Saúl Cabrera, Jamal El Haskouri, Carmen Guillem, Aurelio Beltrán-Porter, Daniel Beltrán-Porter, M. Dolores Marcos, Pedro Amorós and Sagrario Mendioroz
Thermally stable porous aluminophosphates (ICMUV-3) with P/Al molar ratios in the range 0.15 ⩽ P/Al ⩽ 0.75 and showing continuously adjustable pore sizes from 13 to 37 Å have been prepared through a surfactant-assisted procedure without changing the surfactant length and/or addition of organic expansors.