Mixtures of SiC powder with diamond seeds were subjected to hydrothermal treatment at 700–750 °C under pressures of 100–500 MPa. The results of this study demonstrate that well crystallised diamond is formed after hydrothermal treatment of SiC when diamond seeds are present.

Article information

Article type
Paper

J. Mater. Chem., 1995,5, 2313-2314

Hydrothermal synthesis of diamond from diamond-seeded β-SiC powder

Y. G. Gogotsi, K. G. Nickel and P. Kofstad, J. Mater. Chem., 1995, 5, 2313 DOI: 10.1039/JM9950502313

To request permission to reproduce material from this article, please go to the Copyright Clearance Center request page.

If you are an author contributing to an RSC publication, you do not need to request permission provided correct acknowledgement is given.

If you are the author of this article, you do not need to request permission to reproduce figures and diagrams provided correct acknowledgement is given. If you want to reproduce the whole article in a third-party publication (excluding your thesis/dissertation for which permission is not required) please go to the Copyright Clearance Center request page.

Read more about how to correctly acknowledge RSC content.

Spotlight

Advertisements