Preparation of LiCoO2 and LiCo1–xFexO2 using hydrothermal reactions

Abstract

Iron doped/undoped LiCoO 2 powders could be obtained from hydrothermal reactions of either Fe 3+ or Co 3+ containing co-precipitates or a CoCl 2 -NaOH-NaClO 3 (oxidant) mixture with an excess amount of LiOH·H 2 O at 220 °C for 8-48 h. The LiFe x Co 1–x O 2 solid solution maintained a layered rock-salt structure until x=0.25. 57 Fe Mössbauer and Co K-edge XANES spectra and magnetic susceptibility data reveal that iron and cobalt in the solid solution are in high-spin Fe 3+ (S=5/2) and low-spin Co 3+ (S=0) configurations.

Article information

Article type
Paper

J. Mater. Chem., 1999,9, 199-204

Preparation of LiCoO2 and LiCo1–xFexO2 using hydrothermal reactions

M. Tabuchi, K. Ado, H. Kobayashi, H. Sakaebe, H. Kageyama, C. Masquelier, M. Yonemura, A. Hirano and R. Kanno, J. Mater. Chem., 1999, 9, 199 DOI: 10.1039/A805311A

To request permission to reproduce material from this article, please go to the Copyright Clearance Center request page.

If you are an author contributing to an RSC publication, you do not need to request permission provided correct acknowledgement is given.

If you are the author of this article, you do not need to request permission to reproduce figures and diagrams provided correct acknowledgement is given. If you want to reproduce the whole article in a third-party publication (excluding your thesis/dissertation for which permission is not required) please go to the Copyright Clearance Center request page.

Read more about how to correctly acknowledge RSC content.

Spotlight

Advertisements