Critical silicon-anode size for averting lithiation-induced mechanical failure of lithium-ion batteries
Abstract
Silicon
* Corresponding authors
a
Key Laboratory of Low Dimensional Materials & Application Technology of Ministry of Education, Faculty of Materials, Optoelectronics and Physics, Xiangtan University, Hunan 411105, China
E-mail:
zsma@xtu.edu.cn, zhouyc@xtu.edu.cn
Fax: +86 731 58293586
Tel: +86 731 58293586
b State Key Laboratory of Rare Earth Resource Utilization, Changchun Institute of Applied Chemistry, Chinese Academy of Sciences, Changchun 130022, China
Silicon
Z. Ma, T. Li, Y. L. Huang, J. Liu, Y. Zhou and D. Xue, RSC Adv., 2013, 3, 7398 DOI: 10.1039/C3RA41052H
To request permission to reproduce material from this article, please go to the Copyright Clearance Center request page.
If you are an author contributing to an RSC publication, you do not need to request permission provided correct acknowledgement is given.
If you are the author of this article, you do not need to request permission to reproduce figures and diagrams provided correct acknowledgement is given. If you want to reproduce the whole article in a third-party publication (excluding your thesis/dissertation for which permission is not required) please go to the Copyright Clearance Center request page.
Read more about how to correctly acknowledge RSC content.
Fetching data from CrossRef.
This may take some time to load.
Loading related content