Abstract

The uptake of 1,4,10,13-tetraoxa-7,16-diazacyclooctadecane (tdco) by α- and γ-zirconium phosphates was studied at 25 °C. The α phosphate incompletely reacts with tdco to form an intercalated phase in which the guest molecules are arranged as 0.68 nm thick monolayer, probably in their twisted conformation. The γ phosphate is totally converted into a single phase containing a 0.91 nm thick bilayer of tdco molecules with their molecular planes parallel to the inorganic layers.

Article information

Article type
Paper

J. Chem. Soc., Dalton Trans., 1996, 1245-1248

Intercalation of 1,4,10,13-tetraoxa-7,16-diazacyclooctadecane by α- and γ-zirconium phosphates

T. Kijima, K. Sakoh and M. Machida, J. Chem. Soc., Dalton Trans., 1996, 1245 DOI: 10.1039/DT9960001245

To request permission to reproduce material from this article, please go to the Copyright Clearance Center request page.

If you are an author contributing to an RSC publication, you do not need to request permission provided correct acknowledgement is given.

If you are the author of this article, you do not need to request permission to reproduce figures and diagrams provided correct acknowledgement is given. If you want to reproduce the whole article in a third-party publication (excluding your thesis/dissertation for which permission is not required) please go to the Copyright Clearance Center request page.

Read more about how to correctly acknowledge RSC content.

Spotlight

Advertisements