Issue 17, 2014
Previous Article Next Article

Direct visualization of initial SEI morphology and growth kinetics during lithium deposition by in situ electrochemical transmission electron microscopy

Author affiliations

Abstract

Deposition of Li is a major safety concern existing in Li-ion secondary batteries. Here we perform the first in situ high spatial resolution measurement coupled with real-time quantitative electrochemistry to characterize SEI formation on gold using a standard battery electrolyte. We demonstrate that a dendritic SEI forms prior to Li deposition and that it remains on the surface after Li electrodissolution.

Graphical abstract: Direct visualization of initial SEI morphology and growth kinetics during lithium deposition by in situ electrochemical transmission electron microscopy

Back to tab navigation
Please wait while Download options loads

Supplementary files

Publication details

The article was received on 26 Nov 2013, accepted on 19 Dec 2013 and first published on 20 Dec 2013


Article type: Communication
DOI: 10.1039/C3CC49029G
Citation: Chem. Commun., 2014,50, 2104-2107
  •   Request permissions

    Direct visualization of initial SEI morphology and growth kinetics during lithium deposition by in situ electrochemical transmission electron microscopy

    R. L. Sacci, N. J. Dudney, K. L. More, L. R. Parent, I. Arslan, N. D. Browning and R. R. Unocic, Chem. Commun., 2014, 50, 2104