an RSC publication, you do not need to request permission provided correct acknowledgement is given.

If you are the author of this article, you do not need to request permission to reproduce figures and diagrams provided correct acknowledgement is given. If you want to reproduce the whole article in a third-party publication (excluding your thesis/dissertation for which permission is not required) please go to the Copyright Clearance Center request page.

Read more about how to correctly acknowledge RSC content.

Social activity

Spotlight

Advertisements