Issue 17, 2014

Direct visualization of initial SEI morphology and growth kinetics during lithium deposition by in situ electrochemical transmission electron microscopy

Abstract

Deposition of Li is a major safety concern existing in Li-ion secondary batteries. Here we perform the first in situ high spatial resolution measurement coupled with real-time quantitative electrochemistry to characterize SEI formation on gold using a standard battery electrolyte. We demonstrate that a dendritic SEI forms prior to Li deposition and that it remains on the surface after Li electrodissolution.

Graphical abstract: Direct visualization of initial SEI morphology and growth kinetics during lithium deposition by in situ electrochemical transmission electron microscopy

Supplementary files

Article information

Article type
Communication
Submitted
26 Xim 2013
Accepted
19 Kax 2013
First published
20 Kax 2013

Chem. Commun., 2014,50, 2104-2107

Direct visualization of initial SEI morphology and growth kinetics during lithium deposition by in situ electrochemical transmission electron microscopy

R. L. Sacci, N. J. Dudney, K. L. More, L. R. Parent, I. Arslan, N. D. Browning and R. R. Unocic, Chem. Commun., 2014, 50, 2104 DOI: 10.1039/C3CC49029G

To request permission to reproduce material from this article, please go to the Copyright Clearance Center request page.

If you are an author contributing to an RSC publication, you do not need to request permission provided correct acknowledgement is given.

If you are the author of this article, you do not need to request permission to reproduce figures and diagrams provided correct acknowledgement is given. If you want to reproduce the whole article in a third-party publication (excluding your thesis/dissertation for which permission is not required) please go to the Copyright Clearance Center request page.

Read more about how to correctly acknowledge RSC content.

Social activity

Spotlight

Advertisements