Reaction sequences occurring in dense Li-doped sialon ceramics: influence of temperature and holding time
Abstract
Spark Plasma Sintering (
* Corresponding authors
a
Department of Inorganic Chemistry, Arrhenius Laboratory, Stockholm University, Stockholm, Sweden.
E-mail:
shen@inorg.su.se
Fax: 46-8-152187
Tel: 46-8-162388
Spark Plasma Sintering (
H. Peng, Z. Shen and M. Nygren, J. Mater. Chem., 2003, 13, 2285 DOI: 10.1039/B304899C
To request permission to reproduce material from this article, please go to the Copyright Clearance Center request page.
If you are an author contributing to an RSC publication, you do not need to request permission provided correct acknowledgement is given.
If you are the author of this article, you do not need to request permission to reproduce figures and diagrams provided correct acknowledgement is given. If you want to reproduce the whole article in a third-party publication (excluding your thesis/dissertation for which permission is not required) please go to the Copyright Clearance Center request page.
Read more about how to correctly acknowledge RSC content.
Fetching data from CrossRef.
This may take some time to load.
Loading related content