The activation of H3PW12O40 under different thermal conditions has been evaluated by calorimetry in acetonitrile solution using pyridine as a probe, and the results correlated to the dehydration of 1-propanol. Treatments at 200, 300, and 400 °C show substantial changes in the catalytic activity of 12-tungstophosphoric acid as a function of activation temperature and time. Analysis of the samples by XRD, FTIR, TGA and DSC was performed to determine structural changes and thermal stability of the heteropolytungstic acid.

Graphical abstract: Dehydration of 1-propanol using H3PW12O40 as catalyst

Article information

Article type
Paper
Submitted
30 Jun 2000
Accepted
09 Nov 2000
First published
09 Jan 2001

J. Chem. Soc., Dalton Trans., 2001, 228-231

Dehydration of 1-propanol using H3PW12O40 as catalyst

J. A. Dias, S. C. L. Dias and N. E. Kob, J. Chem. Soc., Dalton Trans., 2001, 228 DOI: 10.1039/B005256F

To request permission to reproduce material from this article, please go to the Copyright Clearance Center request page.

If you are an author contributing to an RSC publication, you do not need to request permission provided correct acknowledgement is given.

If you are the author of this article, you do not need to request permission to reproduce figures and diagrams provided correct acknowledgement is given. If you want to reproduce the whole article in a third-party publication (excluding your thesis/dissertation for which permission is not required) please go to the Copyright Clearance Center request page.

Read more about how to correctly acknowledge RSC content.

Spotlight

Advertisements