Issue 39, 2023

The effect of non-intrinsic factors on pulse discharge and energy releasing performance of dielectric ceramics

Abstract

Power pulse ceramic capacitors are widely used in pulse generators and other fields because of their excellent charge and discharge performance. In this work, 0.55Bi0.5Na0.5TiO3–0.45Ba0.85Ca0.15Ti0.85Zr0.1Sn0.05O3(0.55NBT–0.45BCZTS) relaxor ferroelectric ceramics were manufactured using the solid-state reaction method. The charge and discharge properties of 0.55NBT–0.45BCZTS relaxor ferroelectric ceramics with different electrode areas and dielectric thicknesses were measured under the same electric field. The shape of the ceramic capacitor is related to its static capacitance value. As the static capacitance value changes, the charge and discharge performance of the sample presents different laws. Additionally, the charge and discharge performance of the sample is also affected by the resistance and inductance of the RLC circuit. These non-intrinsic factors seriously affect the characterization of charge and discharge performance of power pulse ceramic capacitors. Presently, a unified standard for the charge and discharge test of ceramic capacitors is needed. To standardize the charge and discharge test, avoid the non-intrinsic factors and better compare the charge and discharge performances of different materials, we suggest that the sample for charge and discharge tests should be set with a thickness of 0.03 cm, an electrode diameter of 0.4 cm, an RLC circuit resistance of 100 Ω and an inductance of 2 μH.

Graphical abstract: The effect of non-intrinsic factors on pulse discharge and energy releasing performance of dielectric ceramics

Supplementary files

Article information

Article type
Paper
Submitted
29 شوال 1444
Accepted
16 ذو الحجة 1444
First published
17 ذو الحجة 1444

J. Mater. Chem. C, 2023,11, 13220-13227

The effect of non-intrinsic factors on pulse discharge and energy releasing performance of dielectric ceramics

H. Xie, Y. Pu, Y. Shang, L. Zhang, B. Wang and Y. Hao, J. Mater. Chem. C, 2023, 11, 13220 DOI: 10.1039/D3TC01737K

To request permission to reproduce material from this article, please go to the Copyright Clearance Center request page.

If you are an author contributing to an RSC publication, you do not need to request permission provided correct acknowledgement is given.

If you are the author of this article, you do not need to request permission to reproduce figures and diagrams provided correct acknowledgement is given. If you want to reproduce the whole article in a third-party publication (excluding your thesis/dissertation for which permission is not required) please go to the Copyright Clearance Center request page.

Read more about how to correctly acknowledge RSC content.

Social activity

Spotlight

Advertisements