Abstract

Polyesters based on polyols and sebacic acid, known as poly(polyol sebacate)s (PPS) are good candidates to develop degradable materials, due to their combination of flexibility and degradability, which are both useful properties in the context of soft-tissue engineering (Z. Sun, C. Chen, M. Sun, C. Ai, X. Lu, Y. Zheng, B. Yang and D. Dong, Biomaterials, 2009, 30, 5209, C. Sundback, J. Shyu, Y. Wang, W. Faquin, R. Langer, J. Vacanti and T. Hadlock, Biomaterials, 2005, 26, 5454, D. Motlagh, J. Yang, K. Lui, A. Webb and G. Ameer, Biomaterials, 2006, 27, 4315, A. Mahdavi, L. Ferreira, C. Sundback, J. W. Nichol, E. P. Chan, D. J. D. Carter, C. J. Bettinger, S. Patanavanich, L. Chignozha, E. Ben-Joseph, A. Galakatos, H. Pryor, I. Pomerantseva, P. T. Masiakos, W. Faquin, A. Zumbuehl, S. Hong, J. Borenstein, J. Vacanti, R. Langer and J. M. Karp, Proc. Natl. Acad. Sci. U. S. A., 2008, 105, 2307). However, PPS generally display poor mechanical properties, in particular a low modulus, that limit the true potential of these materials in the biomedical field. Here, we introduce an approach to obtain nanocomposites based on poly(mannitol sebacate) (PMS) matrices reinforced with cellulose nanocrystals (CNCs) in order to improve the application range of these materials. Different strategies were used based on varying the feed ratios between mannitol : sebacic acid (1 : 1 and 1 : 2), crosslinking conditions and CNCs content, resulting in different degrees of crosslinking and, therefore, mechanical and degradation behavior. All of the developed nanocomposites displayed the expected mass loss during the degradation studies in simulated body fluid (SBF) similar to the neat matrix, however, doubling the sebacic acid feed ratio or extending the curing temperature and time, resulted in higher mechanical properties, structural integrity, and shape stability during a degradation time lessening mass loss rate. Changing mannitol : sebacic acid reaction ratios from 1 : 1 to 1 : 2 and for low crosslinking degree neat samples, the Young's modulus increases four-fold, while mass loss after 150 days of incubation is reduced by half. The Young's modulus range obtained with this process covers the range of human elastic soft tissues to tough tissues (0.7–200 MPa).

Graphical abstract: Mechanical properties and degradation studies of poly(mannitol sebacate)/cellulose nanocrystals nanocomposites

Supplementary files

Article information

Article type
Paper
Submitted
15 Apr 2015
Accepted
18 Jun 2015
First published
19 Jun 2015

RSC Adv., 2015,5, 55879-55891

Author version available

Mechanical properties and degradation studies of poly(mannitol sebacate)/cellulose nanocrystals nanocomposites

Á. Sonseca, O. Sahuquillo, E. J. Foster and E. Giménez, RSC Adv., 2015, 5, 55879 DOI: 10.1039/C5RA06768E

To request permission to reproduce material from this article, please go to the Copyright Clearance Center request page.

If you are an author contributing to an RSC publication, you do not need to request permission provided correct acknowledgement is given.

If you are the author of this article, you do not need to request permission to reproduce figures and diagrams provided correct acknowledgement is given. If you want to reproduce the whole article in a third-party publication (excluding your thesis/dissertation for which permission is not required) please go to the Copyright Clearance Center request page.

Read more about how to correctly acknowledge RSC content.

Social activity

Spotlight

Advertisements