Porous SnO2–Fe2O3 nanocubes with improved electrochemical performance for lithium ion batteries†
Abstract
Mixed oxide SnO2–Fe2O3 porous nanocubes were prepared by simply annealing the precursor of Sn3[Fe(CN)6]4 nanocubes, which were obtained through a facile solvothermal method. Calcination of the precursor at 350 °C produced uniform SnO2–Fe2O3 nanocubes without obvious morphological deformation, but with lots of open void space in the nanocubes. The Brunauer–Emmett–Teller N2 adsorption–desorption analysis shows that the as-synthesized SnO2–Fe2O3 has a specific surface area of 170.2 m2 g−1 with a pore size of around 5 nm. The porous SnO2–Fe2O3 nanocubes as anode materials for the lithium-ion battery show a high initial capacity of 1020.2 mA h g−1 at a current density of 200 mA g−1 and maintain at 567.5 mA h g−1 at the 50th cycle, which is distinctly higher than those reported for SnO2-based materials. The enhanced performance towards lithium storage can be ascribed to the high specific area, an appropriate pore size and the synergistic effect of SnO2 and Fe2O3.