Issue 7, 1988

Cr3+ electron spin resonance linewidth in ZnO—ZnCr2O4—(Pd) solid mixtures

Abstract

The e.s.r. signal generated by a solid catalyst, based on a ZnO, ZnCr2O4 and Pd mixture, has been studied as a function of the concentration of the components. The linewidth broadening and narrowing of the signal is strongly dependent on both the Zn/Cr ratio and the Pd concentration and is connected with a change in the relative distance between the Cr3+ ions.

Article information

Article type
Paper

J. Chem. Soc., Faraday Trans. 1, 1988,84, 2477-2482

Cr3+ electron spin resonance linewidth in ZnO—ZnCr2O4—(Pd) solid mixtures

L. Forni and C. Oliva, J. Chem. Soc., Faraday Trans. 1, 1988, 84, 2477 DOI: 10.1039/F19888402477

To request permission to reproduce material from this article, please go to the Copyright Clearance Center request page.

If you are an author contributing to an RSC publication, you do not need to request permission provided correct acknowledgement is given.

If you are the author of this article, you do not need to request permission to reproduce figures and diagrams provided correct acknowledgement is given. If you want to reproduce the whole article in a third-party publication (excluding your thesis/dissertation for which permission is not required) please go to the Copyright Clearance Center request page.

Read more about how to correctly acknowledge RSC content.