Correction for ‘Three-dimensional TiNb2O7 anchored on carbon nanofiber core–shell arrays as an anode for high-rate lithium ion storage’ by Meili Qi et al., RSC Adv., 2020, 10, 6342–6350, https://doi.org/10.1039/C9RA10485B.
The in situ Raman spectra at 1.25 V during the discharge process for the TNO/CNF core/shell array electrode, as shown in Fig. 5a of the published article, contained an error. Specifically, a duplicated spectrum (the green line in Fig. 5a) was inadvertently included.
The incorrect spectrum (the green line in Fig. 5a) has been replaced with the correct one, and the corrected in situ Raman spectra for the TNO/CNF core/shell array electrode during the discharge process are provided here.
Fig. 5a In situ Raman spectra evolution of the TNO/CNF core/shell array electrode at different (a) discharge curves of the TNO/CNF electrode.
An independent expert has viewed the corrected figure and has concluded that it is consistent with the discussions and conclusions presented.
The Royal Society of Chemistry apologises for these errors and any consequent inconvenience to authors and readers.