Abstract

On hydration template-free SAPO-34 shows the opening of some Si–O–Al bonds as suggested by 29Si MAS NMR and XRD results, the effect being reversible upon dehydration; the hydrated distorted structure is stable for months with no further modifications and the ordered material can be regenerated by removal of water at 423 K.

Article information

Article type
Paper

J. Chem. Soc., Chem. Commun., 1993, 544-546

Reversible modification of the Si environment in template-free SAPO-34 structure upon hydration-dehydration cycles below ca. 400 K

R. Vomscheid, M. Briend, M. J. Peltre, P. Massiani, P. P. Man and D. Barthomeuf, J. Chem. Soc., Chem. Commun., 1993, 544 DOI: 10.1039/C39930000544

To request permission to reproduce material from this article, please go to the Copyright Clearance Center request page.

If you are an author contributing to an RSC publication, you do not need to request permission provided correct acknowledgement is given.

If you are the author of this article, you do not need to request permission to reproduce figures and diagrams provided correct acknowledgement is given. If you want to reproduce the whole article in a third-party publication (excluding your thesis/dissertation for which permission is not required) please go to the Copyright Clearance Center request page.

Read more about how to correctly acknowledge RSC content.

Spotlight

Advertisements