Issue 33, 2024

Revealing the critical pore size for hydrogen storage via simultaneous enclathration and physisorption in activated carbon

Abstract

Hydrogen hydrate is regarded as an ideal hydrogen storage medium, but it faces unsolved challenges related to its extreme formation and stabilization conditions. Recent experiments have demonstrated that utilizing porous host materials can ease hydrate formation conditions and enhance stability. However, there is an urgent need to examine the nanoscopic interactions between hydrogen hydrates and solid porous materials to understand and optimize the mechanisms of hydrogen storage in the combined system. Here, the effect of pore size on hydrogen storage in hydrates confined in porous activated carbon is explored through molecular dynamics simulations, with initial validation by ab initio calculations. The results revealed a critical pore size of ∼2 nm, below which hydrogen hydrate decomposes. This critical size is primarily influenced by temperature and oxygen surface groups, while being largely unaffected by other properties of the activated carbon host. Furthermore, pockets of physisorbed H2 gas were found to occupy the smallest pores (around 1 nm). The results revealed a previously unreported dual-storage mechanism for H2 gas in hierarchical porous structures, where H2 can simultaneously be stored in micropores through physisorption and larger meso- and macro-pores through enclathration. Given further research and experimental verification, the hybrid mechanism could enable hydrogen storage capacities in hydrate-filled porous media to match or exceed that of pure hydrogen hydrate, while simultaneously offering milder formation and stability conditions.

Graphical abstract: Revealing the critical pore size for hydrogen storage via simultaneous enclathration and physisorption in activated carbon

Supplementary files

Transparent peer review

To support increased transparency, we offer authors the option to publish the peer review history alongside their article.

View this article’s peer review history

Article information

Article type
Paper
Submitted
16 ذو القعدة 1445
Accepted
09 محرم 1446
First published
10 محرم 1446

J. Mater. Chem. A, 2024,12, 21830-21844

Revealing the critical pore size for hydrogen storage via simultaneous enclathration and physisorption in activated carbon

E. V. Rothmund, J. He, Z. Zhang and S. Xiao, J. Mater. Chem. A, 2024, 12, 21830 DOI: 10.1039/D4TA03607G

To request permission to reproduce material from this article, please go to the Copyright Clearance Center request page.

If you are an author contributing to an RSC publication, you do not need to request permission provided correct acknowledgement is given.

If you are the author of this article, you do not need to request permission to reproduce figures and diagrams provided correct acknowledgement is given. If you want to reproduce the whole article in a third-party publication (excluding your thesis/dissertation for which permission is not required) please go to the Copyright Clearance Center request page.

Read more about how to correctly acknowledge RSC content.

Social activity

Spotlight

Advertisements