Xiuze
Hei
ab and
Jing
Li
*ba
aHoffmann Institute of Advanced Materials, Shenzhen Polytechnic, 7098 Liuxian Blvd, Nanshan District, Shenzhen, 518055, People's Republic of China. E-mail: jingli@rutgers.edu
bDepartment of Chemistry and Chemical Biology, Rutgers University, 123 Bevier Road, Piscataway, New Jersey 08854, USA
First published on 8th August 2023
The development of high-performance, solution-processable semiconducting materials is crucial for the advancement of emerging clean-energy technologies such as light-emitting diodes and photovoltaics. While hybrid perovskites have shown considerable promise for implementation in these technologies, their reliance on toxic metals and relatively low stability towards moisture and chemical environments remain to be addressed. In this Chemistry Frontiers article, we describe a unique strategy to build nontoxic, robust and solution-processable hybrid semiconductors based on copper halide by incorporating ionic bonds in coordination complexes (molecular or extended network structures). Specifically, these compounds are made of anionic copper(I) halide and cationic organic ligands that form both coordinate and ionic bonds at the inorganic/organic interfaces and are referred to as all-in-one (AIO)-type structures. The unique bonding nature renders the AIO-type structures with greatly enhanced solubility, excellent optical tunability and remarkable framework stability, all highly desirable for thin-film based optoelectronic devices. We will highlight the most recent progress in the development of this material group, including their design strategies, important properties and potential for clean-energy related applications. We will also briefly discuss the existing challenges and future outlook of these materials.
Despite their superior optoelectronic properties, the utility of many conventional inorganic semiconductors in high-end thin-film based devices is often hampered due to their very poor solution processability. Designing new semiconducting materials that are solution-processable is critical for the device industries.6 Hybrid perovskites, an important class of crystalline inorganic–organic hybrid structures, represent a good example. Having excellent solubility in polar aprotic solvents, cost-effective and high-quality thin films of these materials can be fabricated via various solution processing methods, including screen printing, spin/spray coating, and inkjet printing.6,7 Optoelectronic devices (e.g. LEDs and PVs) based on hybrid perovskite thin-films have achieved competitive performance. Nevertheless, these materials suffer generally from their toxicity and instability.8,9 Though applaudable progress has been made to improve their stability, the search for alternative semiconductors that are nontoxic, robust, and solution-processable represents an important research objective, which may impact the field significantly.
Copper(I) halide (CuX, X = Cl, Br, I) based inorganic–organic hybrid semiconductors, especially those made of Cu–L (L = ligand) coordinate bonds, have attracted substantial interest in luminescence-related applications due to their numerous desired features including excellent structural/optical tunability, strong photoluminescence (PL), high resistance towards heat/moisture/chemical environment, and low cost, facile synthesis.10–12 However, the main issue that limits their applications, especially in optoelectronic devices, is their generally poor solubility. To address this issue, we have recently developed a new subclass of CuX based hybrid semiconductor materials, namely the all-in-one (AIO) type structures.13–15 The AIO-type structures differ from the CuX(L) family in that their inorganic motifs are not neutral CuX, but anionic (CumIm+n)n− and likewise, their organic ligands are not neutral L, but cationic Lk+. The inorganic anions and organic cations are further connected via Cu–L coordinate (dative) bonds to complete the bonding within the structure, as depicted in Fig. 1a. The unique multi-fold bonding at the inorganic/organic interface renders AIO-type structures with integrated properties from both coordinate bonds (e.g., structural/optical tunability, strong luminescence) and ionic bonds (e.g., solubility and stability), greatly raising their potential for applications in optoelectronic devices.
Fig. 1 (a) Schematic illustration of AIO structures. Color scheme: blue: organic ligand; gray: inorganic motif; yellow rod: coordinate bond. Reproduced with permission from ref. 15 from the Royal Society of Chemistry. (b) Left: Selected AIO-type compounds coated on a soft fabric and glass substrate under daylight and UV light; Right: Top-view of the SEM (top) and AFM (bottom) image of the as-made thin film sample of a selected AIO compound. Reproduced with permission from ref. 13 and 18, from American Chemical Society. (c) Color chromaticity of all AIO-type compounds reported to date. (d) Schematic energy diagrams of different emission mechanisms of AIO compounds (Phos. = phosphorescence). |
Since the success in systematic construction of the first group of the AIO-type structures in 2017,14 great efforts by us and others have been devoted to the design of new AIO structures and 60+ AIO compounds have been synthesized to date.13,14,16–26 Their structures range from molecular (zero-dimensional, 0D) species to one-dimensional (1D) chains and two-dimensional (2D) layers. A variety of inorganic anionic modules from the smallest CuI2− monomer to an infinite 2D network of Cu8I102− have been identified, revealing excellent structural diversity of this interesting material class. To gain insight into the ligand effects in these structures, which is crucial to guide the structure modification and property optimization, comprehensive studies have been carried out on different aspects, including coordination affinity,13,23 steric effect,20,22 connectivity19 and hybridization.21 The structure formation of AIO-type compounds may also be influenced by the synthesis conditions. By controlling the ratios of the reagents, different types of AIO structures may result even with the same ligand.
Various methods have been developed to grow high-quality single crystals of AIO-type compounds. The layered diffusion method is one of the most efficient approaches, wherein the reactants are dissolved in different solvents first and then transferred to a reaction vessel as two separated layers to allow slow diffusion to reduce the nucleation rate. In most cases, a middle buffer layer between the two reactant layers is used to further control the reaction rate. For the phases that require high temperatures, the solvothermal method is generally used, in which the solvent system plays an important role in the determination of the resulting structures. Additionally, this synthetic method sometimes involves in situ generation of the cationic ligands when alcohols are used as solvents, which can act as alkylating reagents at high temperatures.
The intriguing solvation behavior of the AIO compounds has been studied in detail and the results suggest it is a direct result of introducing ionic bonds between neutral inorganic motifs (CuX) and organic ligands (L).13,20 Because of the unique bonding characteristics, the solvation of AIO compounds involves the structure complexation in DMSO to generate soluble small fragments, similar to those of hybrid perovskites.15,31,32 The dissolved species were identified as anionic CuX clusters which remain coordinated to the cationic ligands via dative bonds by NMR and mass spectrometry.20,21
In pure ionic CuX hybrid structures, as the organic cations are generally far away from the anionic inorganic motifs with only weak interactions, their photoluminescence is typically cluster-centered (CC) emission. As such, their optical properties are mainly determined by the inorganic modules with negligible ligand effect in most cases, making the fine tuning of electronic structures difficult.33 In contrast, having Cu–L dative bonds, the emission mechanisms of AIO compounds may include metal halide-to-ligand charge transfer [(M + X)LCT], CC and a combination of the two (Fig. 1d), with a strong dependence on the Cu⋯Cu distances (an indicator of cuprophilic interaction). These variables can be altered to suit different application needs.
Generally, ligands with aliphatic binding sites afford AIO structures with relatively short Cu⋯Cu distances (<2.80 Å, twice the vdW radius of Cu atom) and CC emission mechanism. On the other hand, AIO compounds composed of ligands with aromatic binding sites often have longer Cu⋯Cu distance and follow the (M + X)LCT emission mechanism. Electronic structure analysis shows that for this subgroup of structures, the valence band maximum (VBM) is populated mainly by the inorganic motifs, while the conduction band minimum (CBM) is primarily made of the lowest unoccupied molecular orbital (LUMO) of the ligands. Therefore, by selecting ligands with different functional groups (e.g., electron donating or electron withdrawing groups), their LUMO energies, and consequently the bandgap and emission energy of the resultant AIO structures, can be systematically tuned. Interestingly, when the Cu⋯Cu distances approach ∼2.80 Å, the two emission pathways 3CC and3(M + X)LCT may couple and both are responsible for the photoluminescence of the hybrid structures.19 As the higher laying excited state requires higher energy, its relative intensity can be varied by adjusting the excitation energy, including temperature and excitation wavelength, which is often associated with responsive color change of the compounds toward heat and excitation energy.
Moreover, AIO materials often exhibit efficient thermally activated delayed fluorescence (TADF), which is highly favored in harvesting excitons generated in LED devices.34 The extensive (M + X)LCT character of their excited states generally induces distinct spatial separations of the frontier orbitals, leading to relatively small exchange integrals and, consequently, small energy gaps ΔE(S1–T1) between the lowest singlet state S1 and the lowest triplet state T1.35 As a result, a fraction of the electrons can be thermally populated back to S1 from T1via reverse intersystem crossing (RISC) and then follow S1 to S0 radiative transition, benefitting the harvesting of generated singlet and triplet excitons.
The AIO materials were first tested as phosphors in phosphor-converted white LEDs (pc-WLEDs). Such WLEDs generate warm-white light by coating a blue LED chip with blue-excitable yellow phosphor or multiple (green-red) phosphors.36 As phosphors currently dominating the pc-WLED market are made of rare-earth elements (REEs), which not only are subject to the potential supply and cost risks, but also cause severe environmental impact,37 seeking eco-friendly and REE-free alternative phosphor materials would bring substantial benefits to society. The AIO materials stand out as promising candidates due to the advantages mentioned in the previous section, coupled with their easily scalable synthesis, earth-abundance, and excellent blue-excitability.13,14,23 Prototype LED bulbs using selected AIO compounds as phosphors have been assembled.14 The findings imply that the molecular motions of compounds can be suppressed by the use of multidentate ligands, which effectively reduce nonradiative decay and lead to enhancements in IQYs.
Using chiral cationic ligands, a series of hierarchically structured noncentrosymmetrical AIO materials have been successfully synthesized via a non-classical crystallization process involving nanocrystal nucleation, aggregation, oriented attachment and mesoscopic transformation (Fig. 2a). They show interesting circularly polarized luminescence (CPL).25 The chiral AIO polycrystals assemble at nano- and micro-scales and yield a significantly improved luminescence dissymmetry factor (glum) of 1.5 × 10−2 without significant loss of its photoluminescence quantum yield (PLQY). Interestingly, the chiroptical properties of these AIO aggerates strongly hinge on the position of the chiral centre in the ligand, which can substantially influence the interactions among chiral groups within the hierarchically structured polycrystals. These findings point to the possibility of using these compounds as efficient CPL active materials.
Fig. 2 (a) Schematic illustration of the non-classical crystallization process of chiral AIO nanocrystals. Reproduced with permission from ref. 25 from Springer Nature. (b) Left to right: Cross-sectional HeIM image of the prototype YLED device structure using 1D-Cu4I6(bttmp)2 as the sole EML, overall energy band diagram and photographs of the fabricated device at “off” and “on” stages. (c) Left: EQE and current efficiency of the best-performing LED; right: T50 values of the yellow LED device and those of PeLEDs. (b) and (c) are reproduced with permission from ref. 18 from American Chemical Society. (d) Light transmittance (left) and light propagation property of the fabricated AIO based LSC film. Reproduced with permission from ref. 26 from American Chemical Society. |
Recently, we successfully demonstrated the use of AIO materials as an active emissive layer (EML).18 A first-ever yellow LED (YLED) device using an AIO-type hybrid semiconductor 1D-Cu4I6(bttmp)2 as the sole EML was fabricated (Fig. 2b). The spin-coated thin-film samples remain stable under harsh conditions (e.g., elevated temperature and high humidity) for over 2000 h without protection. The prototype YLED device achieves an external quantum efficiency (EQE) of 5.02%. Remarkably, the device demonstrates outstanding stability with its half-lifetime (T50) reaching 35.5 h under ambient conditions (Fig. 2c), while those of most hybrid perovskite-based LED devices are much shorter even tested under one form of protection (in a glovebox, under dry air or being encapsulated).38,39 This work certainly demonstrates the potential of AIO compounds for the construction of robust and nontoxic LED devices.
The possible use of AIO materials as luminescent solar concentrators (LSCs) was also investigated (Fig. 2d).26 LSCs are transparent waveguide substrates that help to provide higher optical concentration to the attached solar cells and thus increase their power output. The higher energy portion of the sunlight (at which the solar cell has low absorption) first gets absorbed by the luminescent material in LSC and converted to lower energy light, and the reemitted light then gets directed to the solar cell.40 A strongly luminescent film (9 cm × 4.5 cm) of 0D-AIO-Cu4I6(pr-ted)2/PVP (polyvinylpyrrolidone) was fabricated by facile blade coating to evaluate the performance of this AIO material as an LSC. The optimized film shows over 85% average transmittance in the visible light range and a high PLQY of 76.1%. In addition, it demonstrates much better waveguide properties than CsPbBr3. The good performance, coupled with their high stability, validates AIO materials as good candidates for LSCs.
First of all, improving the performance and stability of the solution-processable blue-emitting LEDs (BLEDs), particularly deep blue-emitting LEDs, is of great interest to the lighting industry.41,42 The successful assembly of an ultrastable YLED device using the AIO compound as a sole EML may offer an alternative solution.18 To do so, robust and efficient AIO emitters (λem at ∼450 nm) with high photoluminescence and good charge transport properties need to be developed. In addition, the research on AIO compounds as the sole EML in LED devices is still in its infancy. Continuous and thorough investigations to further optimize and increase their EQE are vital to their ultimate implementation in general lighting technologies.
Secondly, the application of AIO semiconductors in the PV solar cells, one of the most important branches of optoelectronic devices, accounts for an important aspect of future research of these materials. Most recent work by us and others has yielded promising solution-processable low bandgap AIO compounds as efficient solar light absorbers. Although the photogenerated excitons may be somewhat localized due to the (M + X)LCT feature and can lead to low carrier mobility, a possible solution is to use ligands with strong π–π stackings to facilitate charge transfer.43 This is a very interesting new direction for the design of nontoxic and robust semiconductors targeted for PV solar cells.
Third, UV emissive AIO-type compounds represent an equally interesting subgroup but are yet to be synthesized. These materials will be extensively explored in our future studies.
Furthermore, building AIO compounds composed of high-dimensional inorganic modules is very desirable. Most of the AIO compounds reported to date contain inorganic modules limited to 0D clusters to 1D chains, with only a few exceptions of 2D layers. AIO structures with 3D inorganic backbones remain to be discovered. Increasing the dimensionality of inorganic motifs would, presumably, largely enhance/improve some very important properties directly relevant to device performance (e.g., conductivity, carrier mobility, diffusion length).
Finally, as a general tool for the design of solution processable and stable hybrid semiconductors, the strategy of including ionic bonds within coordinate networks can be extended to other hybrid materials44 beyond the copper halide-based hybrid family. By applying the AIO approach to other hybrid systems, exciting new opportunities for discovering advanced functional semiconductors could be unlocked.
This journal is © the Partner Organisations 2023 |