A Ni/apatite-type lanthanum silicate supported catalyst in glycerol steam reforming reaction

Author affiliations

Abstract

In the glycerol steam reforming reaction a 5 wt% Ni/La9.83Si4.5Fe1.5O26±δ catalyst was found to be active and up to 3.2 times more selective to H2 than a 5 wt% Ni/Al2O3 catalyst, especially at low temperatures (<500 °C). A H2/CO molar ratio of 5 was achieved under a space velocity of 50 000 h−1.

Graphical abstract: A Ni/apatite-type lanthanum silicate supported catalyst in glycerol steam reforming reaction

Back to tab navigation

Supplementary files

Publication details

The article was received on 22 Apr 2016, accepted on 04 Aug 2016 and first published on 04 Aug 2016


Article type: Communication
DOI: 10.1039/C6RA10437A
Author version
available:
Download author version (PDF)
Citation: RSC Adv., 2016,6, 78954-78958

  •   Request permissions

    A Ni/apatite-type lanthanum silicate supported catalyst in glycerol steam reforming reaction

    M. A. Goula, N. D. Charisiou, P. K. Pandis and V. N. Stathopoulos, RSC Adv., 2016, 6, 78954
    DOI: 10.1039/C6RA10437A

Search articles by author

Spotlight

Advertisements