Issue 27, 2011

Solvothermal synthesis of lithium iron phosphate nanoplates

Abstract

Uniform lithium iron phosphate nanoplates with a thickness of 30 nm, width of 100 nm, and length of 200 nm are synthesized by a solvothermal method. Electrochemical measurements show that the nanoplates exhibit low polarization and reach a discharge capacity of 165 mAh g−1 at 0.1 C, 140 mAh g−1 at 5 C.

Graphical abstract: Solvothermal synthesis of lithium iron phosphate nanoplates

Supplementary files

Article information

Article type
Communication
Submitted
29 Nov 2010
Accepted
06 Jan 2011
First published
14 Jan 2011

J. Mater. Chem., 2011,21, 9994-9996

Solvothermal synthesis of lithium iron phosphate nanoplates

C. Nan, J. Lu, C. Chen, Q. Peng and Y. Li, J. Mater. Chem., 2011, 21, 9994 DOI: 10.1039/C0JM04126B

To request permission to reproduce material from this article, please go to the Copyright Clearance Center request page.

If you are an author contributing to an RSC publication, you do not need to request permission provided correct acknowledgement is given.

If you are the author of this article, you do not need to request permission to reproduce figures and diagrams provided correct acknowledgement is given. If you want to reproduce the whole article in a third-party publication (excluding your thesis/dissertation for which permission is not required) please go to the Copyright Clearance Center request page.

Read more about how to correctly acknowledge RSC content.

Spotlight

Advertisements