Jump to main content
Jump to site search

Issue 60, 2013
Previous Article Next Article

A magnesiothermic reaction process for the scalable production of mesoporous silicon for rechargeable lithium batteries

Author affiliations

Abstract

Mesoporous, 3-D, nanocrystalline Si has been synthesized via the magnesiothermic reduction of SiO particles at a peak temperature of only 500 °C in a scalable flow-through reactor setup. Such 3-D porous Si as an anode material exhibited high, reversible capacities (i.e., >900 mA h g−1 after 160 charge–discharge cycles at 1000 mA g−1).

Graphical abstract: A magnesiothermic reaction process for the scalable production of mesoporous silicon for rechargeable lithium batteries

Back to tab navigation

Supplementary files

Article information


Submitted
27 Apr 2013
Accepted
06 Jun 2013
First published
20 Jun 2013

Chem. Commun., 2013,49, 6743-6745
Article type
Communication

A magnesiothermic reaction process for the scalable production of mesoporous silicon for rechargeable lithium batteries

A. Xing, J. Zhang, Z. Bao, Y. Mei, A. S. Gordin and K. H. Sandhage, Chem. Commun., 2013, 49, 6743
DOI: 10.1039/C3CC43134G