Highly recoverable rosin-based shape memory polyurethanes

Author affiliations

Abstract

Improving the phase separation and stability of the hard segment domains at the same time is the novel method reported here to improve the recovery of thermoplastic shape memory polyurethanes (SMPUs) at high strain (>1000%). The shape recovery of the corresponding SMPUs with a more than 1000% strain can reach about 96% at room temperature in 3 min, the recoverable strain (εmaxεpermanent) is more than 960%, which is nearly 2.5 times that of the best value (400%) previously reported.

Graphical abstract: Highly recoverable rosin-based shape memory polyurethanes

Back to tab navigation

Supplementary files

Publication details

The article was received on 27 Dec 2012, accepted on 23 Jan 2013 and first published on 24 Jan 2013


Article type: Communication
DOI: 10.1039/C3TA01655B
J. Mater. Chem. A, 2013,1, 3263-3267

  •   Request permissions

    Highly recoverable rosin-based shape memory polyurethanes

    L. Zhang, Y. Jiang, Z. Xiong, X. Liu, H. Na, R. Zhang and J. Zhu, J. Mater. Chem. A, 2013, 1, 3263
    DOI: 10.1039/C3TA01655B

Search articles by author

Spotlight

Advertisements