Issue 16, 2000

On the rehydration of vanadyl pyrophosphate to vanadyl hydrogenphosphate hemihydrate

Abstract

Vanadyl pyrophosphate-based VPO catalysts for butane oxidation to maleic anhydride can be completely rehydrated in the solid phase into their vanadyl hydrogenphosphate hemihydrate precursors which again can be transformed into vanadyl pyrophosphate thus enabling a reuse of spent catalysts.

Article information

Article type
Communication
Submitted
09 May 2000
Accepted
06 Jul 2000
First published
21 Jul 2000

Chem. Commun., 2000, 1517-1518

On the rehydration of vanadyl pyrophosphate to vanadyl hydrogenphosphate hemihydrate

G. Wolf, B. Kubias, B. Jacobi and B. Lücke, Chem. Commun., 2000, 1517 DOI: 10.1039/B003700L

To request permission to reproduce material from this article, please go to the Copyright Clearance Center request page.

If you are an author contributing to an RSC publication, you do not need to request permission provided correct acknowledgement is given.

If you are the author of this article, you do not need to request permission to reproduce figures and diagrams provided correct acknowledgement is given. If you want to reproduce the whole article in a third-party publication (excluding your thesis/dissertation for which permission is not required) please go to the Copyright Clearance Center request page.

Read more about how to correctly acknowledge RSC content.