Proton conductivity in the dry membrane of poly(sulfonic acid) and polyamine layer-by-layer complex

Abstract

A layer-by-layer assembled and molecular-complexed polymer membrane was prepared by the simple combination of poly(4-styrenesulfonic acid) and poly(allylamine) on a comb-shaped gold electrode: it displayed a very high proton conductivity of 10−3 S cm−1 under a dry condition at 120 °C.

Graphical abstract: Proton conductivity in the dry membrane of poly(sulfonic acid) and polyamine layer-by-layer complex

Supplementary files

Article information

Article type
Communication
Submitted
15 Mar 2007
Accepted
26 Apr 2007
First published
17 May 2007

Chem. Commun., 2007, 2989-2991

Proton conductivity in the dry membrane of poly(sulfonic acid) and polyamine layer-by-layer complex

T. Tago, H. Shibata and H. Nishide, Chem. Commun., 2007, 2989 DOI: 10.1039/B703947F

To request permission to reproduce material from this article, please go to the Copyright Clearance Center request page.

If you are an author contributing to an RSC publication, you do not need to request permission provided correct acknowledgement is given.

If you are the author of this article, you do not need to request permission to reproduce figures and diagrams provided correct acknowledgement is given. If you want to reproduce the whole article in a third-party publication (excluding your thesis/dissertation for which permission is not required) please go to the Copyright Clearance Center request page.

Read more about how to correctly acknowledge RSC content.

Social activity

Spotlight

Advertisements