Decomposition of formic acid on titanium, vanadium, chromium, manganese, iron, cobalt, nickel, and copper

Abstract

The catalytic decomposition of formic acid has been investigated on evaporated films of the first transition-series elements from titanium to copper. Zero-order rates were observed for the first 15–20% of the decomposition with acid pressures of 30 mm Hg at temperatures, depending on the metal, in the range 100–300°. The product ratio CO2/H2 was always unity, but the CO2/CO ratio varied in a twin-peaked manner across the series, with maxima at chromium and nickel. The latter product ratio was constant for a given metal irrespective of reaction temperature and percentage decomposition. Titanium was unique in that only dehydration of the acid was observed. The results are consistent with the occurrence, except with titanium, of a bimolecular transition state intermediate which breaks down to give both CO2 and CO in proportions determined by the nature of the metal catalyst.

Article information

Article type
Paper

J. Chem. Soc. A, 1969, 2985-2987

Decomposition of formic acid on titanium, vanadium, chromium, manganese, iron, cobalt, nickel, and copper

H. S. Inglis and D. Taylor, J. Chem. Soc. A, 1969, 2985 DOI: 10.1039/J19690002985

To request permission to reproduce material from this article, please go to the Copyright Clearance Center request page.

If you are an author contributing to an RSC publication, you do not need to request permission provided correct acknowledgement is given.

If you are the author of this article, you do not need to request permission to reproduce figures and diagrams provided correct acknowledgement is given. If you want to reproduce the whole article in a third-party publication (excluding your thesis/dissertation for which permission is not required) please go to the Copyright Clearance Center request page.

Read more about how to correctly acknowledge RSC content.

Spotlight

Advertisements