Preparation of La0.3Sr0.7CoO3–δ perovskite by thermal decomposition of metal-EDTA complexes

Abstract

Perovskite powders of La0.3Sr0.7CoO3–δwere prepared by the thermal decomposition of precursor complexes derived from nitrate solutions using ethylenediaminetetraacetic acid (EDTA) as a complexing agent. The calcination temperature is 920 °C. Powders thus obtained have a low carbon contamination. Dense ceramics with a relative density of about 96% have been prepared after sintering at 1150 °C.

Article information

Article type
Paper

J. Mater. Chem., 1998,8, 2109-2112

Preparation of La0.3Sr0.7CoO3–δ perovskite by thermal decomposition of metal-EDTA complexes

R. H. E. van Doorn, H. Kruidhof, A. Nijmeijer, L. Winnubst and A. J. Burggraaf, J. Mater. Chem., 1998, 8, 2109 DOI: 10.1039/A800500A

To request permission to reproduce material from this article, please go to the Copyright Clearance Center request page.

If you are an author contributing to an RSC publication, you do not need to request permission provided correct acknowledgement is given.

If you are the author of this article, you do not need to request permission to reproduce figures and diagrams provided correct acknowledgement is given. If you want to reproduce the whole article in a third-party publication (excluding your thesis/dissertation for which permission is not required) please go to the Copyright Clearance Center request page.

Read more about how to correctly acknowledge RSC content.

Spotlight

Advertisements